Ti-48Al-2Cr-2Nb alloys prepared by electron beam selective melting additive manufacturing: Microstructural and tensile properties

被引:8
作者
Feng, Jiawen [1 ]
Gui, Wanyuan [1 ]
Liu, Qian [1 ]
Bi, Wenya [1 ]
Ren, Xuechong [1 ]
Liang, Yongfeng [2 ]
Lin, Junpin [2 ]
Luan, Benli [1 ,3 ]
机构
[1] Univ Sci & Technol Beijing, Natl Ctr Mat Serv Safety, Beijing 100083, Peoples R China
[2] Univ Sci & Technol Beijing, State Key Lab Adv Met & Mat, Beijing 100083, Peoples R China
[3] Western Univ, Dept Chem, London, ON N6A 5B7, Canada
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 26卷
关键词
Electron beam selective melting; TiAl alloys; Microstructure evolution; Phase transformation; Mechanical properties; TIAL ALLOY; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; HIGH NIOBIUM; HIGH NB; BEHAVIOR; PHASE; TRANSFORMATION; TEXTURE;
D O I
10.1016/j.jmrt.2023.09.267
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Here, an electron beam selective melting (EBM) technique was employed to shape Ti-48Al-2Cr-2Nb alloy to combat its intrinsic brittleness and insufficient hot workability. Through process optimization, high-density samples (4.2327 g/cm3) were produced. First, the mechanism of interaction between phase transformation and microstructural evolution of EBM-formed Ti-48Al-2Cr-2Nb alloy was investigated using scanning electron microscopy (SEM), X-ray diffraction (XRD), and electron backscattering diffraction (EBSD). And then, the mechanism of interaction between tensile properties and microstructural evolution of EBM-formed Ti-48Al-2Cr-2Nb alloy was discussed. Based on the results, the microstructure consists of coarse equiaxed grains and fine lamellar grains, which gradually coarsen from upper to bottom. As the thickness of the layer increases from upper to bottom, the content of the B2 phase increases continuously, with a predominant component of TiAl and a small amount of Ti3Al and B2 phases. The majority of the g-TiAl phase does not exhibit significant texture, while the a2-Ti3Al phase shows a texture of (0001) with 19.32 times the random intensity, and its c-axis is parallel to the deposition direction. Benefiting from its unique structure features, the maximum room temperature tensile strength of as-deposited Ti-48Al-2Nb-2Cr alloy reaches 854.6 MPa with an elongation of over 2%. And the maximum high -temperature tensile strength of EBM-formed Ti-48Al-2Nb-2Cr alloy reaches 707 MPa at 650 degrees C with an elongation over 3.5%. According to these results, the mechanical properties of our EBM Ti-48Al-2Cr-2Nb alloy are superior to those previously reported. (c) 2023 The Author(s). Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:9357 / 9369
页数:13
相关论文
共 43 条
  • [11] In-situ study of the time-temperature-transformation behaviour of a multi-phase intermetallic β-stabilised TiAl alloy
    Erdely, Petra
    Werner, Robert
    Schwaighofer, Emanuel
    Clemens, Helmut
    Mayer, Svea
    [J]. INTERMETALLICS, 2015, 57 : 17 - 24
  • [12] [高润奇 Gao Runqi], 2022, [航空材料学报, Journal of Aeronautical Materials], V42, P91
  • [13] Gong XB, 2013, PROCEEDINGS OF THE ASME/ISCIE INTERNATIONAL SYMPOSIUM ON FLEXIBLE AUTOMATION, ISFA 2012, P507
  • [14] Microstructure stability of γ-TiAl produced by selective laser melting
    Gussone, J.
    Garces, G.
    Haubrich, J.
    Stark, A.
    Hagedorn, Y. -C.
    Schell, N.
    Requena, G.
    [J]. SCRIPTA MATERIALIA, 2017, 130 : 110 - 113
  • [15] Microstructure characterization and tensile properties of a Ni-containing TiAl-based alloy with heat treatment
    Han, Jian-Chao
    Xiao, Shu-Long
    Tian, Jing
    Chen, Yu-Yong
    Xu, Li-Juan
    Wang, Xiao-Peng
    Jia, Yi
    Cao, Shou-Zhen
    [J]. RARE METALS, 2016, 35 (01) : 26 - 34
  • [16] Processing-property-microstructure relationships in TiAl-based alloys
    Hu, D
    Godfrey, A
    Blenkinsop, PA
    Loretto, MH
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1998, 29 (3A): : 919 - 925
  • [17] Thermal exposure induced α2+γ→B2(ω) and α2→B2(ω) phase transformations in a high Nb fully lamellar TiAl alloy
    Huang, ZW
    Voice, W
    Bowen, P
    [J]. SCRIPTA MATERIALIA, 2003, 48 (01) : 79 - 84
  • [18] Rapid manufacturing of metallic objects
    Karunakaran, K. P.
    Bernard, Alain
    Suryakumar, S.
    Dembinski, Lucas
    Taillandier, Georges
    [J]. RAPID PROTOTYPING JOURNAL, 2012, 18 (04) : 264 - 280
  • [19] Characterization of hot deformation behavior of as-forged TiAl alloy
    Kong, Fantao
    Cui, Ning
    Chen, Yuyong
    Wang, Xiaopeng
    Xiong, Ningning
    [J]. INTERMETALLICS, 2014, 55 : 66 - 72
  • [20] Microstructure and mechanical properties of large size as-cast Ti-43Al-9V-0.2Y (at.%) alloy ingot from brim to centre
    Kong, Fantao
    Xu, Xingchen
    Chen, Yuyong
    Zhang, Deliang
    [J]. MATERIALS & DESIGN, 2012, 33 : 485 - 490