Sustainable and recyclable thermosets with performances for high technology sectors. An environmental friendly alternative to toxic derivatives

被引:3
作者
Dinu, Roxana [1 ]
Lafont, Ugo [2 ]
Damiano, Olivier [3 ]
Mija, Alice [1 ]
机构
[1] Univ Cote Azur, Inst Chim Nice, Nice, France
[2] European Space Agcy, European Space Res & Technol Ctr, Noordwijk, Netherlands
[3] Thales Alenia Space, Cannes, France
关键词
thermosets; biobased materials; natural and renewable raw materials; high-end properties; recyclability; PHTHALIC-ANHYDRIDE; WATER SORPTION; EPOXY-RESIN; DIFFUSION;
D O I
10.3389/fmats.2023.1242507
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This study focuses on the development of environmentally friendly and chemically recyclable thermosets using or a renewable based monomer, the triglycidyl ether of phloroglucinol (TGPh), or a commercial non-toxic tris(4-hydroxyphenyl) methane triglycidyl ether (THPMTGE) monomer. The recyclable polyester thermosets were prepared by crosslinking the two monomers with hexahydro-4-methylphthalic anhydride (HMPA) or methyl nadic anhydride The TGPh-based formulations exhibited lower reaction temperatures and narrower reaction intervals. Additionally, these systems showed higher tan d values (189 degrees C-199 degrees C), higher crosslinking densities (7.6-7.8 mmol cm(-3)) and compact networks, crucial for high-performance industries. Tensile tests demonstrated the remarkable mechanical properties of the thermosets, including high Young modulus (1.3-1.4 GPa), tensile stress (55-69 MPa), and an elongation at break around 3%-8%. Moreover, the thermosets exhibited complete dissolution at a temperature of 170 degrees C, with depolymerization times of approximately 2.5 h for TGPh-based resins and 4.5 h for THPMTGE-based formulations. In conclusion, this study shows that sustainable and eco-friendly thermosets with excellent physico-chemical and thermo-mechanical properties, low hydrophilicity, and rapid dissolution capacity can be developed. These thermosets offer a viable alternative to non-recyclable and toxic resins in high-end industrial applications.
引用
收藏
页数:11
相关论文
共 51 条
[1]  
Alabi OA., 2019, J Toxicol Risk Assess, V5, P21, DOI [10.23937/2572-4061.1510021, DOI 10.23937/2572-4061.1510021, 10.23937/2572, DOI 10.23937/2572]
[2]  
Andrews Hester E., 1920, PHTHALIC ANHYDRIDE
[3]  
ASTM, 2007, D57098 ASTM, DOI [10.1520/D0570-98R18, DOI 10.1520/D0570-98R18]
[4]  
ASTM-D2765-16, 2016, ASTMD276516
[5]   Impact of polar groups concentration and free volume on water sorption in model epoxy free films and coatings [J].
Bouvet, G. ;
Dang, Nguyen ;
Cohendoz, S. ;
Feaugas, X. ;
Mallarino, S. ;
Touzain, S. .
PROGRESS IN ORGANIC COATINGS, 2016, 96 :32-41
[6]   Eco-friendly synthesis of cardanol-based AB monomer for formaldehyde-free phenolic thermosets [J].
Briou, Benoit ;
Jego, Lucas ;
Miguel, Thomas De Dios ;
Duguet, Nicolas ;
Caillol, Sylvain .
RSC SUSTAINABILITY, 2023, 1 (04) :994-1005
[7]   Sliding wear, viscoelasticity, and brittleness of polymers [J].
Brostow, Witold ;
Lobland, Haley E. Hagg ;
Narkis, Moshe .
JOURNAL OF MATERIALS RESEARCH, 2006, 21 (09) :2422-2428
[8]   The concept of materials brittleness and its applications [J].
Brostow, Witold ;
Lobland, Haley E. Hagg ;
Narkis, Moshe .
POLYMER BULLETIN, 2011, 67 (08) :1697-1707
[9]   Brittleness of materials: implications for composites and a relation to impact strength [J].
Brostow, Witold ;
Lobland, Haley E. Hagg .
JOURNAL OF MATERIALS SCIENCE, 2010, 45 (01) :242-250
[10]   Diffusion and hydrolysis effects during water aging on an epoxyanhydride system [J].
Capiel, Guillermina ;
Uicich, Julieta ;
Fasce, Diana ;
Montemartini, Pablo E. .
POLYMER DEGRADATION AND STABILITY, 2018, 153 :165-171