Effect of manganese on mechanical properties and deformation mechanism of CoCrFeNi high entropy alloys

被引:8
作者
Chang, Man-Ping [1 ]
Fang, Te-Hua [2 ]
Zhu, Ting-Yu [2 ]
Lin, Jau-Wen [2 ]
机构
[1] Natl United Univ, Dept Mat Sci & Engn, Miaoli 36063, Taiwan
[2] Natl Kaohsiung Univ Sci & Technol, Dept Mech Engn, Kaohsiung 807, Taiwan
关键词
High-entropy alloys; Phase transformation; Toughness; Mechanical properties; PHASE-STABILITY; FRACTURE-TOUGHNESS; STAINLESS-STEELS; SINGLE-PHASE; MICROSTRUCTURE; CRMNFECONI; STRENGTH; BEHAVIORS; STRESS;
D O I
10.1016/j.mtcomm.2023.105844
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this study, the predominant mechanical properties and deformation mechanisms of CoCrFeNiMnx high entropy alloys (HEAs) were explored by using the molecular dynamics (MD) simulation. A uniaxial tensile process with different temperatures (100-700 K) and compositions of manganese (x = 0, 5, 10 and 20) were conducted. Besides, a circular defect was created on the CoCrFeNiMnx HEAs to investigate the damage tolerance of these HEAs. The equiatomic CoCrFeNiMn HEA performed a strongly temperature dependence. The ultimate tensile strength (UTS) was 4.83 GPa at 100 K, and was decreased with the temperature increased. Based on the dislocation distribution and von Mises strain results, the early stage deformation was governed by the 1/2 < 110 >-type dislocation slip. On the contrary, the grain boundaries glide was dominated the later stage deformation. In addition, the manganese content in this work was higher than the limit to form the face-centered cubic (FCC) single phase solid solution. Instead, hexagonal close-packed (HCP) and amorphous phases appeared, and thus decreased the strength of CoCrFeNiMnx HEAs. The Mn0 HEA showed the highest yield stress, UTS and Young's modulus, which were 4.9, 4.8 and 218.4 GPa, respectively. In addition, the damage tolerance of these HEAs was enhanced by the amorphous phase formation, which inhibited the propagation of cracks and improved the ductility. Based on the results, the Mn5 HEA presented the best damage tolerance than others.
引用
收藏
页数:11
相关论文
共 56 条
[41]   Deformation-induced crystalline-to-amorphous phase transformation in a CrMnFeCoNi high-entropy alloy [J].
Wang, Hao ;
Chen, Dengke ;
An, Xianghai ;
Zhang, Yin ;
Sun, Shijie ;
Tian, Yanzhong ;
Zhang, Zhefeng ;
Wang, Anguo ;
Liu, Jinqiao ;
Song, Min ;
Ringer, Simon P. ;
Zhu, Ting ;
Liao, Xiaozhou .
SCIENCE ADVANCES, 2021, 7 (14)
[42]   Novel microstructure and properties of multicomponent CoCrCuFeNiTix alloys [J].
Wang, X. F. ;
Zhang, Y. ;
Qiao, Y. ;
Chen, G. L. .
INTERMETALLICS, 2007, 15 (03) :357-362
[43]   Microstructure and compressive properties of AlCrFeCoNi high entropy alloy [J].
Wang, Y. P. ;
Li, B. S. ;
Ren, M. X. ;
Yang, C. ;
Fu, H. Z. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 491 (1-2) :154-158
[44]   Microstructures and properties of Al0.3CoCrFeNiMnx high entropy alloys [J].
Wong, Sze-Kwan ;
Shun, Tao-Tsung ;
Chang, Chieh-Hsiang ;
Lee, Che-Fu .
MATERIALS CHEMISTRY AND PHYSICS, 2018, 210 :146-151
[45]   Effect of Ti on the wear behavior of AlCoCrFeNi high-entropy alloy during unidirectional and bi-directional sliding wear processes [J].
Xu, Zhen ;
Li, D. Y. ;
Chen, D. L. .
WEAR, 2021, 476
[46]   Multicomponent intermetallic nanoparticles and superb mechanical behaviors of complex alloys [J].
Yang, T. ;
Zhao, Y. L. ;
Tong, Y. ;
Jiao, Z. B. ;
Wei, J. ;
Cai, J. X. ;
Han, X. D. ;
Chen, D. ;
Hu, A. ;
Kai, J. J. ;
Lu, K. ;
Liu, Y. ;
Liu, C. T. .
SCIENCE, 2018, 362 (6417) :933-+
[47]   A novel, single phase, non-equiatomic FeMnNiCoCr high-entropy alloy with exceptional phase stability and tensile ductility [J].
Yao, M. J. ;
Pradeep, K. G. ;
Tasan, C. C. ;
Raabe, D. .
SCRIPTA MATERIALIA, 2014, 72-73 :5-8
[48]   Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes [J].
Yeh, JW ;
Chen, SK ;
Lin, SJ ;
Gan, JY ;
Chin, TS ;
Shun, TT ;
Tsau, CH ;
Chang, SY .
ADVANCED ENGINEERING MATERIALS, 2004, 6 (05) :299-303
[49]   Aluminum oxide from trimethylaluminum and water by atomic layer deposition: The temperature dependence of residual stress, elastic modulus, hardness and adhesion [J].
Ylivaara, Oili M. E. ;
Liu, Xuwen ;
Kilpi, Lauri ;
Lyytinen, Jussi ;
Schneider, Dieter ;
Laitinen, Mikko ;
Julin, Jaakko ;
Ali, Saima ;
Sintonen, Sakari ;
Berdova, Maria ;
Haimi, Eero ;
Sajavaara, Timo ;
Ronkainen, Helena ;
Lipsanen, Harri ;
Koskinen, Jari ;
Hannula, Simo-Pekka ;
Puurunen, Riikka L. .
THIN SOLID FILMS, 2014, 552 :124-135
[50]   Effect of stacking fault energy on mechanical behavior of bulk nanocrystalline Cu and Cu alloys [J].
Youssef, Khaled ;
Sakaliyska, Miroslava ;
Bahmanpour, Hamed ;
Scattergood, Ronald ;
Koch, Carl .
ACTA MATERIALIA, 2011, 59 (14) :5758-5764