Thermal stability and degradation mechanism of C60 fullerene-based polymers

被引:1
作者
Lisa, Gabriela [1 ,3 ]
Cleminte, Cerasela-Ionela [1 ]
Michinobu, Tsuyoshi [2 ]
机构
[1] Gheorghe Asachi Tech Univ Iasi, Cristofor Simionescu Fac Chem Engn & Environm Pro, Dept Chem Engn, Iasi, Romania
[2] Tokyo Inst Technol, Dept Mat Sci & Engn, Tokyo, Japan
[3] Gheorghe Asachi Tech Univ Iasi, Cristofor Simionescu Fac Chem Engn & Environm Pro, Dept Chem Engn, 73 Prof Doctor Docent Dimitrie Mangeron St, Iasi 700050, Romania
关键词
degradation mechanism; fullerene polymers; molecular modeling; thermal stability; POLYSTYRENE; CHEMISTRY;
D O I
10.1002/app.55079
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this paper, the thermal stability and degradation mechanisms of C-60 fullerene-based polymers, obtained by click polymerization between dialkyne-substituted C-60 derivative monomers and 1,3,5-tris(dodecyloxy)benzene-based diazide comonomers, were evaluated. The activation energy of the fullerene polymer C(60)P2 with an ethylene spacer, determined under peak degradation rate conditions, was lower than that of the counter polymer C(60)P1 with a methylene spacer, suggesting lower thermal stability of C(60)P2. The combined technique of thermogravimetric analysis-mass spectroscopy and Fourier transform infrared spectroscopy revealed that the thermal decomposition onset of the analyzed samples is accompanied by C C cleavage of the dodecyloxyside chain groups, followed by the decomposition of the 1,2,3-triazole, dicarboxylate and benzoate moieties. It was found that no thermal decomposition of the fullerene carbon cage occurs up to 670 degrees C. Molecular modeling with Hyperchem software version 7.5 confirmed that C(60)P1 is more thermally stable than C(60)P2.
引用
收藏
页数:12
相关论文
共 33 条
  • [1] Degradation mechanism and oxidation kinetics of C60 fullerene
    Aghili, Siavash
    Panjepour, Masoud
    Ghiaci, Mehran
    [J]. DIAMOND AND RELATED MATERIALS, 2022, 124
  • [2] [Anonymous], 2002, HYPERCHEM VERSION 75
  • [3] [Anonymous], 1994, ASTM BOOK STANDARDS, P1042
  • [4] ASTM, 1984, E698 ASTM, P56
  • [5] Thermal degradation studies of poly(urethane-siloxane) thermosets based on co-poly(dimethyl)(methyl, hydroxypolyoxyethylenepropyl) siloxane
    Byczynski, Lukasz
    Dutkiewicz, Michal
    Maciejewski, Hieronim
    [J]. THERMOCHIMICA ACTA, 2014, 589 : 252 - 261
  • [6] Fullerene (C60) Nanowires: The Preparation, Characterization, and Potential Applications
    Fan, Xiao
    Soin, Navneet
    Li, Haitao
    Li, Hua
    Xia, Xiaohong
    Geng, Junfeng
    [J]. ENERGY & ENVIRONMENTAL MATERIALS, 2020, 3 (04) : 469 - 491
  • [7] Inhibition of thermal degradation of polystyrene by C60 and PCBM: A comparative study
    Fernandes, Liliana
    Gaspar, Hugo
    Bernardo, Gabriel
    [J]. POLYMER TESTING, 2014, 40 : 63 - 69
  • [8] Fullerene C60 derivatives as antimicrobial photodynamic agents
    Heredia, Daniel A.
    Durantini, Andres M.
    Durantini, Javier E.
    Durantini, Edgardo N.
    [J]. JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY C-PHOTOCHEMISTRY REVIEWS, 2022, 51
  • [9] Synthesis and Characterization of [60] Fullerene-Glycidyl Azide Polymer and Its Thermal Decomposition
    Huang, Ting
    Jin, Bo
    Peng, Ru Fang
    Chen, Cong Di
    Zheng, Rong Zong
    He, Yi
    Chu, Shi Jin
    [J]. POLYMERS, 2015, 7 (05) : 896 - 908
  • [10] Thermal stability of a fullerene-amine adduct
    Janaki, J
    Premila, M
    Gopalan, P
    Sastry, VS
    Sundar, CS
    [J]. THERMOCHIMICA ACTA, 2000, 356 (1-2) : 109 - 116