Application of Ag-Cu-Ti active metal composite filler in ceramic joining: a review

被引:2
作者
Li, Yuhang [1 ]
Wang, Jun [2 ]
Shen, Ziyan [2 ]
Qian, Hangli [1 ]
Zhang, Wanliang [1 ]
Zhang, Kaiyu [1 ]
Ying, Danqing [1 ]
Zhou, Qihang [1 ]
Zhou, Chengshuang [1 ]
Zhang, Lin [1 ]
机构
[1] Zhejiang Univ Technol, Inst Mat Forming & Control Engn, Hangzhou 310014, Peoples R China
[2] Zhejiang Baima Lake Lab Co Ltd, Hangzhou 310053, Peoples R China
基金
中国国家自然科学基金;
关键词
brazing; composite filler; residual stress; active metal; ceramic-metal joints; CONTROL INTERFACIAL MICROSTRUCTURE; IMPROVE MECHANICAL-PROPERTIES; RESIDUAL-STRESS; STRENGTHENING MECHANISM; CBN GRAINS; COMPRESSIVE STRENGTH; MATRIX COMPOSITES; THERMAL-EXPANSION; F/SIC COMPOSITE; ENERGY-STORAGE;
D O I
10.1007/s11706-023-0664-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
As a structural and functional material with excellent properties, ceramics play an extremely important role in a wide range of industries, including life and production. To expand the range of applications for ceramic materials, ceramics are often joined to metals and then used. Among the physical and chemical joining methods of ceramics to metals, the AMB method is efficient and simple, suitable for industrial applications, and has been a hot topic of research. However, due to the problems of residual stresses caused by the large difference in thermal expansion coefficients between ceramic and metal brazing, composite fillers have become a very worthwhile solution by regulating the physical properties of the brazing material and improving the weld structure. This review describes the wetting principle and application of Ag-Cu-Ti active metal filler in the field of ceramic joining, with emphasis on the current stage of composite filler, and discusses the influence on the former brazing properties and organization after the introduction of dissimilar materials.
引用
收藏
页数:35
相关论文
共 50 条
[41]   Dealloying of a Ag-Cu-Ti alloy in liquid sodium at 350 °C [J].
Heo, Hoejun ;
Park, Yoon-Cheol ;
Kang, Chung-Yun ;
Jung, Keeyoung .
CORROSION SCIENCE, 2018, 144 :35-43
[42]   Joining alumina to Inconel 600 and UMCo-50 superalloys using an Sn10Ag4Ti active filler metal [J].
S. Y. Chang ;
Y. T. Hung ;
T. H. Chuang .
Journal of Materials Engineering and Performance, 2003, 12 (2) :123-127
[43]   Brazeability, Microstructure, and Joint Characteristics of ZrO2/Ti-6Al-4V Brazed by Ag-Cu-Ti Filler Reinforced with Cerium Oxide Nanoparticles [J].
Sharma, Ashutosh ;
Ahn, Byungmin .
ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2019, 2019
[44]   Joining alumina to Inconel 600 and UMCo-50 superalloys using an Sn10Ag4Ti active filler metal [J].
Chang, SY ;
Hung, YT ;
Chuang, TH .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2003, 12 (02) :123-127
[45]   Joining of Cf/SiC composite to Ti alloy using composite filler materials [J].
Xiong, J. ;
Huang, J. ;
Wang, Z. ;
Lin, G. ;
Zhang, H. ;
Zhao, X. .
MATERIALS SCIENCE AND TECHNOLOGY, 2009, 25 (08) :1046-1050
[46]   Joining Alumina to Titanium Alloys Using Ag-Cu Sputter-Coated Ti Brazing Filler [J].
Emadinia, Omid ;
Guedes, Anibal ;
Tavares, Carlos Jose ;
Simoes, Sonia .
MATERIALS, 2020, 13 (21) :1-14
[47]   Microstructure evolution of Si3N4/Si3N4 joint brazed with Ag-Cu-Ti plus SiCp composite filler [J].
Zhang, J. ;
He, Y. M. ;
Sun, Y. ;
Liu, C. F. .
CERAMICS INTERNATIONAL, 2010, 36 (04) :1397-1404
[48]   Microstructure and mechanical properties of SiO2-BN ceramic and Invar alloy joints brazed with Ag-Cu-Ti [J].
Wang, Y. ;
Yang, Z. W. ;
Zhang, L. X. ;
Wang, D. P. ;
Feng, J. C. .
JOURNAL OF MATERIOMICS, 2016, 2 (01) :66-74
[49]   Microstructure and mechanical properties of Si3N4/Si3N4 joint brazed with Ag-Cu-Ti plus SiCp composite filler [J].
He, Y. M. ;
Zhang, J. ;
Liu, C. F. ;
Sun, Y. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (12) :2819-2825
[50]   Effect of Ti Content on Microstructure and Mechanical Properties of Si3N4/Si3N4 Joints Brazed with Ag-Cu-Ti plus Mo Composite Filler [J].
Zhang, Jie ;
He, Yanming .
PRICM 7, PTS 1-3, 2010, 654-656 :2018-2021