Comparison between different fracture toughness techniques in zirconia dental ceramics

被引:11
作者
Alves, Manuel Fellipe Rodrigues Pais [1 ]
dos Santos, Claudinei [2 ]
Elias, Carlos Nelson [3 ]
Amarante, Jose Eduardo Vasconcellos [4 ]
Ribeiro, Sebastiao [5 ]
机构
[1] Univ Aveiro, Dept Mat & Ceram Engn, CICECO, Aveiro, Portugal
[2] Univ Estado Rio De Janeiro, Fac Technol, UERJ FAT, Resende, Brazil
[3] Mil Inst Engn, Dept Mat Sci, IME, Brasilia, DF, Brazil
[4] Univ Fed Fluminense UFF, Dept Specif Training, Nova Friburgo, Brazil
[5] Univ Sao Paulo, Dept Mat Engn, Lorena Engn Sch, USP EEL, Sao Paulo, Brazil
关键词
ceramic; fracture toughness; single-edge-V-notched beam (SEVNB); Vickers indentation (IF); MICROSTRUCTURE-DEVELOPMENT MECHANISM; Y-TZP CERAMICS; TETRAGONAL ZIRCONIA; GRAIN-SIZE; TRANSFORMATION BEHAVIOR; DIFFRACTION; CRACK; TEMPERATURE; STRENGTH; HARDNESS;
D O I
10.1002/jbm.b.35137
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
Vickers indentation (IF) and single-edge-V-notched beam (SEVNB), to measure the fracture toughness (K-IC) of zirconia-based dental ceramics and mathematical models were proposed to establish a correlation between both. Zirconia (ZrO2) stabilized with 3 mol. % of Y2O3 (3Y-TZP) and 5 mol% of Y2O3 (5Y-PSZ) were compacted (n = 42) and sintered for 2 h at different temperatures (1475 degrees C, 1500 degrees C, 1550 degrees C, or 1600 degrees C). After sintering, they were characterized by relative density using the ASTM C373-88 standard, X-ray diffraction (XRD) and scanning electron microscopy (SEM). The average grain size was measured according to the ASTM E1382-97 standard. The fracture toughness (K-IC) was determined using two methods: Vickers indentation fracture toughness (KIC-IF): method based on mathematical modeling that considers the parameters used for the Vickers hardness test and Fracture toughness by the single-edge-V-notch-beam (KIC-SEVNB): method proposed by ISO 23146:08. The main phases of the 3Y-TZP and 5Y-PSZ ceramics were ZrO2-tetragonal and ZrO2-cubic, respectively. The 3Y-TZP specimens showed equiaxed grains with average grain sizes ranging from 0.55 to 0.79 mu m. The grain sizes of 5Y-PSZ of specimens sintered at 1475 degrees C and 1600 degrees C were 0.62 and 2.32 mu m, respectively. For all ceramics the crack size ratio was c/a < 2.5, suggesting a Palmqvist-type crack system. The fracture toughness measured by the Vickers indentation method (KIC-IF) and by the SEVNB method (KIC-SEVNB) was the same when the experimental data were fit to a mathematical model.
引用
收藏
页码:103 / 116
页数:14
相关论文
共 50 条
[1]  
American Society for Testing and Materials, 2019, C1327 ASTM
[2]  
[Anonymous], 2015, E138297 ASTM
[3]  
[Anonymous], 2008, IMPL SURG CER MAT BA
[4]  
ASTM, 2006, C37388 ASTM, P1
[5]  
Barsoum M.W., 2003, Fundamentals of Ceramics
[6]   Toughening of yttria-stabilised tetragonal zirconia ceramics [J].
Basu, B .
INTERNATIONAL MATERIALS REVIEWS, 2005, 50 (04) :239-256
[7]   Transformation behaviour of tetragonal zirconia: role of dopant content and distribution [J].
Basu, B ;
Vleugels, J ;
Van Der Biest, O .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 366 (02) :338-347
[8]   GRAIN-SIZE-DEPENDENT TRANSFORMATION BEHAVIOR IN POLYCRYSTALLINE TETRAGONAL ZIRCONIA [J].
BECHER, PF ;
SWAIN, MV .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (03) :493-502
[9]   The influence of yttrium-segregation-dependent phase partitioning and residual stresses on the aging and fracture behaviour of 3Y-TZP ceramics [J].
Bucevac, Dusan ;
Kosmac, Tomaz ;
Kocjan, Andraz .
ACTA BIOMATERIALIA, 2017, 62 :306-316
[10]   Aging resistance, mechanical properties and translucency of different yttria-stabilized zirconia ceramics for monolithic dental crown applications [J].
Camposilvan, E. ;
Leone, R. ;
Gremillard, L. ;
Sorrentino, R. ;
Zarone, F. ;
Ferrari, M. ;
Chevalier, J. .
DENTAL MATERIALS, 2018, 34 (06) :879-890