MICRO-ARC OXIDATION ENHANCES MECHANICAL PROPERTIES AND CORROSION RESISTANCE OF TI-6AL-7NB ALLOY

被引:0
|
作者
Naji, Qabas Khalid [1 ]
Salman, Jassim Mohammed [2 ]
Dawood, Nawal Mohammed [2 ]
机构
[1] AL Mustaqbal Univ Collage, Biomed Engn Dept, Hillah, Babil, Iraq
[2] Univ Babylon, Coll Mat Engn, Dept Met Engn, Hillah, Iraq
来源
3C TECNOLOGIA | 2023年 / 12卷 / 01期
关键词
MAO; Contact Angle; Clinical Application; Oxidation Time; porosity; and Corrosion Resistance; TITANIUM; SURFACE; BEHAVIOR; TI6AL4V; TI;
D O I
10.17993/3ctecno.2023.v12n1e43.262-280
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Investigation results of micro-arc coating on the (Ti-7Nb-6Al) alloy were presented. It has potential clinical value in applications such as dental implant, knee, and hip prostheses. An electrolyte solution of ( Na2CO3 + Na2SiO3). The micro-arc oxidation (MAO) technique was employed for in situ oxidation of Ti-6Al-7Nb surface. The wettability of a porous TiO2 covering made up of anatase and rutile phases was investigated. The test findings revealed that the possibility of deposition of ceramics coatings on the surface of Ti-6Al-7Nb alloy by using voltages (400V )at different deposition times (7, 15, and 30) min. The results indicate that ceramics layer of titanium oxide (TiO2) which is formed during coating porous and homogenous distribution. The bioactive composition of the oxide layers can be suitable for use as advanced biomedical implants. The coatings also revealed an increased surface roughness, porosity, microhardness, surface wettability and corrosion resistance of the Ti-6Al-7Nb substrate reaches to (CR= 0.1114x10-3mpy) in Ringer's solution and (CR= 1.03x10-3mpy) in Saliva's solution with increased deposition time.
引用
收藏
页码:262 / 280
页数:19
相关论文
共 50 条
  • [1] Characterization of microporous oxide layer synthesized on Ti-6Al-7Nb alloy by micro-arc oxidation
    Moskalewicz, T.
    Kruk, A.
    Kot, M.
    Kayali, S.
    Czyrska-Filemonowicz, A.
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2014, 14 (03) : 370 - 375
  • [2] Mechanical properties and corrosion resistance of Ti-6Al-7Nb alloy dental castings
    Kobayashi, E
    Wang, TJ
    Doi, H
    Yoneyama, T
    Hamanaka, H
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1998, 9 (10) : 567 - 574
  • [3] Mechanical Properties, Corrosion Resistance and Bioactivity of Oxide Layers Formed by Isothermal Oxidation of Ti-6Al-7Nb Alloy
    Aniolek, Krzysztof
    Losiewicz, Bozena
    Kubisztal, Julian
    Osak, Patrycja
    Stroz, Agnieszka
    Barylski, Adrian
    Kaptacz, Slawomir
    COATINGS, 2021, 11 (05)
  • [4] Fatigue behavior of modified surface of Ti-6Al-7Nb and CP-Ti by micro-arc oxidation
    Campanelli, Leonardo Contri
    Duarte, Lais Tereza
    Carvalho Pereira da Silva, Paulo Sergio
    Bolfarini, Claudemiro
    MATERIALS & DESIGN, 2014, 64 : 393 - 399
  • [5] Isothermal oxidation of Ti-6Al-7Nb alloy
    Aniolek, K.
    Kupka, M.
    Luczuk, M.
    Barylski, A.
    VACUUM, 2015, 114 : 114 - 118
  • [6] Cyclic oxidation of Ti-6Al-7Nb alloy
    Aniolek, Krzysztof
    Kupka, Marian
    Dercz, Grzegorz
    VACUUM, 2019, 168
  • [7] Mechanical Properties and Corrosion Behavior of Thermally Treated Ti-6Al-7Nb Dental Alloy
    Hulka, Iosif
    Florido-Suarez, Nestor R.
    Mirza-Rosca, Julia C.
    Saceleanu, Adriana
    MATERIALS, 2022, 15 (11)
  • [8] Evaluation of the mechanical properties of powder metallurgy Ti-6Al-7Nb alloy
    Bolzoni, L.
    Ruiz-Navas, E. M.
    Gordo, E.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2017, 67 : 110 - 116
  • [9] Mechanical Properties of Anodically Oxidized cpTi and Ti-6Al-7Nb Alloy
    Basiaga, Marcin
    Paszenda, Zbigniew
    Karasinski, Pawel
    Kajzer, Anita
    Walke, Witold
    APPLICATIONS OF COMPUTATIONAL TOOLS IN BIOSCIENCES AND MEDICAL ENGINEERING, 2015, 71 : 123 - 132
  • [10] Mechanical property and corrosion resistance evaluations of Ti-6Al-7Nb alloy brazed with bulk metallic glasses
    Miura, Eri
    Kato, Hidemi
    Ogata, Toshiaki
    Nishiyama, Nobuyuki
    Specht, Eliot D.
    Shiraishi, Takanobu
    Inoue, Akihisa
    Hisatsune, Kunihiro
    MATERIALS TRANSACTIONS, 2007, 48 (08) : 2235 - 2243