Effect of Temperature on the Early-age Hydration and Setting Behaviour of Mixes Containing GGBS

被引:2
作者
Kanavaris, Fragkoulis [1 ]
Soutsos, Marios [2 ]
Chen, Jian-Fei [3 ]
机构
[1] ARUP, Tech Specialist Serv, Specialist Technol Analyt Res, London, England
[2] Queens Univ Belfast, Sch Nat & Built Environm, Belfast, North Ireland
[3] Southern Univ Sci & Technol, Dept Ocean Sci & Engn, Shenzhen, Peoples R China
关键词
APPARENT ACTIVATION-ENERGY; BLAST-FURNACE SLAG; STRENGTH DEVELOPMENT; PORTLAND-CEMENT; BLENDED CEMENT; HEAT EVOLUTION; CONCRETE; SHRINKAGE; ADMIXTURES; FINENESS;
D O I
10.3151/jact.22.14
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Over the past years there has been an increasing trend to use supplementary cementitious materials in concrete to improve its sustainability credentials and durability properties. Perhaps amongst the most popular supplementary cementitious materials is ground granulated blast -furnace slag (GGBS). While the hydration and setting characteristics of mixes with GGBS cured under standard conditions (20 degrees C) has been adequately investigated, the effect of temperature on heat of hydration and setting and the interrelation of these properties has not been evaluated for GGBS containing mixes. In this study, the heat of hydration and setting behaviour of mixes with various levels of GGBS (0, 20, 35, 50 and 70%) cured under elevated temperatures (20, 30, 40, 50 and 60 degrees C) is determined. Elevated curing temperature accelerates the hydration reactions and can significantly reduce the setting time of GGBS-containing mixes. The investigation of heat of hydration at very early ages, can provide an indication of the initial and final setting times of cementitious mixes. The "apparent" activation energy used to characterise temperature sensitivity of cementitious systems, is calculated based on heat of hydration and setting time measurements. It was found that the "apparent" activation energy increases with GGBS content for both heat of hydration and setting behaviour. The value of "apparent" activation energy differs significantly depending on the material property that is considered, such as compressive strength, heat of hydration or setting time.
引用
收藏
页码:14 / 32
页数:19
相关论文
共 85 条
[21]   Effect of autogenous deformation on the cracking risk of slag cement concretes [J].
Darquennes, Aveline ;
Staquet, Stephanie ;
Delplancke-Ogletree, Marie-Paule ;
Espion, Bernard .
CEMENT & CONCRETE COMPOSITES, 2011, 33 (03) :368-379
[22]   Reactivity of blast-furnace slag in Portland cement blends hydrated under different conditions [J].
Escalante, JI ;
Gómez, LY ;
Johal, KK ;
Mendoza, G ;
Mancha, H ;
Méndez, J .
CEMENT AND CONCRETE RESEARCH, 2001, 31 (10) :1403-1409
[23]   The effect of temperature on the early hydration of Portland cement and blended cements [J].
Escalante-Garcia, JI ;
Sharp, JH .
ADVANCES IN CEMENT RESEARCH, 2000, 12 (03) :121-130
[24]   Effect of w/c ratio on fresh electrical resistivity of various pumice based HPC and computation of setting time [J].
Ghosh, Pratanu ;
Ganesan, Rajthilak .
MATERIALS AND STRUCTURES, 2022, 55 (03)
[25]   Influence of Temperature in the Early-age Elastic Modulus Evolution of Cement Pastes and Concrete [J].
Granja, Jose ;
Ribeiro, Renan Rocha ;
Russo, Thomas ;
Lameiras, Rodrigo ;
Azenha, Miguel .
JOURNAL OF ADVANCED CONCRETE TECHNOLOGY, 2023, 21 (10) :803-820
[26]   Hydration heat evolution and kinetics of blended cement containing steel slag at different temperatures [J].
Han, Fanghui ;
Zhang, Zengqi ;
Wang, Dongmin ;
Yan, Peiyu .
THERMOCHIMICA ACTA, 2015, 605 :43-51
[27]  
Hansen P. F., 1985, CEB Information Bulletin, V166
[28]  
Hinrichs W., 1989, ADV CEM RES, V2, P9, DOI DOI 10.1680/ADCR.1989.2.5.9
[29]   Influence of cement fineness and water-to-cement ratio on mortar early-age heat of hydration and set times [J].
Hu, Jiong ;
Ge, Zhi ;
Wang, Kejin .
CONSTRUCTION AND BUILDING MATERIALS, 2014, 50 :657-663
[30]  
Japan Concrete Institute, 1999, Autogenous Shrinkage of Concrete, DOI 10.1201/9781482272123