Effect of Fe addition in W-Ni-Cu heavy alloy processed through powder metallurgy on microstructure and mechanical properties

被引:22
作者
Shakunt, Navindra Shekhar [1 ]
Upadhyaya, Anish [1 ]
机构
[1] Indian Inst Technol Kanpur, Dept Mat Sci & Engn, Kanpur 208016, Uttar Pradesh, India
关键词
Tungsten Heavy Alloy; Microstructure quantification; Contiguity; Compressive strength; Fracture mechanism; DIHEDRAL ANGLE; BEHAVIOR; DENSIFICATION; DEFORMATION; TEMPERATURE; COMPOSITES; CONTIGUITY;
D O I
10.1016/j.jallcom.2023.172578
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present investigation, effect of Fe addition to 90 W-aNi-bCu-xFe, (where a/b was 6/4; x = 0, 0.5, 1.0, 1.5, and 2.0) on the microstructure and mechanical behaviour of Tungsten heavy alloys (WHAs) was undertaken. WHAs were fabricated via powder metallurgy processing. Sintering of green compact was done with a horizontal tubular furnace at 1400 degrees C under hydrogen atmosphere for 60 min. A synergetic effect of Fe dissolution in Ni-Cu binder on densification response was observed. The tungsten solubility in the matrix was measured using EPMA and found to decrease with the increase of Fe content. The tungsten particle size reduction of up to 20%, compared to 90 W-6Ni-4Cu heavy alloy, was observed. The bulk hardness measurements showed a maximum of about 332 HV5 for 2.0 wt% Fe containing W-Ni-Cu alloy. The mechanical properties, such as compressive and flexural/bending strength were determined by employing the uniaxial compression and three-point bend test and found to be 1732 +/- 36 MPa and 1147 +/- 22 MPa, respectively. Because of Fe content in the WHAs, lower volume % of the matrix and higher W-W contiguity in the microstructure resulted leading to superior compressive strength. Detailed fractography was done on all sintered WHA samples to understand the failure response during transverse loading. Fractography on fracture surface of bend tested samples was carried out. The separation of the W-W interface and W/W trans-granular failure was the predominant fracture mechanism observed.
引用
收藏
页数:11
相关论文
共 45 条
[31]   LIQUID IMMISCIBLE ALLOYS [J].
RATKE, L ;
DIEFENBACH, S .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 1995, 15 (7-8) :263-347
[32]   Effects of sintering conditions on mechanical properties of mechanically alloyed tungsten heavy alloys [J].
Ryu, HJ ;
Hong, SH .
METALS AND MATERIALS INTERNATIONAL, 2001, 7 (03) :221-226
[33]   Effect of partial and full substitution of Ni with NiB on densification, structure and properties of 90W-6Ni-2Fe-2Co heavy alloys [J].
Sengupta, P. ;
Debata, M. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 774 :145-152
[34]   Segregation and immiscibility in liquid binary alloys [J].
Singh, RN ;
Sommer, F .
REPORTS ON PROGRESS IN PHYSICS, 1997, 60 (01) :57-150
[35]   Combination of mechanical alloying and two-stage sintering of a 93W-5.6Ni-1.4Fe tungsten heavy alloy [J].
Soon, HH ;
Ryu, HJ .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 344 (1-2) :253-260
[36]  
Wang CB, 2002, J MATER SCI TECHNOL, V18, P234
[37]   PRODUCTION OF TUNGSTEN-IRON-NICKEL ALLOYS BY MECHANICAL ALLOYING TECHNIQUE [J].
WILLIAMS, DJ ;
CLYENS, S ;
JOHNSON, W .
POWDER METALLURGY, 1980, 23 (02) :92-94
[38]  
Wittenauer J.P., 1991, Report no. LMSC-F404866
[39]   Dihedral angle measurement in microgravity liquid phase sintered microstructures [J].
Ye, S ;
He, Y ;
Smith, JE .
JOURNAL OF MATERIALS SCIENCE, 2003, 38 (02) :377-388
[40]   Compressive behavior of liquid phase sintered 90 W-7Ni-3Fe heavy alloy at high temperature and low strain rate condition [J].
Yu, Yang ;
Ren, Chaoyuan ;
Zhang, Wencong .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2018, 76 :149-157