Coupling effect of thermal aging and pre-strain on fracture behavior of SMAW welded joints

被引:3
作者
Wang, Chunhui [1 ,2 ]
Fan, Minyu [3 ]
Yu, Min [3 ]
Yu, Weiwei [3 ]
Liu, Zheng [1 ]
Chen, Xu [1 ]
机构
[1] Tianjin Univ, Sch Chem Engn & Technol, Tianjin 300072, Peoples R China
[2] Daya Bay Nucl Power Operat & Management Co Ltd, Shenzhen 518120, Peoples R China
[3] Suzhou Nucl Power Res Inst, Suzhou 215004, Peoples R China
关键词
SMAW welded joints; Pre-strain; Thermal aging; Fracture toughness; Charpy impact test; DUPLEX STAINLESS-STEELS; MECHANICAL-PROPERTIES; DIFFERENT LOCATIONS; TOUGHNESS; EMBRITTLEMENT; MICROSTRUCTURE; TIG;
D O I
10.1016/j.engfracmech.2023.109224
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
A repairing process is commonly needed to correct installation slope and geometrical deviation of nuclear power piping, but the resulting pre-strain has obvious degradation impacts on the long-term operation of surge pipeline, especially for the shielded metal arc welding (SMAW) joints. In this paper, to investigate the embrittlement induced by thermal aging and pre-strain, the SMAW welded joints with the base metal Z2CND18-12N2 and welded metal ER316L were subjected to different pre-strain (0%, 8%, 12% and 15%) and the accelerated thermal aging from 0 h to 13000 h at 400 celcius. Then, the Charpy impact test and compact tension fracture test were conducted to determine fracture properties of the SMAW welded joints. Results showed that both thermal aging and pre-strain can significantly reduce the fracture properties of SMAW welded joints. The impact absorbed energy reached stable after thermal aging 500 h, but it has been decreasing with the pre-strain varying from 0% to 15%. Moreover, it is shown that for pre-strained SMAW welded joints, with the increase of thermal aging duration, the absorbed energy first recovers, and then de-creases until stable. Compared with pre-strain, the influence of thermal aging is dominant. Finally, combined with microscopic analysis, the comprehensive effects of thermal aging and pre-strain on the embrittlement mechanism of SMAW welded joints were discussed.
引用
收藏
页数:14
相关论文
共 50 条
[21]   Effect of pre-strain on fracture toughness of ductile structural steels under static and dynamic loading [J].
Qiu, H ;
Enoki, M ;
Hiraoka, K ;
Kishi, T .
ENGINEERING FRACTURE MECHANICS, 2005, 72 (10) :1624-1633
[22]   Multistage strain aging phenomenon of low-carbon steels with rolling pre-strain [J].
Rizehvandy, Sirous .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 15 :7136-7144
[23]   The Effect of Pre-Strain on Microalloyed Steel Weld Metal in the Presence of Hydrogen [J].
Khatib Zadeh Davani, Reza ;
Miresmaeili, Reza .
TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2022, 75 (02) :565-576
[24]   Effect of pre-strain on the strength of spot-welds [J].
Mukhopadhyay, G. ;
Bhattacharya, S. ;
Ray, K. K. .
MATERIALS & DESIGN, 2009, 30 (07) :2345-2354
[25]   Effect of pre-strain on the fatigue behavior of SAPH440 steel [J].
Zhao, Li-Hui ;
Cai, Hong-Chang ;
Weng, Shuo ;
Zheng, Song-Lin .
MATERIALS EXPRESS, 2019, 9 (09) :1001-1008
[26]   Influence of pre-strain on the aging hardening effect of the Mg-9.02Zn-1.68Y alloy [J].
Ye, Jie ;
Lin, Xiao-ping ;
Zhao, Tian-bo ;
Liu, Ning-ning ;
Xie, Hong-bin ;
Niu, Yi ;
Teng, Fei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 663 :49-55
[27]   Thermal aging effect on the tensile and fatigue properties of the narrow-gap TIG welded joints in offshore floating nuclear power plants [J].
Yu, Weiwei ;
Fan, Minyu ;
Jia, Wenqing ;
Xue, Fei ;
Yu, Min ;
Liu, Hui ;
Chen, Xu .
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 126 :143-154
[28]   Effect of Pre-Strain on The Longitudinal Residual Strain of Dissimilar Metal Welded Between Stainless Steel and Carbon Steel [J].
Pambudi, Susilo Luhur ;
Triyono ;
Muslih, M. Refai ;
Muhayat, Nurul .
PROCEEDINGS OF THE 2014 INTERNATIONAL CONFERENCE ON PHYSICS AND ITS APPLICATIONS, 2015, :165-170
[29]   Effect of pre-strain on hydrogen induced cracking of PAW welded 304 austenitic stainless steel [J].
Zhou, Chilou ;
Ren, Yingjie ;
Yokogawa, Kiyoshi ;
Xue, Jinxin ;
Li, Xiang .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2024, 54 :713-728
[30]   Effect of pre-strain on fatigue crack growth behavior for commercial pure titanium at ambient temperature [J].
Li, Jian ;
Zhang, Peng ;
Lu, Lei ;
Lv, Fei ;
Miao, Xin-Ting ;
Chang, Le ;
Zhou, Bin-Bin ;
He, Xiao-Hua ;
Zhou, Chang-Yu .
INTERNATIONAL JOURNAL OF FATIGUE, 2018, 117 :27-38