Coupling effect of thermal aging and pre-strain on fracture behavior of SMAW welded joints

被引:3
作者
Wang, Chunhui [1 ,2 ]
Fan, Minyu [3 ]
Yu, Min [3 ]
Yu, Weiwei [3 ]
Liu, Zheng [1 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Daya Bay Nucl Power Operat & Management Co Ltd, Shenzhen 518120, Peoples R China
[3] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
关键词
SMAW welded joints; Pre-strain; Thermal aging; Fracture toughness; Charpy impact test; DUPLEX STAINLESS-STEELS; MECHANICAL-PROPERTIES; DIFFERENT LOCATIONS; TOUGHNESS; EMBRITTLEMENT; MICROSTRUCTURE; TIG;
D O I
10.1016/j.engfracmech.2023.109224
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A repairing process is commonly needed to correct installation slope and geometrical deviation of nuclear power piping, but the resulting pre-strain has obvious degradation impacts on the long-term operation of surge pipeline, especially for the shielded metal arc welding (SMAW) joints. In this paper, to investigate the embrittlement induced by thermal aging and pre-strain, the SMAW welded joints with the base metal Z2CND18-12N2 and welded metal ER316L were subjected to different pre-strain (0%, 8%, 12% and 15%) and the accelerated thermal aging from 0 h to 13000 h at 400 celcius. Then, the Charpy impact test and compact tension fracture test were conducted to determine fracture properties of the SMAW welded joints. Results showed that both thermal aging and pre-strain can significantly reduce the fracture properties of SMAW welded joints. The impact absorbed energy reached stable after thermal aging 500 h, but it has been decreasing with the pre-strain varying from 0% to 15%. Moreover, it is shown that for pre-strained SMAW welded joints, with the increase of thermal aging duration, the absorbed energy first recovers, and then de-creases until stable. Compared with pre-strain, the influence of thermal aging is dominant. Finally, combined with microscopic analysis, the comprehensive effects of thermal aging and pre-strain on the embrittlement mechanism of SMAW welded joints were discussed.
引用
收藏
页数:14
相关论文
共 50 条
[31]   Effect of Tensile Pre-strain on Mechanical Properties of Austenitic 301 Stainless Steel [J].
Xu, Jingsheng ;
Wang, ManFu .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2024, 33 (22) :12721-12728
[32]   Effect of pre-strain path on suppression of abnormal grain growth in friction-stir welded 6061 aluminum alloy [J].
Vysotskiy, Igor ;
Malopheyev, Sergey ;
Mironov, Sergey ;
Kaibyshev, Rustam .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 760 :206-213
[33]   Effects of Pre-Strain on the Aging Behavior of Al 7075 Alloy for Hot-Stamping Capability [J].
Jung, Seon-Ho ;
Lee, Jongsup ;
Kawasaki, Megumi .
METALS, 2018, 8 (02)
[34]   Effect of pre-strain on compression mode properties of magnetorheological elastomers [J].
Vatandoost, Hossein ;
Sedaghati, Ramin ;
Rakheja, Subhash ;
Hemmatian, Masoud .
POLYMER TESTING, 2021, 93
[35]   Effect of pre-strain on hydrogen-induced delayed cracking and hydrogen trapping behavior in high-strength martensitic steels [J].
Li, Weiguo ;
Cao, Zhongqian ;
Yang, Zixuan ;
Zhou, Qingjun ;
Li, Jinxu .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 91 :470-487
[36]   Effect of thermal aging on metallurgical, tensile and impact toughness performance of electron beam welded AISI 316 SS joints [J].
Kumar, Arun ;
Singh, Beant ;
Sandhu, Sandeep Singh .
FUSION ENGINEERING AND DESIGN, 2020, 159
[37]   Effect of torsional pre-strain on low cycle fatigue performance of 304 stainless steel [J].
Ji, Shengyuan ;
Liu, Caiming ;
Li, Yajing ;
Shi, Shouwen ;
Chen, Xu .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 746 :50-57
[38]   Long term ageing effect on fracture toughness of the GTAW welded joints for nuclear power main pipelines [J].
Wu, Songwei ;
Zhang, Zhe .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2020, 188
[39]   Effect of Pre-strain Aging on the Damage Properties of Composite Solid Propellants based on a Constitutive Equation [J].
Zhou, Dongmo ;
Liu, Xiangyang ;
Sui, Xin ;
Wei, Zhijun ;
Wang, Ningfei .
PROPELLANTS EXPLOSIVES PYROTECHNICS, 2017, 42 (04) :430-437
[40]   Effect of small pre-strain on the resistance of molybdenum [100] single crystal to high strain rate deformation and fracture [J].
Kanel, G. I. ;
Garkushin, G. V. ;
Savinykh, A. S. ;
Razorenov, S. V. ;
Paramonova, I. V. ;
Zaretsky, E. B. .
JOURNAL OF APPLIED PHYSICS, 2022, 131 (09)