Direct laser-filler wire welding of Al-Si coated 22MnB5 steel without removing the Al-Si coating

被引:9
|
作者
Xu, Wei [1 ,2 ]
Jiang, Zhigong [4 ]
Zhang, Jiazhi [1 ]
Tao, Wu [1 ]
Zhang, Xuzhi [1 ,2 ]
Yang, Shanglu [1 ,3 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Opt & Fine Mech, Shanghai 201800, Peoples R China
[2] Univ Chinese Acad Sci, Beijing 100049, Peoples R China
[3] Univ Chinese Acad Sci, Ctr Mat Sci & Optoelect Engn, Beijing, Peoples R China
[4] CCAS Changchun Steel Serv Ctr Ltd, Changchun 130012, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
关键词
Al-Si coating; Press-hardened steel; Laser welding; Filler wire; Microstructure; Mechanical property; PRESS-HARDENED STEEL; MICROSTRUCTURE EVOLUTION; MECHANICAL-PROPERTIES; MARANGONI CONVECTION; WELDED BLANKS; BORON STEEL; HOT;
D O I
10.1016/j.jmrt.2023.03.138
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-Si coated 22MnB5 steels are one of the most important lightweight materials for automotive weight reduction and safety improvement due to its advantages of light weight, high strength and good formability at high temperature. Considering the formation of a-ferrite caused by the Al-Si coating deteriorating the weld mechanical performance, the common way in the automotive industry is to remove the Al-Si coating prior to laser welding. In this work, a patented laser-filler wire welding process was developed with a high strength steel wire to inhibit the formation of a-ferrite and achieve high quality laser weld in Al-Si coated 22MnB5 without the requirement of removing the Al-Si coating. A formula for calculating the average content of Al element in the fusion zone was provided and verified by experiment. Experimental results show that Al segregation in the fusion zone with the designated filler wire was reduced, and the microstructure was full martensite with high dislocation density. The strain of the welded joint was concentrated in the hot-stamped base metal (HSBM) and fractured in an obvious necking during the tensile shear test. The tensile strength and elongation of the welded joint with filler wire increased by 7.5% and 183.9% compared with that without filler wire. (c) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:2265 / 2278
页数:14
相关论文
共 50 条
  • [41] Microstructure and properties of laser welded joint with filler wire of Al-Si coated press-hardened steel
    Zhang Z.
    Wang X.
    Ye S.
    Sun Q.
    Liu Z.
    Di H.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2021, 42 (12): : 18 - 25
  • [42] Effect of Welding Processes on Microstructure and Mechanical Properties of Laser-Welded Al-Si-Coated 22MnB5 Steel
    He, Qi
    Hou, Zeran
    Kong, Jie
    Deng, Lulu
    Ma, Xiaolong
    Min, Junying
    NUMERICAL METHODS IN INDUSTRIAL FORMING PROCESSES, NUMIFORM 2023, 2024, : 261 - 271
  • [43] Laser welding of Al-Si coated hot stamping steel
    Kim, C.
    Kang, M. J.
    Park, Y. D.
    11TH INTERNATIONAL CONFERENCE ON THE MECHANICAL BEHAVIOR OF MATERIALS (ICM11), 2011, 10
  • [44] MICROSTRUCTURE MODIFICATIONS OF Al-Si-COATED PRESS-HARDENED STEEL 22MnB5 BY LASER WELDING
    Sebestova, Hana
    Hornik, Petr
    Mika, Filip
    Mikmekova, Sarka
    Ambroz, Ondrej
    Mrna, Libor
    32ND INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, METAL 2023, 2024, : 302 - 307
  • [45] Hydrogen embrittlement behavior of Al-Si coated steel laser wire filling welding joint
    Xiong, Li
    Du, Yu
    Teng, Fei
    Zhang, Zhao-Yang
    Liu, Ren-Dong
    Xu, Xin
    Jiang, Zhi-Gong
    Li, Tian
    Li, Xiang
    Wang, Xiao-Nan
    OPTICS AND LASER TECHNOLOGY, 2025, 181
  • [46] Suppression of δ-ferrite formation on Al-Si coated press-hardened steel during laser welding
    Sun, Qian
    Di, Hong-Shuang
    Wang, Xiao-Nan
    Chen, Xia-Ming
    MATERIALS LETTERS, 2019, 245 : 106 - 109
  • [47] STATE OF STRAIN AND DEVELOPMENT OF MICROSTRUCTURE OF 22MnB5 STEEL AND Al-Si COATING DURING DEEP DRAwING OF AUTOMOTIVE B PILLAR
    PACKO, M.
    KRAWCZYK, J.
    SLEBODA, T.
    FROCISZ, L.
    RUMINSKI, M.
    LYPCHANSKYI, O.
    TOKARSKI, T.
    PIASECKI, P.
    ARCHIVES OF METALLURGY AND MATERIALS, 2021, 66 (02) : 601 - 608
  • [48] Material transfer during high temperature sliding of Al-Si coated 22MnB5 steel against PVD coatings with and without aluminium
    Mozgovoy, Sergej
    Alik, Lotfi
    Hardell, Jens
    Prakash, Braham
    WEAR, 2019, 426 : 401 - 411
  • [49] Effect of Al-Si coating on laser spot welding of press hardened steel and process improvement with annular stirring
    Chen, Nannan
    Wan, Zixuan
    Wang, Hui-Ping
    Li, Jingjing
    Solomon, Joshua
    Carlson, Blair E.
    MATERIALS & DESIGN, 2020, 195 (195)
  • [50] The influence of in-situ alloying of electro-spark deposited coatings on the multiscale morphological and mechanical properties of laser welded Al-Si coated 22MnB5
    Khan, M. Shehryar
    Enrique, P.
    Ghatei-Kalashami, A.
    Lopes, J. G.
    Schell, N.
    Oliveira, J. P.
    Biro, E.
    Zhou, Y. Norman
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 839