Corrosion Inhibition Mechanism of Ultra-High-Temperature Acidizing Corrosion Inhibitor for 2205 Duplex Stainless Steel

被引:6
作者
Li, Danping [1 ,2 ]
Song, Wenwen [3 ]
Zhang, Junping [4 ]
Yin, Chengxian [1 ]
Zhao, Mifeng [3 ]
Chao, Hongzhou [3 ]
Zhang, Juantao [1 ]
Lei, Zigang [1 ,2 ]
Fan, Lei [1 ]
Liu, Wan [1 ,2 ]
Li, Xiaolong [1 ]
机构
[1] CNPC, Tubular Goods Res Inst, Xian 710077, Peoples R China
[2] Xian Dexincheng Technol Co Ltd, Xian 710075, Peoples R China
[3] PetroChina Tarim Oilfield Co, Korla 841000, Peoples R China
[4] Northwestern Polytech Univ, Sch Chem & Chem Engn, Xian 710082, Peoples R China
关键词
duplex stainless steel; selective corrosion; high-temperature acidification; corrosion inhibitor; molecular dynamics simulation; MOLECULAR-DYNAMICS SIMULATION; SELECTIVE DISSOLUTION; ADSORPTION BEHAVIOR; GALVANIC CORROSION; MEDIUM DIFFUSION; MICROSTRUCTURE; PHASES;
D O I
10.3390/ma16062358
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The acidizing corrosion inhibitors reported so far have a poor effect on duplex stainless steel in high-temperature and high-concentration acid systems and cannot effectively inhibit the occurrence of selective corrosion. In this paper, a new acidizing corrosion inhibitor was designed, which was mainly composed of Mannich base and antimony salt. The inorganic substance in the corrosion inhibitor had good stability at high temperatures and could quickly form a complex with the metal matrix to enhance the binding ability. The organic substance can make up for the non-dense part of the inorganic film. The properties of developed corrosion inhibitors were analyzed by quantum chemical calculation, molecular dynamics simulation, and scanning electron microscopy. The results showed that a double-layer membrane structure could be constructed after adding the corrosion inhibitor, which could play a good role in blocking the diffusion of acid solution at high-temperature. The uniform corrosion rate of 2205 duplex stainless steel after adding acidizing corrosion inhibitor immersion in a simulated service condition (9 wt.% HCl + 1.5 wt.% HF + 3 wt.% CH3COOH + 4 similar to 6 wt.%) at 140 degrees C, 160 degrees C and 180 degrees C for a 4 h test is 6.9350 g center dot m(-2)center dot h(-1), 6.3899 g center dot m(-2)center dot h(-1) and 12.1881 g center dot m(-2)center dot h(-1), respectively, which shows excellent corrosion inhibition effect and is far lower than that of the commonly accepted 81 g center dot m(-2)center dot h(-1) and no selective corrosion could be detected.
引用
收藏
页数:19
相关论文
共 50 条
  • [41] The effect of phase transformation route on the intergranular corrosion susceptibility of 2205 duplex stainless steel
    Haghdadi, Nima
    Laleh, Majid
    Kosari, Ali
    Moayed, M. H.
    Cizek, Pavel
    Hodgson, Peter D.
    Beladi, Hossein
    MATERIALS LETTERS, 2019, 238 : 26 - 30
  • [42] Cavitation corrosion of duplex stainless steel in seawater
    AlHashem, A
    Caceres, PG
    Abdullah, A
    Shalaby, HM
    CORROSION, 1997, 53 (02) : 103 - 113
  • [43] Improved Surface Morphology and Corrosion Resistance Performance of 2205 Duplex Stainless Steel by Low Temperature Gas Nitriding
    Dan N.E.
    Hussain P.B.
    Shaik N.B.
    Bakthavatchalam B.
    Mohapatra R.K.
    Behera A.
    Journal of Bio- and Tribo-Corrosion, 2022, 8 (4)
  • [44] Probing propensity of grade 2205 duplex stainless steel towards atmospheric chloride-induced stress corrosion cracking
    Engelberg, D. L.
    Ornek, C.
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2014, 49 (06) : 535 - 539
  • [45] Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel
    Qi Sun
    Jian Wang
    Hua-bing Li
    Yue Li
    Ya-di Hu
    Jin-gang Bai
    Pei-de Han
    Journal of Iron and Steel Research International, 2016, 23 : 1071 - 1079
  • [46] Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel
    Qi SUN
    Jian WANG
    Hua-bing LI
    Yue LI
    Ya-di HU
    Jin-gang BAI
    Pei-de HAN
    JournalofIronandSteelResearch(International), 2016, 23 (10) : 1071 - 1079
  • [47] Microstructure and corrosion resistance of welding seam of SAF 2205 duplex stainless steel by different welding materials
    Li, JC
    Zhao, M
    Jiang, Q
    CORROSION REVIEWS, 2004, 22 (02) : 115 - 125
  • [48] Chi Phase after Short-term Aging and Corrosion Behavior in 2205 Duplex Stainless Steel
    Sun, Qi
    Wang, Jian
    Li, Hua-bing
    Li, Yue
    Hu, Ya-di
    Bai, Jin gang
    de Han, Pei
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (10) : 1071 - 1079
  • [49] MECHANISM OF INTERGRANULAR CORROSION AND PITTING CORROSION OF AUSTENITIC AND DUPLEX 308 STAINLESS-STEEL
    DEVINE, TM
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (03) : 374 - 385
  • [50] Galvanic corrosion between the constituent phases in duplex stainless steel
    Tsai, Wen-Ta
    Chen, Jhen-Rong
    CORROSION SCIENCE, 2007, 49 (09) : 3659 - 3668