The effect of SiC whiskers addition on the microstructure and mechanical properties of a (Hf-Ta-Zr-Nb-Ti)C-SiC composite

被引:9
作者
Hrubovcakova, Monika [1 ]
Csanadi, Tamas [1 ]
Sedlak, Richard [1 ]
Kovalcikova, Alexandra [1 ]
Shepa, Ivan [1 ]
Mudra, Erika [1 ]
Sopcak, Tibor [1 ]
Unsal, Hakan [2 ]
Tatarko, Peter [2 ]
Sajgalik, Pavol [2 ]
Dusza, Jan [1 ,3 ]
机构
[1] Slovak Acad Sci, Inst Mat Res, Watsonova 47, Kosice 04001, Slovakia
[2] Slovak Acad Sci, Inst Inorgan Chem, Dubravska Cesta 9, Bratislava 84511, Slovakia
[3] Obuda Univ, Donat Banki Fac Mech & Safety Engn, Nepszinhaz Utca 8, H-1081 Budapest, Hungary
基金
欧盟地平线“2020”;
关键词
High-entropy carbide; SiC whiskers; Spark plasma sintering; Microstructure; Mechanical properties; HIGH-ENTROPY CARBIDE; PHASE EVOLUTION; CERAMICS; BEHAVIOR; INDENTATION; RESISTANCE; FRACTURE; GRAINS;
D O I
10.1016/j.ceramint.2022.10.239
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
High-energy ball milling of carbide powders, mixing with SiC whiskers, and following spark plasma sintering was used for the processing of a (Hf-Ta-Zr-Nb-Ti)C-SiC composite. A high relative density composite (99.4%) was achieved consisting of a single-phase high-entropy carbide (HEC) matrix and homogenously distributed SiC phase with evident degradation of the whiskers to particles. The grain size of the HEC matrix was in the range of 1.0-5.0 & mu;m and the diameter of the SiC phase was about 0.5-6.0 & mu;m with a low aspect ratio. The nano-hardness of the HEC matrix and SiC phase was about 38 GPa and 42 GPa, respectively. The microhardness increased with SiC addition from 24.4 to 28.7 GPa together with the indentation fracture resistance from 2.68 to 3.16 MPa m1/2 in comparison with the monolithic HEC of similar relative density and grain size. The toughening mechanisms were revealed to be crack deflection, crack branching, and crack bridging.
引用
收藏
页码:24179 / 24186
页数:8
相关论文
共 37 条
[1]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[2]  
BECHER PF, 1984, J AM CERAM SOC, V67, pC267, DOI 10.1111/j.1151-2916.1984.tb19694.x
[3]   Processing and Properties of High-Entropy Ultra-High Temperature Carbides [J].
Castle, Elinor ;
Csanadi, Tamas ;
Grasso, Salvatore ;
Dusza, Jan ;
Reece, Michael .
SCIENTIFIC REPORTS, 2018, 8
[4]   Small scale fracture and strength of high-entropy carbide grains during microcantilever bending experiments [J].
Csanadi, Tamas ;
Vojtko, Marek ;
Dankhazi, Zoltan ;
Reece, Michael J. ;
Dusza, Jan .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (14) :4774-4782
[5]   Anisotropic dislocation nucleation in ZrB2 grains and deformation behaviour of constituents of ZrB2-SiC and ZrB2-B4C composites during nanoindentation [J].
Csanadi, Tamas ;
Vojtko, Marek ;
Sedlak, Richard ;
Naughton-Duszova, Annamaria ;
Pedzich, Zbigniew ;
Dusza, Jan .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (07) :2674-2682
[6]   Strength enhancement and slip behaviour of high-entropy carbide grains during micro-compression [J].
Csanadi, Tamas ;
Castle, Elinor ;
Reece, Michael J. ;
Dusza, Jan .
SCIENTIFIC REPORTS, 2019, 9 (1)
[7]   Slip activation controlled nanohardness anisotropy of ZrB2 ceramic grains [J].
Csanadi, Tamas ;
Kovalcikova, Alexandra ;
Dusza, Jan ;
Fahrenholtz, William G. ;
Hilmas, Gregory E. .
ACTA MATERIALIA, 2017, 140 :452-464
[8]   Nanoindentation and tribology of a (Hf-Ta-Zr-Nb-Ti)C high-entropy carbide [J].
Dusza, Jan ;
Csanadi, Tamas ;
Medved, David ;
Sedlak, Richard ;
Vojtko, Marek ;
Ivor, Michal ;
Unsal, Hakan ;
Tatarko, Peter ;
Tatarkova, Monika ;
Sajgalik, Pavol .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (11) :5417-5426
[9]   Microstructure of (Hf-Ta-Zr-Nb)C high-entropy carbide at micro and nano/atomic level [J].
Dusza, Jan ;
Svec, Peter ;
Girman, Vladimir ;
Sedlak, Richard ;
Castle, Elinor G. ;
Csanadi, Tamas ;
Kovalcikova, Alexandra ;
Reece, Michael J. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (12) :4303-4307
[10]   Strength of single-phase high-entropy carbide ceramics up to 2300°C [J].
Feng, Lun ;
Chen, Wei-Ting ;
Fahrenholtz, William G. ;
Hilmas, Gregory E. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2021, 104 (01) :419-427