Contrasting graphitization differences between vitrinite and inertinite based on high-temperature and high-pressure experiments

被引:5
|
作者
Liu, Zhifei [1 ,2 ]
Cao, Daiyong [2 ]
Chen, Gaojian [2 ]
Chen, Qingtong [1 ]
Zhao, Heming [1 ]
机构
[1] China Coal Technol & Engn Grp Corp, China Coal Res Inst, Beijing 100013, Peoples R China
[2] China Univ Min & Technol Beijing, Beijing 100083, Peoples R China
关键词
Coal-based graphite; High-temperature high-pressure experiments; Vitrinite; Inertinite; GRAPHITE; COALS;
D O I
10.1016/j.fuel.2023.130796
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
It has been recognized that vitrinite and inertinite exhibit different evolutionary characteristics during coalification processs, but the study of their evolutionary differences after entering the graphitization process is limited. To investigate the graphitization differences, this study conducted high -temperature high-pressure (HT -HP) experiments under different temperature and pressure conditions. The precursor used in the HT -HP experiments was concentrated inertinite-rich samples and vitrinite-rich samples obtained through manual selection, and the parent coal is low volatile bituminous coal (Rmax (%) = 1.7). X-ray diffraction (XRD), Raman spectroscopy, and high -resolution transmission electron microscopy (HRTEM) were employed to compare and analyze the graphite lattice evolution of the maceral. The experimental results indicated the following: (1) During the construction of the three-dimensional graphite lattice, vitrinite and inertinite exhibited differences in response to temperature and pressure conditions. Inertinite had a higher graphitization threshold compared to vitrinite, and once reached or exceeded, inertinite underwent rapid graphitization seen by the significant decrease of the interlayer spacing d002; (2) In terms of defect healing, under the same stress conditions, vitrinite was more sensitive to temperature compared to inertinite as observed by the Raman parameters R2 and R3; (3) By comparing the development of graphite structure under different temperature and pressure conditions, we found that both efficient graphitization process and development of the graphite structure require a synergistic combination of temperature and pressure, where an excessive or insufficient pressure can inhibit graphitization and even dismantle and damage the formed graphite structure.
引用
收藏
页数:14
相关论文
共 50 条
  • [41] XANES, Raman and XRD study of anthracene-based cokes and saccharose-based chars submitted to high-temperature pyrolysis
    Bernard, S.
    Beyssac, O.
    Benzerara, K.
    Findling, N.
    Tzvetkov, G.
    Brown, G. E., Jr.
    CARBON, 2010, 48 (09) : 2506 - 2516
  • [42] Safer Triethyl-Phosphate-Based Electrolyte Enables Nonflammable and High-Temperature Endurance for a Lithium Ion Battery
    Jiang, Lihua
    Liang, Chen
    Li, Huang
    Wang, Qingsong
    Sun, Jinhua
    ACS APPLIED ENERGY MATERIALS, 2020, 3 (02) : 1719 - 1729
  • [43] A relation between a metallic film covering on diamond and diamond nucleation and growth at high-temperature-high-pressure in a Ni-Mn-C system
    Bin Xu
    Li, Mu-sen
    Li, Li
    Xu, Ai-min
    Niu, Yu-chao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 454 : 293 - 299
  • [44] On enhancing the high-temperature wear behaviour of Al2090-based hybrid composites using tertiary ceramic particles
    Sharath, B. N.
    Mahesh, Vinyas
    Mahesh, Vishwas
    Kattimani, Subhaschandra
    Harursampath, Dineshkumar
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2024,
  • [45] Differences and correlations between microstructure and macroscopic properties of mesophase cokes derived from the components of high temperature coal tar pitch
    Hu, Chaoshuai
    Chu, Hongyu
    Zhu, Yaming
    Xu, Yunliang
    Cheng, Junxia
    Gao, Lijuan
    Lai, Shiquan
    Zhao, Xuefei
    FUEL, 2022, 310
  • [46] Assessment of amount and concentration of tritium in HTTR-IS system based on tritium behavior during high-temperature continuous operation of HTTR
    Dipu, Arnoldus Lambertus
    Ohashi, Hirofumi
    Hamamoto, Shimpei
    Sato, Hiroyuki
    Nishihara, Tetsuo
    ANNALS OF NUCLEAR ENERGY, 2016, 88 : 126 - 134
  • [47] Innovative Early Detection of High-Temperature Abuse of Prismatic Cells and Post-Abuse Degradation Analysis Using Pressure and External Fiber Bragg Grating Sensors
    Hebenbrock, Andre
    Orazov, Nury
    Benger, Ralf
    Schade, Wolfgang
    Hauer, Ines
    Turek, Thomas
    BATTERIES-BASEL, 2024, 10 (03):
  • [48] Improved high-temperature performance of lithium-ion batteries through use of a thermally stable co-polyimide-based cathode binder
    Choi, Jaecheol
    Ryou, Myung-Hyun
    Son, Bongki
    Song, Jongchan
    Park, Jung-Ki
    Cho, Kuk Young
    Lee, Yong Min
    JOURNAL OF POWER SOURCES, 2014, 252 : 138 - 143
  • [49] Towards chrome-free lining for plasma gasifiers using the CA6-SiC castable based on high-temperature water vapor corrosion
    Chen, Ding
    Gu, Huazhi
    Huang, Ao
    Ni, Hongwei
    CERAMICS INTERNATIONAL, 2019, 45 (09) : 12429 - 12435
  • [50] Nickel-catalyzed synthesis of nano-diamonds during the high-temperature chlorination of the layered structured bulk of Ti3C2 under atmospheric pressure
    Zhang, Zhao
    Ma, Huaxin
    Zhang, Jingjie
    Li, Shuo
    Zhang, Ruijun
    DIAMOND AND RELATED MATERIALS, 2023, 137