Impact of high-current pulsed electron beam modification on element diffusion and performance of Ti6Al4V/AISI 316 L stainless steel diffusion bonded joints

被引:7
|
作者
Tian, Nana [1 ]
Zhang, Conglin [2 ]
Lyu, Peng [1 ]
Guan, Jintong [1 ]
Peng, Chingtun [1 ]
Cai, Jie [3 ]
Guan, Qingfeng [1 ]
机构
[1] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Peoples R China
[2] Yancheng Inst Technol, Sch Mat Sci & Engn, Yancheng 221051, Peoples R China
[3] Jiangsu Univ, Engn Inst Adv Mfg & Modern Equipment Technol, Zhenjiang 212013, Peoples R China
基金
中国国家自然科学基金;
关键词
High-current pulsed electron beam (HCPEB); Diffusion activation energy; Bonding interface; Shear strength; Crystal defects; Surface modification; TC4; TITANIUM-ALLOY; INTERFACIAL MICROSTRUCTURE; SURFACE MICROSTRUCTURE; LOW-ENERGY; HCPEB; FE;
D O I
10.1016/j.matchar.2023.113163
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The diffusion bonding process between Ti6Al4V and 022Cr17NiMo2 stainless steel (AISI 316 L SS) was carried out under vacuum conditions, applying a 10 MPa load for 40 min within a temperature range of 800-900 & DEG;C. This study investigates the influence of high-current pulsed electron beam (HCPEB) modification on the micro-structure at the interface and the shear strength of Ti6Al4V/AISI 316 L SS joints. After HCPEB pretreatment, a well-formed diffusion bond was achieved between Ti6Al4V and AISI 316 L SS at 900 & DEG;C. Through calculations, the diffusion coefficient and diffusion activation energy of Fe in the Ti6Al4V section were determined, which demonstrated that Fe exhibits higher diffusion rates in the HCPEB-modified joints. The modified joint, subjected to 900 & DEG;C, exhibited a maximum bond strength of 208 MPa, which is attributed to dispersion and solid solution strengthening. Consequently, the implementation of HCPEB modification proves effective in promoting element diffusion and enhancing the mechanical performance of the joints. The presence of abundant crystal defects, including vacancies, dislocations, and grain boundaries (GBs) generated by HCPEB, is believed to be responsible for the observed improvement in diffusion.
引用
收藏
页数:10
相关论文
共 36 条
  • [21] Surface modification of 316L stainless steel by high current pulsed electron beam - II. Corrosion behaviors in the simulated body fluid
    Zhang Kemin
    Yang Dazhi
    Zou Jianxin
    Dong Chuang
    ACTA METALLURGICA SINICA, 2007, 43 (01) : 71 - 76
  • [22] Surface modification of 316L stainless steel by high current pulsed electron beam - I. Selective purification of surface and its mechanism
    Zhang Kemin
    Yang Dazhi
    Zou Jianxin
    Dong Chuang
    ACTA METALLURGICA SINICA, 2007, 43 (01) : 64 - 70
  • [23] Experimental investigation on the bio-tribocorrosive behavior of Ti6Al4V alloy and 316 L stainless steel in two biological solutions
    Ruggiero, Alessandro
    De Stefano, Marco
    TRIBOLOGY INTERNATIONAL, 2023, 190
  • [24] Influence of bonding time during diffusion bonding of Ti-6Al-4V to AISI 321 stainless steel on metallurgical and mechanical properties
    Wang, Hongliang
    Paidar, Moslem
    Kumar, N. Keerthi
    Eldin, Hany M. Seif
    Kannan, Sathish
    Abdullaev, Sherzod
    Mehrez, Sadok
    VACUUM, 2024, 222
  • [25] Interfacial microstructure and shear strength of Ti6Al4V alloy/316 L stainless steel joint brazed with Ti33.3Zr16.7Cu50-xNix amorphous filler metals
    Xia, Yueqing
    Dong, Honggang
    Zhang, Runze
    Wang, Yaqiang
    Hao, Xiaohu
    Li, Peng
    Dong, Chuang
    MATERIALS & DESIGN, 2020, 187
  • [26] A novel dissimilar resistance spot welding of Ti6Al4V alloy and 316L stainless steel via copper as interlayer by using optimal electrodes
    Zhang, Weihua
    Zhang, Kunlong
    Yang, Yue
    Sun, Xiangyu
    Yu, Sirong
    Li, Yongqiang
    Yu, Yongtao
    Sun, Daqian
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 33 : 5425 - 5437
  • [27] Influence of laser surface modification on corrosion behavior of stainless steel 316L and Ti-6Al-4V in simulated biofluid
    Singh, R
    Martin, M
    Dahotre, NB
    SURFACE ENGINEERING, 2005, 21 (04) : 297 - 306
  • [28] The effect of holding time on dissimilar resistance spot welding of stainless steel 316L and Ti6Al4V titanium alloy with aluminum interlayer
    Taufiqurrahman, Iqbal
    Ginta, Turnad Lenggo
    Mustapha, Mazli
    MATERIALS TODAY-PROCEEDINGS, 2021, 46 : 1563 - 1568
  • [29] Influence of Diffusion Bonding Pressure on Microstructural Features and Strength Performance of Dissimilar Ti-6Al-4V Alloy and AISI 304 Steel Joints Developed Using Copper Interlayer
    Negemiya, A. Arun
    Rajakumar, Selvarajan
    Sonar, Tushar
    Ivanov, Mikhail
    JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME, 2023, 145 (04):
  • [30] Principle for obtaining high joint quality in dissimilar friction welding of Ti-6Al-4V alloy and SUS316L stainless steel
    Liu, Huihong
    Aoki, Yo
    Aoki, Yasuhiro
    Ushioda, Kohsaku
    Fujii, Hidetoshi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 46 : 211 - 224