Corrosion Inhibition Mechanism of Ultra-High-Temperature Acidizing Corrosion Inhibitor for 2205 Duplex Stainless Steel

被引:6
作者
Li, Danping [1 ,2 ]
Song, Wenwen [3 ]
Zhang, Junping [4 ]
Yin, Chengxian [1 ]
Zhao, Mifeng [3 ]
Chao, Hongzhou [3 ]
Zhang, Juantao [1 ]
Lei, Zigang [1 ,2 ]
Fan, Lei [1 ]
Liu, Wan [1 ,2 ]
Li, Xiaolong [1 ]
机构
[1] CNPC, Tubular Goods Res Inst, Xian 710077, Peoples R China
[2] Xian Dexincheng Technol Co Ltd, Xian 710075, Peoples R China
[3] PetroChina Tarim Oilfield Co, Korla 841000, Peoples R China
[4] Northwestern Polytech Univ, Sch Chem & Chem Engn, Xian 710082, Peoples R China
关键词
duplex stainless steel; selective corrosion; high-temperature acidification; corrosion inhibitor; molecular dynamics simulation; MOLECULAR-DYNAMICS SIMULATION; SELECTIVE DISSOLUTION; ADSORPTION BEHAVIOR; GALVANIC CORROSION; MEDIUM DIFFUSION; MICROSTRUCTURE; PHASES;
D O I
10.3390/ma16062358
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The acidizing corrosion inhibitors reported so far have a poor effect on duplex stainless steel in high-temperature and high-concentration acid systems and cannot effectively inhibit the occurrence of selective corrosion. In this paper, a new acidizing corrosion inhibitor was designed, which was mainly composed of Mannich base and antimony salt. The inorganic substance in the corrosion inhibitor had good stability at high temperatures and could quickly form a complex with the metal matrix to enhance the binding ability. The organic substance can make up for the non-dense part of the inorganic film. The properties of developed corrosion inhibitors were analyzed by quantum chemical calculation, molecular dynamics simulation, and scanning electron microscopy. The results showed that a double-layer membrane structure could be constructed after adding the corrosion inhibitor, which could play a good role in blocking the diffusion of acid solution at high-temperature. The uniform corrosion rate of 2205 duplex stainless steel after adding acidizing corrosion inhibitor immersion in a simulated service condition (9 wt.% HCl + 1.5 wt.% HF + 3 wt.% CH3COOH + 4 similar to 6 wt.%) at 140 degrees C, 160 degrees C and 180 degrees C for a 4 h test is 6.9350 g center dot m(-2)center dot h(-1), 6.3899 g center dot m(-2)center dot h(-1) and 12.1881 g center dot m(-2)center dot h(-1), respectively, which shows excellent corrosion inhibition effect and is far lower than that of the commonly accepted 81 g center dot m(-2)center dot h(-1) and no selective corrosion could be detected.
引用
收藏
页数:19
相关论文
共 50 条
  • [31] The effect of plasma nitriding on the synergism between wear and corrosion of SAF 2205 duplex stainless steel
    Nunez, Yamid
    Mafra, Marcio
    Morales, Rigoberto E.
    Borges, Paulo Cesar
    Pintaude, Giuseppe
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2020, 72 (09) : 1117 - 1122
  • [32] Alternating voltage induced oscillation on electrochemical behavior and pitting corrosion in duplex stainless steel 2205
    Dai, Nianwei
    Wu, Jun
    Zhang, Lai-Chang
    Sun, Yangting
    Liu, Yuanyuan
    Yang, Yuanyuan
    Jiang, Yiming
    Li, Jin
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (03): : 419 - 433
  • [33] Effect of metastable pitting on stress corrosion cracking in 2205 duplex stainless steel welded joints
    Wang, Dengyun
    Ye, Wenhui
    Zhang, Houwei
    Zheng, Qing
    Su, Hang
    Fu, Anqing
    Xu, Lining
    CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2024,
  • [34] Effect of Thiosulfate on Corrosion Behavior and Passive Films of Duplex Stainless Steel 2205 in Chloride Solutions
    Zhang, Jiantao
    Hu, Xiaojun
    Chou, Kuochih
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2019, 14 (10): : 9960 - 9973
  • [35] Understanding Corrosion Morphology of Duplex Stainless Steel Wire in Chloride Electrolyte
    Ornek, Cem
    Davut, Kemal
    Kocabas, Mustafa
    Bayatli, Aleyna
    Urgen, Mustafa
    CORROSION AND MATERIALS DEGRADATION, 2021, 2 (03) : 397 - 411
  • [36] Corrosion Properties and Impact Toughness of 2205 Duplex Stainless Steel after TIG Welding
    Basyigit, Aziz Baris
    Kurt, Adem
    MATERIALS TESTING, 2014, 56 (10) : 786 - 794
  • [37] Studies on pitting corrosion of 2205 duplex stainless steel induced by sulphate reducing bacteria
    Michalska, Joanna
    Jaworska-Kik, Marzena
    Dzierzewicz, Zofia
    OCHRONA PRZED KOROZJA, 2013, 56 (06): : 250 - 253
  • [38] Effect of solution annealing on the microstructure evolution and corrosion behavior of 2205 duplex stainless steel
    Zhang, Jiantao
    Hu, Xiaojun
    Lin, Ping
    Chou, Kuochih
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (04): : 676 - 687
  • [39] Corrosion behavior of 2205 duplex stainless steel in NaCl solutions containing sulfide ions
    Xiao, Ying
    Tang, Junlei
    Wang, Yingying
    Lin, Bing
    Nie, Zhen
    Li, Yunfei
    Normand, Bernard
    Wang, Hu
    CORROSION SCIENCE, 2022, 200
  • [40] Effect of Alkaline Artificial Seawater Environment on the Corrosion Behaviour of Duplex Stainless Steel 2205
    Tien Tran Thi Thuy
    Kannoorpatti, Krishnan
    Padovan, Anna
    Thennadil, Suresh
    APPLIED SCIENCES-BASEL, 2020, 10 (15):