The Influence of Process Parameters on the Microstructural Properties of Spray-Pyrolyzed β-Ga2O3
被引:6
作者:
Schmidt, Constance
[1
]
Fechner, Axel
[1
]
Selyshchev, Oleksandr
[1
]
Zahn, Dietrich R. T.
[1
]
机构:
[1] Tech Univ Chemnitz, Semicond Phys, D-09107 Chemnitz, Germany
关键词:
beta-Ga2O3;
spray pyrolysis;
spray coating;
ultrasonic nebulization;
microstructures;
Raman spectroscopy;
X-ray diffraction;
scanning electron microscopy;
residual stress measurements;
GALLIUM OXIDE;
THIN-FILMS;
OPTICAL-PROPERTIES;
CATALYTIC GROWTH;
RAMAN-SPECTRA;
GA2O3;
FILMS;
PHOTOLUMINESCENCE;
DECOMPOSITION;
NANOWIRES;
CRYSTAL;
D O I:
10.3390/nano13091455
中图分类号:
O6 [化学];
学科分类号:
0703 ;
摘要:
In this work, the deposition of beta-Ga2O3 microstructures and thin films was performed with Ga(NO3)(3) solutions by ultrasonic nebulization and spray coating as low-cost techniques. By changing the deposition parameters, the shape of beta-Ga2O3 microstructures was controlled. Micro-spheres were obtained by ultrasonic nebulization. Micro-flakes and vortices were fabricated by spray coating aqueous concentrated and diluted precursor solutions, respectively. Roundish flakes were achieved from water-ethanol mixtures, which were rolled up into tubes by increasing the number of deposition cycles. Increasing the ethanol-to-water ratio allows continuous thin films at an optimal Ga(NO3)(3) concentration of 0.15 M and a substrate temperature of 190 degrees C to be formed. The monoclinic beta-Ga2O3 phase was achieved by thermal annealing at 1000 degrees C in an ambient atmosphere. Scanning electronic microscopy (SEM), X-ray diffraction (XRD), and UV-Raman spectroscopy were employed to characterize these microstructures. In the XRD study, in addition to the phase information, the residual stress values were determined using the sin(2)(psi) method. Raman spectroscopy confirms that the beta-Ga2O3 phase and relative shifts of the Raman modes of the different microstructures can partially be assigned to residual stress. The high-frequency Raman modes proved to be more sensitive to shifting and broadening than the low-frequency Raman modes.