Dissolution behavior of dizinc magnesium phase in Al-Zn-Mg-Cu alloy

被引:22
作者
Yang, Hongfu [1 ]
Zhang, Yelin [1 ]
Zheng, Shanju [1 ]
Zaki, Zaki I. [2 ]
Huang, Rensong [1 ]
Lu, Shumeng [1 ]
Sun, Peng [1 ]
Ibrahim, Mohamed M. [2 ]
Hou, Hua [3 ]
Li, Mengnie [1 ]
Yuan, Xiaohong [4 ]
Wang, Xiaojing [5 ]
El-Bahy, Zeinhom M. [6 ]
机构
[1] Kunming Univ Sci & Technol, Fac Mat Sci & Engn, Kunming 650093, Peoples R China
[2] Taif Univ, Coll Sci, Dept Chem, POB 11099, At Taif 21944, Saudi Arabia
[3] Taiyuan Univ Sci & Technol, Sch Mat Sci & Engn, Taiyuan 030024, Peoples R China
[4] Sino Platinum Met Co Ltd, Kunming Inst Precious Met, Kunming 650106, Peoples R China
[5] Jiangsu Univ Sci & Technol, Zhenjiang 212003, Peoples R China
[6] Al Azhar Univ, Fac Sci, Dept Chem, Cairo 11884, Egypt
关键词
Dizinc magnesium phase; Dissolution behavior; Kinetic model; Al-Zn-Mg-Cu alloy; MECHANICAL-PROPERTIES; PRECIPITATION BEHAVIOR; IN-SITU; KINETICS; HOMOGENIZATION; MICROSTRUCTURE; EVOLUTION; ETA'; TRANSFORMATIONS;
D O I
10.1007/s42114-023-00785-3
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The presence of the dizinc magnesium (MgZn2) phase in Al-Zn-Mg-Cu alloy significantly enhances its mechanical properties due to the high density, uniform distribution, and fine size of the MgZn2 phase. While previous studies have focused on precipitation evolution during solid solution and aging, little attention has been given to dissolution behavior. The dissolution behavior of MgZn2 phase during heat treatment was studied by changing the heat treatment temperature and time in the article. It was found to be completely dissolved at 480 degrees C and 490 degrees C/60 min. Experimental results were fitted to establish the relationship between the volume fraction of the MgZn2 phase and time at temperatures ranging from 460 to 490 degrees C. Additionally, a kinetic model for dissolution process was derived based on classical particle system dissolution model and diffusion-controlled transformation theory with adjusted parameters representing physical quantities accurately. These results are helpful to obtain precipitates with smaller size, more quantity and better dispersion, which is of great significance for improving the mechanical properties of the alloy.Graphical abstractKinetic model of solute diffusion including MgZn2/Al-matrix interface is established based on the classical dissolution model.
引用
收藏
页数:16
相关论文
共 50 条
[21]   Ageing precipitation and strengthening behavior of the spray formed Al-Zn-Mg-Cu alloy [J].
Liu Hongwei ;
Wang Feng ;
Xiong Baiqing ;
Zhang Yong'an ;
Li Zhihui ;
Li Xiwu .
ADVANCED ENGINEERING MATERIALS II, PTS 1-3, 2012, 535-537 :903-908
[22]   Research on Dynamic Shock Response Behavior of Al-Zn-Mg-Cu Aluminum Alloy [J].
Huang Dan ;
Li Zhuo ;
Zhou Xudong ;
Yuan Fangtong ;
Zhao Wu .
RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (01) :242-248
[23]   Effect of retrogression treatment on microstructure, mechanical properties, and corrosion behavior in Al-Zn-Mg-Cu alloy [J].
Hwang, Hyo Jin ;
Lee, Chang-Gi ;
Kayani, Saif Haider ;
Kim, Hyoung-Wook ;
Lee, Je In ;
Kim, Se-Ho ;
Jo, Yong Hee .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2025, 36 :10577-10590
[24]   Phase transformation and microstructure evolution of an ultra-high strength Al-Zn-Mg-Cu alloy during homogenization [J].
Xu, Da ;
Li, Zhihui ;
Wang, Guojun ;
Li, Xiwu ;
Lv, Xinyu ;
Zhang, Yong'an ;
Fan, Yunqiang ;
Xiong, Baiqing .
MATERIALS CHARACTERIZATION, 2017, 131 :285-297
[25]   Effect of various aging treatment on thermal stability of a novel Al-Zn-Mg-Cu alloy for oil drilling [J].
Zhao, Juangang ;
Liu, Zhiyi ;
Bai, Song ;
Huang, Tiantian ;
Wang, Jian ;
Xie, Haoyu ;
Zeng, Diping ;
Luo, Lei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 803
[26]   The effect of pre-ageing/stretching on the ageing-hardening behavior of Al-Zn-Mg-Cu alloys correlated with Zn/Mg ratio [J].
Zou, Yan ;
Wu, Xiaodong ;
Tang, Songbai ;
Wang, Yichang ;
Zhao, Kai ;
Cao, Lingfei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 830
[27]   Aging behavior and precipitate characterization of a high Zn-containing Al-Zn-Mg-Cu alloy with various tempers [J].
Wen, Kai ;
Fan, Yunqiang ;
Wang, Guojun ;
Jin, Longbin ;
Li, Xiwu ;
Li, Zhihui ;
Zhang, Yongan ;
Xiong, Baiqing .
MATERIALS & DESIGN, 2016, 101 :16-23
[28]   Effect of Zn/Mg ratio on the microstructure and mechanical properties of as-cast Al-Zn-Mg-Cu alloys and the phase transformation during homogenization [J].
Yin, He ;
Wen, Kai ;
Li, Zhihui ;
Li, Xiwu ;
Li, Yanan ;
Yan, Lizhen ;
Yan, Hongwei ;
Yu, Mingyang ;
Zhang, Yongan ;
Xiong, Baiqing .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 26 :3646-3660
[29]   Effect of Yb Microalloying on Microstructure and Properties of Al-Zn-Mg-Cu Alloy [J].
Xu Yongxiang ;
Zhu Mengzhen ;
Fang Huachan ;
Zhang Zhuo ;
Duan Zhiying ;
Sun Zhen .
RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (10) :3556-3562
[30]   Microstructure of spray formed Al-Zn-Mg-Cu alloy with Mn addition [J].
Cai Yuan-hua ;
Liang Rui-guang ;
Su Zhan-pei ;
Zhang Ji-shan .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (01) :9-14