Failure analysis of corroded heat exchanger CuNi tubes from a geothermal plant

被引:11
作者
Morake, Joseph B. [1 ]
Mutua, James M. [1 ]
Ruthandi, Martin M. [1 ]
Olakanmi, Eyitayo O. [2 ,3 ,4 ]
Botes, Annelize [5 ]
机构
[1] Jomo Kenyatta Univ Agr & Technol JKUAT, Sch Mech Mfg & Mat Engn, Nairobi, Kenya
[2] Botswana Int Univ Sci & Technol BIUST, Dept Mech Energy & Ind Engn, Palapye, Botswana
[3] Botswana Int Univ Sci & Technol, UNESCO Chair Sustainable Mfg & Innovat Technol UCo, Palapye, Botswana
[4] Botswana Int Univ Sci & Technol, Adv Mfg & Engn Educ AMEE Res Grp, Palapye, Botswana
[5] Nelson Mandela Univ, Dept Mech Engn, Port Elizabeth, South Africa
关键词
Heat exchanger; Cupronickel; Hydrogen embrittlement; Sulfide stress cracking; Tube wear; STRESS-CORROSION CRACKING; COPPER;
D O I
10.1016/j.engfailanal.2023.107543
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This study examined the premature failure of cupronickel (CuNi10Fe) tubes in a shell-and-tube heat exchanger after five months of service. An investigation to identify the root cause of the tube burst was carried out using macroscopic and microscopic inspection, chemical analysis, and mechanical analysis. The optical microscopy (OM) and scanning electron microscopy (SEM) evaluation revealed crack propagation characterized by pits and inclusions at the tube surface. This was due to the diffusion of hydrogen ions into the material from the hydrogen sulfide (H2S) rich geothermal environment. Furthermore, high tensile residual stresses of 172 MPa were recorded in the failed tube, leading to stress cracking in hydrogen-containing material. Additionally, the high sulfide content in corroded water and condensate samples suggests that the leading cause of tube rupture was through hydrogen embrittlement and sulfide stress cracking mechanism in the presence of hydrogen sulfide. Therefore, the use of laser cladding to protect tubes using functionally graded materials is recommended to mitigate degradation in aggressive environments, through careful material selection and additional water treatment to eliminate the contaminants.
引用
收藏
页数:15
相关论文
共 26 条
[11]   Influence of the Hydrogen Sulfide Concentration on the Corrosion and Hydrogenation of Pipe Steels (A Survey) [J].
Khoma, M. S. ;
Vasyliv, Kh B. ;
Chuchman, M. R. .
MATERIALS SCIENCE, 2021, 57 (03) :308-318
[12]   Erosion-corrosion of heat exchanger tubes [J].
Kuznicka, B. .
ENGINEERING FAILURE ANALYSIS, 2009, 16 (07) :2382-2387
[13]   A metallographic case study of formicary corrosion in heat exchanger copper tubes [J].
Lachowicz, Marzena Malgorzata .
ENGINEERING FAILURE ANALYSIS, 2020, 111
[14]   Influence of H2S on the general corrosion and sulfide stress cracking of pipelines steels for supercritical CO2 transportation [J].
Li, Kaiyang ;
Zeng, Yimin ;
Luo, Jing-Li .
CORROSION SCIENCE, 2021, 190
[15]   A microstructural aspect of intergranular stress corrosion cracking of semi-hard U-bend tubes of commercially pure copper in cooling systems [J].
Miyamoto, H. ;
Saburi, D. ;
Fujiwara, H. .
ENGINEERING FAILURE ANALYSIS, 2012, 26 :108-119
[16]   Effects of Different Parameters on Initiation and Propagation of Stress Corrosion Cracks in Pipeline Steels: A Review [J].
Mohtadi-Bonab, M. A. .
METALS, 2019, 9 (05)
[17]   Failure analysis of a shell and tube oil cooler [J].
Mousavian, R. Taherzadeh ;
Hajjari, E. ;
Ghasemi, D. ;
Manesh, M. Kojouri ;
Ranjbar, K. .
ENGINEERING FAILURE ANALYSIS, 2011, 18 (01) :202-211
[18]  
Tuck C.D.S., 2016, Corrosion of Copper and Its Alloys $, DOI [10.1016/B978-0-12-803581-8.01634-9, DOI 10.1016/B978-0-12-803581-8.01634-9]
[19]   Failure analysis of heat exchanger tubes [J].
Usman, A. ;
Khan, A. Nusair .
ENGINEERING FAILURE ANALYSIS, 2008, 15 (1-2) :118-128
[20]   Study on Stress Corrosion Cracking Behavior of Incoloy825/X65 Bimetallic Composite Pipe Welded Joint in Wet Hydrogen Sulfide Environment [J].
Wang, Bingying ;
Ouyang, Li ;
Xu, Jianxing ;
Huang, Peng ;
Liu, Enyang ;
Yang, Bin .
METALS, 2022, 12 (04)