Cyclic oxidation and hot corrosion performance of direct metal laser sintered and wrought alloy 718 at 800°C in air and molten salts containing Na2SO4, V2O5 and NaCl

被引:3
作者
Muthu, S. M. [1 ]
Veeman, Dhinakaran [1 ]
Paul, Shiladithya [2 ,4 ]
Kumar, M. Prem [3 ]
机构
[1] Chennai Inst Technol, Ctr Addit Mfg, Chennai 600069, Tamil Nadu, India
[2] Univ Leicester, Mat Innovat Ctr, Sch Engn, Leicester, England
[3] VIT, Sch Mech Engn, Vellore, Tamil Nadu, India
[4] TWI, Mat Performance & Integr Grp, Granta Pk, Cambridge, England
关键词
Alloy; 718; additive manufacturing; hot corrosion; oxidation; microstructure; RESISTANCE; MICROSTRUCTURE;
D O I
10.1080/1478422X.2023.2244236
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The main aim of this research work is to investigate the high-temperature cyclic corrosion performance of the wrought and direct metal laser sintered (DMLS) alloy 718 in the air and molten salts NaCl-90%Na2SO4 and three salt mixture (3SM) Na2SO4-10%V2O5-10%NaCl atmosphere for 120 h at 800 & DEG;C. The microstructure of the wrought and DMLS alloy illustrated the austenitic and dendrite structure. Scanning electron microscope (SEM) and X-ray diffraction (XRD) were used to evaluate the structure and phase constitutions of the scale. Visual and microstructural evaluation of the alloy post-exposure indicates that corrosion is more prevalent in molten salt conditions, when compared to air, and Cl-species induced the active oxidation in molten salt. The oxide film development and damage mechanism were detailed and explained by a cross-sectional investigation. Significant spalling and sputtering were also noticed in the S3 salt mixture. This might be attributed to the rapid formation of oxide scales by vanadate, followed by dissolution of the oxide in molten sulphate and chloride. The results divulged that both AM-built and wrought alloy exhibited the similar corrosion properties and both the alloys were undergone severe degradation in MS condition.
引用
收藏
页码:631 / 644
页数:14
相关论文
共 50 条
  • [21] A study on hot corrosion performance of high velocity arc-sprayed FeCrNiAlMnB/Cr3C2 coating exposed to Na2SO4 + K2SO4 and Na2SO4 + NaCl
    Cheng, Jie
    Wu, Yuping
    Shen, Wei
    Hong, Sheng
    Qiao, Lei
    Wang, Yujun
    SURFACE & COATINGS TECHNOLOGY, 2020, 397
  • [22] Hot corrosion behavior of TiO2 doped, Yb2O3 stabilized zirconia exposed to V2O5 + Na2SO4 molten salt at 700-1000 °C
    Guo, Lei
    Yan, Zheng
    Yu, Jianxing
    Zhang, Chenglong
    Li, Mingzhu
    Ye, Fuxing
    Ji, Vincent
    CERAMICS INTERNATIONAL, 2018, 44 (01) : 261 - 268
  • [23] Investigation of the effect of V2O5 and Na2SO4 melted salts on thermal barrier coatings under cyclic conditions
    Ozgurluk, Yasin
    Doleker, Kadir Mert
    Karaoglanli, Abdullah Cahit
    ANTI-CORROSION METHODS AND MATERIALS, 2019, 66 (05) : 644 - 650
  • [24] Hot corrosion behaviour of plasma-sprayed functionally graded thermal barrier coatings in the presence of Na2SO4 + V2O5 molten salt
    Vakilifard, Hamide
    Ghasemi, Reza
    Rahimipour, Mohammadreza
    SURFACE & COATINGS TECHNOLOGY, 2017, 326 : 238 - 246
  • [25] Na2SO4 and V2O5 molten salts corrosion resistance of plasma-sprayed nanostructured ceria and yttria co-stabilized zirconia thermal barrier coatings
    Hajizadeh-Oghaz, Morteza
    Razavi, Reza Shoja
    Ghasemi, Ali
    Valefi, Zia
    CERAMICS INTERNATIONAL, 2016, 42 (04) : 5433 - 5446
  • [26] Microstructure evolution and hot corrosion mechanisms of Ba2REAlO5 (RE = Yb, Er, Dy) exposed to V2O5 + Na2SO4 molten salt
    Guo, Lei
    Zhang, Chenglong
    He, Qing
    Yu, Jianxing
    Yan, Zheng
    Ye, Fuxing
    Dan, Chengyi
    Ji, Vincent
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (10) : 3555 - 3563
  • [27] Hot corrosion behavior of plasma sprayed 8YSZ-alumina-CNT composite coating in Na2SO4-60% V2O5 molten salt environment
    Thakare, J. G.
    Mulik, R. S.
    Mahapatra, M. M.
    Upadhyaya, Rohit
    CERAMICS INTERNATIONAL, 2018, 44 (17) : 21533 - 21545
  • [28] Hot-corrosion behavior of a La2Ce2O7/YSZ thermal barrier coating exposed to Na2SO4 + V2O5 or V2O5 salt at 900 °C
    Wang, Xizhong
    Guo, Lei
    Peng, Hui
    Zheng, Lei
    Guo, Hongbo
    Gong, Shengkai
    CERAMICS INTERNATIONAL, 2015, 41 (05) : 6604 - 6609
  • [29] Hot corrosion behavior of Sc2O3-Y2O3-ZrO2 thermal barrier coatings in presence of Na2SO4 + V2O5 molten salt
    Liu, Huai-fei
    Xiong, Xiang
    Li, Xiao-bin
    Wang, Ya-lei
    CORROSION SCIENCE, 2014, 85 : 87 - 93
  • [30] Role of Magnesia Stabilized Zirconia Dispersion on the Hot Corrosion Behaviour of NiCrAlY Plasma-Sprayed Coatings in Na2SO4+50 wt% V2O5 and Na2SO4+10 wt% NaCl Melts at 800 °C
    Sreedhar, Gosipathala
    Raja, V. S.
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2016, 69 (04) : 869 - 879