Indentation-induced ductile behavior of glass-ceramics involving layered aluminosilicates

被引:3
|
作者
Maeda, Kei [1 ]
Okuma, Gaku [2 ]
Yoshida, Satoshi [3 ]
Wakai, Fumihiro [2 ]
Takeuchi, Akihisa [4 ]
Uesugi, Masayuki [4 ]
Yanagioka, Shun [1 ]
Matsunuma, Shun [1 ]
Machida, Shingo [1 ]
Yasumori, Atsuo [1 ]
机构
[1] Tokyo Univ Sci, Dept Mat Sci & Technol, 6-3-1 Niijuku,Katsushika Ku, Tokyo 1258585, Japan
[2] Natl Inst Mat Sci, Res Ctr Struct Mat, Tsukuba, Japan
[3] AGC Inc, Yokohama Tech Ctr, Yokohama, Japan
[4] Japan Synchrotron Radiat Res Inst, Sayo, Japan
关键词
brittle materials; ductility; glass-ceramics; CRACK DEFLECTION PROCESSES; CAO-AL2O3-SIO2; GLASS; FRACTURE; DESIGN; DEFORMATION; CONTACT;
D O I
10.1111/jace.19335
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Contact damage in materials is critical in engineering applications because it influences mechanical resistance, such as wear, erosion, and impact failure. Indentation tests were performed using a tungsten carbide ball indenter (Hertzian contact) on the surfaces of glass-ceramics containing hexagonal CaAl2Si2O8 or mica crystals (fluorophlogopite), both of which have a layered structure. The stress-strain relation and the permanent deformation on the surface, as well as the observation of the microcrack zone by X-ray computed tomography using synchrotron radiation, revealed that the glass-ceramic with hexagonal CaAl2Si2O8 showed ductility similar to the quasi-plastic behavior previously observed in the mica glass-ceramic. The yield stresses of the glass-ceramics were estimated from the stress deviating from the stress-strain relation assuming complete elastic response between the ball and the sample. The ratio of the yield stress to Young modulus (Y/E) of the glass-ceramic with hexagonal CaAl2Si2O8 was determined to be higher than that of the mica glass-ceramic.
引用
收藏
页码:7440 / 7448
页数:9
相关论文
共 50 条
  • [1] Indentation-induced debonding of ductile films
    Volinsky, AA
    Clift, WM
    Moody, NR
    Gerberich, WW
    INTERFACIAL ENGINEERING FOR OPTIMIZED PROPERTIES II, 2000, 586 : 255 - 260
  • [2] Indentation-induced crystallization in a metallic glass
    Yan Zhi-Jie
    Li Jin-Fu
    Zhou Yao-He
    Wu Yan-Qing
    ACTA PHYSICA SINICA, 2007, 56 (02) : 999 - 1003
  • [3] Indentation-induced crack interaction in alumina ceramics
    Twigg, PC
    Davidge, RW
    Riley, FL
    Franco, A
    Roberts, SG
    PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1996, 74 (05): : 1245 - 1252
  • [4] Indentation-induced crack interaction in alumina ceramics
    Twigg, P. C.
    Davidge, R. W.
    Riley, F. L.
    Franco, A.
    Philosophical Magazine A: Physics of Condensed Matter, Defects and Mechanical Properties, 74 (05):
  • [5] Quantitative evaluation of indentation-induced densification in glass
    Yoshida, S
    Sangleboeuf, JC
    Rouxel, T
    JOURNAL OF MATERIALS RESEARCH, 2005, 20 (12) : 3404 - 3412
  • [6] Hydrothermal corrosion behavior of silicon carbide ceramics with prefabricated indentation-induced cracks
    Liu, Yang-Qing
    Zhan, Chuang-Tian
    Guo, Wei-Ming
    Zhang, Ze-Xi
    Long, Ying
    Lin, Hua-Tay
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2025, 108 (06)
  • [7] Refractory glass-ceramics based on alkaline earth aluminosilicates
    Beall, G. H.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2009, 29 (07) : 1211 - 1219
  • [8] Quantitative evaluation of indentation-induced densification in glass
    Satoshi Yoshida
    Jean-Christophe Sangleboeuf
    Tanguy Rouxel
    Journal of Materials Research, 2005, 20 : 3404 - 3412
  • [9] Indentation-induced interface delamination of a strong film on a ductile substrate
    Abdul-Baqi, A
    Van der Giessen, E
    THIN SOLID FILMS, 2001, 381 (01) : 143 - 154
  • [10] Computational modelling of static indentation-induced damage in glass
    Ismail, Jewan
    Zairi, Fahmi
    Nait-Abdelaziz, Moussa
    Azari, Zitouni
    COMPUTATIONAL MATERIALS SCIENCE, 2008, 42 (03) : 407 - 415