Effects of microstrcture composition and orientation on micro mechanical properties of linear friction welding joint weld zone for heteromorphic TC17 titanium alloy

被引:3
|
作者
Xiao, Xuan [1 ]
Mao, Yue [1 ]
Qin, Dingqiang [1 ]
Wang, Xincheng [1 ]
Fu, Li [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Shaanxi Key Lab Frict Welding Technol, Xian 710072, Shaanxi, Peoples R China
关键词
NANO-INDENTATION METHODS; PLASTIC PROPERTIES; TI-5AL-2SN-2ZR-4MO-4CR TI17; MICROSTRUCTURE; METALS;
D O I
10.1007/s10853-023-09008-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, the microstructure and micro mechanical property of linear friction welded joint for heteromorphic TC17 titanium alloy were investigated by nanoindentation testing and electron backscatter diffraction technique. The results show that the special microstructure in the weld zone (WZ) of the joint has great effects on its micro mechanical property. The WZ is composed of the transformed beta phase, which exists in the form of equiaxed substructure, and the microstructure of the WZ can be divided into two parts along the centerline of the weld based on its main orientation. The WZ of the TC17 (alpha + beta) side has the main orientation < 112 > and < 111 >, while the TC17 (beta) side has the main orientation < 101 >. Meanwhile, more high angle grain boundaries (HAGB) are found in the WZ of the TC17 (alpha + beta) side. These microstructure characteristics have a significant impact on the micro mechanical property of the WZ. Due to more HAGB are in the WZ of the TC17 (alpha + beta) side than the TC17 (beta) side, the interface strengthening effect is a slightly stronger in the TC17 (alpha + beta) side, which leads to better elastic modulus, hardness, and fracture toughness. While the TC17 (alpha + beta) side microstructure has the {101} < 111 > and {112} < 111 > slip modes that are easier activated under RD direction force, so the microstructure in the WZ of the TC17 (alpha + beta) side has a smaller yield strength and a larger hardening exponent than that in the WZ of the TC17 (beta) side. In addition, it was also found that the area in the edge of the WZ near thermo-mechanically affected zone of the TC17 (alpha + beta) side (TC17 (alpha + beta)-TMAZ) has the minimum micro mechanical property and is the weak area of the WZ, which is related to the lower degree of recrystallization compared to other areas of the WZ. This area has the smallest elastic modulus (146.4 MPa), hardness (3.4 GPa), yield strength (904 MPa), and fracture toughness (0.173 MPa*m1/2), while the hardening exponent is 0.107. The macro tensile fracture location also matches the weak area in the WZ of the joints. Besides, it was also found that the average yield strength and tensile strength of the joint are 1016 MPa and 1065 MPa, while the elastic modulus and elongation are 111.2 GPa and 2.1%. And the microhardness distribution of the joint presents a "w" shape, which is due to lower phase alpha/beta interface content in the WZ of the LFW joint for heteromorphic TC17 alloy and leads to the minimum mechanical property.
引用
收藏
页码:16208 / 16224
页数:17
相关论文
共 48 条
  • [41] Effects of heterogeneity and coarse secondary phases on mechanical properties of 7050-T7451 aluminum alloy friction stir welding joint
    Liu, Yong
    Deng, Caiyan
    Gong, Baoming
    Bai, Yanan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 764
  • [42] Effect of three-stage heat treatment on mechanical properties and micro-deformation mechanism of TC4 titanium alloy welded joint
    Su, Rui
    Li, Haizhou
    Wang, Dirui
    Guo, Jinquan
    Wang, Chuangwei
    Li, Zhengrong
    Zeng, Han
    Sun, Zhongtao
    Chen, Hui
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 6753 - 6770
  • [43] Effects of Welding Speed and Post-weld Hot Rolling on Microstructure and Mechanical Properties of Friction Stir-Welded AZ31 Magnesium Alloy
    Gang Liu
    Li-Na Ma
    Zhen-Duo Ma
    Xue-Song Fu
    Guo-Bing Wei
    Yan Yang
    Tian-Cai Xu
    Wei-Dong Xie
    Xiao-Dong Peng
    Acta Metallurgica Sinica(English Letters), 2018, 31 (08) : 853 - 864
  • [44] Effects of Welding Speed and Post-weld Hot Rolling on Microstructure and Mechanical Properties of Friction Stir-Welded AZ31 Magnesium Alloy
    Liu, Gang
    Ma, Li-Na
    Ma, Zhen-Duo
    Fu, Xue-Song
    Wei, Guo-Bing
    Yang, Yan
    Xu, Tian-Cai
    Xie, Wei-Dong
    Peng, Xiao-Dong
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2018, 31 (08) : 853 - 864
  • [45] Effects of Welding Speed and Post-weld Hot Rolling on Microstructure and Mechanical Properties of Friction Stir-Welded AZ31 Magnesium Alloy
    Gang Liu
    Li-Na Ma
    Zhen-Duo Ma
    Xue-Song Fu
    Guo-Bing Wei
    Yan Yang
    Tian-Cai Xu
    Wei-Dong Xie
    Xiao-Dong Peng
    Acta Metallurgica Sinica (English Letters), 2018, 31 : 853 - 864
  • [46] Interface development and microstructure evolution during double-sided friction stir spot welding of magnesium alloy by adjustable probes and their effects on mechanical properties of the joint
    Wang, Xiaopei
    Morisada, Yoshiaki
    Fujii, Hidetoshi
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2021, 294
  • [47] Microstructural evolution and mechanical properties of a linear friction welded two-phase Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy joint
    Wang, Xinyu
    Li, Wenya
    Ma, Tiejun
    Yang, Xiawei
    Vairis, Achilles
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 743 : 12 - 23
  • [48] Friction welding of two carbon low alloy steels 42CrMo and 36Mn2V: Effects of forging pressure and post-weld heat treatment on microstructure and mechanical properties
    Lu, Tian
    Li, Wenya
    Wang, Chuanliu
    Tian, Dongzhuang
    WELDING IN THE WORLD, 2025, 69 (02) : 383 - 395