Molybdenum disulfide/carbon multilayer films achieve ultra-low wear in vacuum

被引:1
|
作者
Cheng, Zhiqiang [1 ,2 ]
Wei, Xiaoli [3 ]
Gao, Kaixiong [2 ,4 ]
Li, Chunyan [1 ,5 ]
机构
[1] Lanzhou Univ Technol, Sch Mat Sci & Engn, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou, Peoples R China
[2] Chinese Acad Sci, Lanzhou Inst Chem Phys, Key Lab Sci & Technol Wear & Protect Mat, Lanzhou, Peoples R China
[3] Lanzhou Univ Arts & Sci, Sch Chem Engn, Lanzhou, Peoples R China
[4] Chinese Acad Sci, Lanzhou Inst Chem Phys, Key Lab Sci & Technol Wear & Protect Mat, Lanzhou 730000, Peoples R China
[5] Lanzhou Univ Technol, Sch Mat Sci & Engn, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Peoples R China
基金
中国国家自然科学基金;
关键词
DLC; MoS2; vacuum; wear; DIAMOND-LIKE; TRIBOLOGICAL PROPERTIES; CARBON-FILMS; LOW-FRICTION; COATINGS; NANOCOMPOSITE; HUMIDITY;
D O I
10.1002/sia.7241
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Although diamond-like carbon (DLC) films are known for their low friction and wear properties in atmospheric environments, they commonly experience failure in vacuum environments. On the other hand, MoS2 exhibits a low friction coefficient under vacuum conditions, but its columnar structure limits its load-bearing capacity and results in high wear rates. In this study, we prepared MoS2/DLC multilayer films using a high-power impulse magnetron sputtering (HIPIMS) technique and examined the composition, bonding structure, mechanical properties, and frictional wear of the resulting films. The study findings revealed that the multilayer film exhibits a significantly low coefficient of friction (0.04), particularly in vacuum conditions (5 x 10(-3) Pa). Remarkably, compared to the pure MoS2 film, the wear rate of the multilayer film is reduced by two orders of magnitude, wear rate as low as 3.6 x 10(-9) mm(3)/Nm. Additionally, the DLC component enhances the hardness and reduces the wear rate of the multilayer film. Furthermore, the use of nanometer thickness (17 nm) allows for the incorporation of more MoS2 and DLC layers, which promotes the formation of graphene bands and further reduces the friction coefficient and wear rate. Our findings open new avenues for the application of MoS2 and DLC in vacuum environments.
引用
收藏
页码:730 / 739
页数:10
相关论文
共 50 条
  • [21] Leveraging trace nanofillers to engineer ultra-low wear polymer surfaces
    Alam, Kazi Istiaque
    Baratz, Andrew
    Burris, David
    WEAR, 2021, 482
  • [22] Friction and Wear Characteristics in Air of Sputtered Molybdenum Disulfide Films-Introduction Effect of Dry Gas to Vacuum Chamber after Film Formation
    Matsuda, Kenji
    Koguma, Kiyonori
    Kaneta, Motohiro
    Ikeda, Michiaki
    JOURNAL OF JAPANESE SOCIETY OF TRIBOLOGISTS, 2009, 54 (12) : 857 - 864
  • [23] Low-temperature synthesis of uniform monolayer molybdenum disulfide films
    Xu, Donghao
    Lu, Jie
    Lin, Gaoxiang
    Zheng, Miaomiao
    Chen, Yangbo
    Miao, Gesong
    Zhou, Yinghui
    Cai, Weiwei
    Zhang, Yufeng
    Wang, Yan
    Zhang, Xueao
    APPLIED PHYSICS LETTERS, 2024, 124 (03)
  • [24] Extremely high wear resistance and ultra-low friction behaviour of oxygen-plasma-treated nanocrystalline diamond films
    Radhika, R.
    Kumar, N.
    Sankaran, K. J.
    Dumpala, Ravikumar
    Dash, S.
    Rao, M. S. Ramachandra
    Arivuoli, D.
    Tyagi, A. K.
    Tai, N. H.
    Lin, I-Nan
    JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2013, 46 (42)
  • [25] Ultra-low friction and excellent elastic recovery of fullerene-like hydrogenated carbon film based on multilayer design
    Yanshuang Meng
    Xiaolong Jia
    Fuliang Zhu
    Junyan Zhang
    Bulletin of Materials Science, 2017, 40 : 1029 - 1034
  • [26] Nanostructured Carbon-Titanium multilayer films obtained by Thermionic Vacuum Arc method
    Ciupina, Victor
    Lungu, Cristian P.
    Vladoiu, Rodica
    Prodan, Gabriel C.
    Porosnicu, Corneliu
    Vasile, Eugeniu
    Prodan, Madalina
    Nicolescu, Virginia
    Mandes, Aurelia
    Dinca, Virginia
    Cupsa, Ovidiu
    NANOSTRUCTURED THIN FILMS XI, 2018, 10731
  • [27] Effect of exfoliated molybdenum disulfide oxide on friction and wear properties of ultra high molecular weight polyethylene
    Amini, Majed
    Ramazani, Ahmad S. A.
    Varjouy, Ali Afkhami
    Faghihi, Morteza
    POLYMERS FOR ADVANCED TECHNOLOGIES, 2018, 29 (12) : 3085 - 3096
  • [28] Synergistic effect of graphene and nanodiamonds to achieve ultra-low friction on rough DLC coatings
    Mescola, Andrea
    Lodi, Alessia
    Zanni, Federico
    Rota, Alberto
    Gerbi, Andrea
    Bernini, Cristina
    Schott, Marine
    Repetto, Luca
    Camisasca, Adalberto
    Giordani, Silvia
    Buzio, Renato
    Paolicelli, Guido
    DIAMOND AND RELATED MATERIALS, 2024, 145
  • [29] TiMoN nano-grains embedded into thin MoSx-based amorphous matrix: A novel structure for superhardness and ultra-low wear
    Yang, Lina
    Wen, Mao
    Chen, Jianhong
    Wang, Jia
    Dai, Xuan
    Gu, Xinlei
    Cui, Xiaoqiang
    Zhang, Kan
    APPLIED SURFACE SCIENCE, 2018, 462 : 127 - 133
  • [30] Is Ultra-Low Friction Needed to Prevent Wear of Diamond-Like Carbon (DLC)? An Alcohol Vapor Lubrication Study for Stainless Steel/DLC Interface
    Matthew J. Marino
    Erik Hsiao
    Laura C. Bradley
    Osman L. Eryilmaz
    Ali Erdemir
    Seong H. Kim
    Tribology Letters, 2011, 42