Mechanisms and kinetics of zinc and iron separation enhanced by calcified carbothermal reduction for electric arc furnace dust

被引:7
作者
Qiu, Jiayong [1 ,2 ,4 ,5 ]
Yu, Shui [1 ,3 ,4 ,5 ]
Shao, Jiugang [3 ]
Zhu, Kaiqi [1 ,4 ,5 ]
Ju, Dianchun [1 ,4 ,5 ]
Chen, Chunyu [1 ,4 ,5 ]
Qi, Dexing [1 ,4 ,5 ]
Wang, Fei [3 ]
Bai, Ni [1 ,4 ,5 ]
Mao, Rui [1 ,3 ]
Wang, Xiaoming [2 ]
机构
[1] Jiangsu Univ Sci & Technol, Sch Met & Mat Engn, Zhangjiagang 215600, Peoples R China
[2] State Key Lab Mineral Proc, Beijing 102628, Peoples R China
[3] Sha Steel, Inst Res Iron & Steel, Zhangjiagang 215625, Peoples R China
[4] Ind Technol Res Inst Zhangjiagang, Inst Fine Met Res, Zhangjiagang 215600, Peoples R China
[5] Jiangsu Univ Sci & Technol, Zhangjiagang 215600, Peoples R China
关键词
EAF Dust; Calcified Carbothermic Reduction; Phase Transition; Kinetics; Non-isothermal; ENERGY;
D O I
10.1007/s11814-022-1295-9
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
A high basicity charge prepared with electric arc furnace dust (EAFD), carbonaceous reducing agent and CaO is proposed. The mechanisms of enhancing separation of zinc and iron by calcified carbothermic reduction of the high basicity charge were analyzed by combining thermal analysis kinetics and experiment. The influences of roasting temperature, carbon ratio (n(c)/n(o), molar ratio of carbon in graphitic carbon powder to oxygen in EAFD), and CaO dosage on phase transition and dezincification ratio in EAFD were investigated. The results show that the intermediates Ca2Fe2O5 and Fe0.85-xZnxO can be produced from the zinc-iron separation of zinc ferrate during the process of calcified carbothermic reduction of EAFD. Addition of CaO and C results in the following transition pathways: ZnFe2O4+ CaO -> Ca2Fe2O5+ZnO -> Ca2Fe2O5+Zn(g)-> CaO+Fe; Fe0.85-xZnxO+CaO -> Ca2Fe2O5+FeO+ZnO -> CaO+Fe+Zn(g). In the range of n(c)/n(o) of 0.4-1.2 and roasting temperature of 1,000-1,100 degrees C, the addition of CaO can promote reduction and dezincification. Based on the Kissinger-Akahira-Sunose (KAS) and Coats-Redfern methods, the kinetic results show that the calcified carbothermic reduction process can be divided into three stages: initial stage (alpha=0-0.3), middle stage (alpha=0.3-0.45), and final stage (alpha=0.45-1.0). The average activation energy of the initial stage is 305.01 kJ center dot mol(-1), and the reaction mechanism is one-dimensional diffusion. The average activation energy is 315.67 kJ center dot mol(-1) for the middle stage and 288.22 kJ center dot mol(-1) for the final stage. The chemical reaction equation is found to be the most suitable mechanism in the medium and final stages. It is also found that the addition of CaO can reduce the average activation energy by about 32 kJ center dot mol(-1) and shorten the intermediate stage of the reaction.
引用
收藏
页码:975 / 985
页数:11
相关论文
共 50 条
  • [41] Unveiling the power of MgCl2 in extracting zinc from electric arc furnace dust
    Huang, Jingdong
    Yang, Xiao
    RESOURCES CONSERVATION AND RECYCLING, 2025, 215
  • [42] Direct Conversion of Electric Arc Furnace Dust to Zinc Ferrite by Roasting: Effect of Roasting Temperature
    Tang, Huimin
    Peng, Zhiwei
    Wang, Liancheng
    Anzulevich, Anton
    Rao, Mingjun
    Li, Guanghui
    JOURNAL OF SUSTAINABLE METALLURGY, 2023, 9 (01) : 363 - 374
  • [43] Direct Conversion of Electric Arc Furnace Dust to Zinc Ferrite by Roasting: Effect of Roasting Temperature
    Huimin Tang
    Zhiwei Peng
    Liancheng Wang
    Anton Anzulevich
    Mingjun Rao
    Guanghui Li
    Journal of Sustainable Metallurgy, 2023, 9 : 363 - 374
  • [44] Selective Zinc Removal from Electric Arc Furnace (EAF) Dust by Using Microwave Heating
    Mamdouh Omran
    Timo Fabritius
    Eetu-Pekka Heikkinen
    Journal of Sustainable Metallurgy, 2019, 5 : 331 - 340
  • [45] The Waelz Slag from Electric Arc Furnace Dust Processing: Characterization and Magnetic Separation Studies
    Grudinsky, Pavel
    Yurtaeva, Anfisa
    Pankratov, Denis
    Pasechnik, Liliya
    Musaelyan, Roman
    Dyubanov, Valery
    MATERIALS, 2024, 17 (10)
  • [46] Purification of the leaching solution of recycling zinc from the hazardous electric arc furnace dust through an as-bearing jarosite
    Hazaveh, Parsa Khanmohammadi
    Karimi, Saeid
    Rashchi, Fereshteh
    Sheibani, Saeed
    ECOTOXICOLOGY AND ENVIRONMENTAL SAFETY, 2020, 202
  • [47] Phase Transformation Characteristics of the ZnO-Fe2O3 System in Zinc-Containing Electric Furnace Dust During Vacuum Carbothermal Reduction
    Lin, Yibo
    Lei, Yuban
    Lv, Xiaodong
    Yang, Jing
    Huang, Run
    JOURNAL OF SUSTAINABLE METALLURGY, 2025, : 1495 - 1510
  • [48] Behavior of zinc, iron and calcium from electric arc furnace (EAF) dust in hydrometallurgical processing in sulfuric acid solutions: Thermodynamic and kinetic aspects
    Kukurugya, F.
    Vindt, T.
    Havlik, T.
    HYDROMETALLURGY, 2015, 154 : 20 - 32
  • [49] Microwave-Assisted Reduction of Electric Arc Furnace Dust with Biochar: An Examination of Transition of Heating Mechanism
    Ye, Qing
    Peng, Zhiwei
    Li, Guanghui
    Lee, Joonho
    Liu, Yong
    Liu, Mudan
    Wang, Liancheng
    Rao, Mingjun
    Zhang, Yuanbo
    Jiang, Tao
    ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2019, 7 (10) : 9515 - 9524
  • [50] A mathematical model for the reduction kinetics of iron oxide in electric furnace slags by graphite injection
    Morales, RD
    RodriguezHernandez, H
    GarnicaGonzalez, P
    RomeroSerrano, JA
    ISIJ INTERNATIONAL, 1997, 37 (11) : 1072 - 1080