摘要
High-temperature design evaluations were conducted on Type 316L stainless steel piping for a 700 degrees C large-capacity thermal energy storage verification test loop (TESET) under construction at KAERI. The hot leg piping with sodium coolant at 700 degrees C connects the main components of the loop heater, hot storage tank, and air-to-sodium heat exchanger. Currently, the design rules of ASME B31.1 and RCC-MRx provide design procedures for high-temperature piping in the creep range for Type 316L stainless steel. However, the design material properties around 700 degrees C are not available in those rules. Therefore, a number of material tests, including creep tests at various temperatures, were conducted to determine the insufficient material properties and relevant design coefficients so that high-temperature design on the 700 degrees C piping may be possible. It was shown that Type 316L stainless steel can be used in a 700 degrees C hightemperature piping system of Generation IV reactor systems or a renewable energy systems, such as thermal energy storage systems, for a limited operation time. (c) 2023 Korean Nuclear Society, Published by Elsevier Korea LLC. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:3581 / 3590
页数:10
相关论文
共 50 条
  • [31] Statistical Properties of High Temperature Low Cycle Fatigue Data of Type 316L Stainless Steel
    Oh, Sae-Hee
    Kim, Seon-Jin
    TRANSACTIONS OF THE KOREAN SOCIETY OF MECHANICAL ENGINEERS A, 2024, 48 (12) : 823 - 830
  • [32] Effect of nitrogen on high temperature low cycle fatigue behaviors in type 316L stainless steel
    Kim, DW
    Ryu, WS
    Hong, JH
    Choi, SK
    JOURNAL OF NUCLEAR MATERIALS, 1998, 254 (2-3) : 226 - 233
  • [33] High-cycle fatigue behavior of type 316L stainless steel
    Huang, JY
    Yeh, JJ
    Jeng, SL
    Chen, CY
    Kuo, RC
    MATERIALS TRANSACTIONS, 2006, 47 (02) : 409 - 417
  • [34] 316L stainless steel designed to withstand intermediate temperature
    Saeidi, K.
    Neikter, M.
    Olsen, J.
    Shen, Zhijian James
    Akhtar, F.
    MATERIALS & DESIGN, 2017, 135 : 1 - 8
  • [35] Gelcasting of 316L stainless steel
    Li, Yan
    Guo, Zhimeng
    Hao, Junjie
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2007, 14 (06): : 507 - 511
  • [36] Effect of heat treatment on corrosion behaviour of additively manufactured 316L stainless steel in high-temperature water
    Xiao, Qian
    Chen, Junjie
    Lee, Hyeon Bae
    Jang, Changheui
    Jang, Kyungnam
    CORROSION SCIENCE, 2023, 210
  • [37] Sintering atmosphere and temperature effects on hydroxyapatite coated type 316L stainless steel
    Sridhar, TM
    Mudali, UK
    Subbaiyan, M
    CORROSION SCIENCE, 2003, 45 (10) : 2337 - 2359
  • [38] Corrosion Behaviour of Plasma-Sprayed Nickel Coating on Type 316L Stainless Steel in High-Temperature Molten FLiNaK Salt
    Y. V. Harinath
    Ch. Jagadeeswara Rao
    S. Ningshen
    T. V. Krishna Mohan
    S. Rangarajan
    Shaju K. Albert
    Transactions of the Indian Institute of Metals, 2021, 74 : 2821 - 2833
  • [39] Microstructure and corrosion resistance of a type 316L stainless steel
    Shieu, FS
    Deng, MJ
    Lin, SH
    CORROSION SCIENCE, 1998, 40 (08) : 1267 - 1279
  • [40] INTERGRANULAR CORROSION OF TYPE 316L STAINLESS-STEEL
    DILLON, CP
    MATERIALS PERFORMANCE, 1995, 34 (03) : 62 - 63