Effects of microstrcture composition and orientation on micro mechanical properties of linear friction welding joint weld zone for heteromorphic TC17 titanium alloy

被引:3
|
作者
Xiao, Xuan [1 ]
Mao, Yue [1 ]
Qin, Dingqiang [1 ]
Wang, Xincheng [1 ]
Fu, Li [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Shaanxi Key Lab Frict Welding Technol, Xian 710072, Shaanxi, Peoples R China
关键词
NANO-INDENTATION METHODS; PLASTIC PROPERTIES; TI-5AL-2SN-2ZR-4MO-4CR TI17; MICROSTRUCTURE; METALS;
D O I
10.1007/s10853-023-09008-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, the microstructure and micro mechanical property of linear friction welded joint for heteromorphic TC17 titanium alloy were investigated by nanoindentation testing and electron backscatter diffraction technique. The results show that the special microstructure in the weld zone (WZ) of the joint has great effects on its micro mechanical property. The WZ is composed of the transformed beta phase, which exists in the form of equiaxed substructure, and the microstructure of the WZ can be divided into two parts along the centerline of the weld based on its main orientation. The WZ of the TC17 (alpha + beta) side has the main orientation < 112 > and < 111 >, while the TC17 (beta) side has the main orientation < 101 >. Meanwhile, more high angle grain boundaries (HAGB) are found in the WZ of the TC17 (alpha + beta) side. These microstructure characteristics have a significant impact on the micro mechanical property of the WZ. Due to more HAGB are in the WZ of the TC17 (alpha + beta) side than the TC17 (beta) side, the interface strengthening effect is a slightly stronger in the TC17 (alpha + beta) side, which leads to better elastic modulus, hardness, and fracture toughness. While the TC17 (alpha + beta) side microstructure has the {101} < 111 > and {112} < 111 > slip modes that are easier activated under RD direction force, so the microstructure in the WZ of the TC17 (alpha + beta) side has a smaller yield strength and a larger hardening exponent than that in the WZ of the TC17 (beta) side. In addition, it was also found that the area in the edge of the WZ near thermo-mechanically affected zone of the TC17 (alpha + beta) side (TC17 (alpha + beta)-TMAZ) has the minimum micro mechanical property and is the weak area of the WZ, which is related to the lower degree of recrystallization compared to other areas of the WZ. This area has the smallest elastic modulus (146.4 MPa), hardness (3.4 GPa), yield strength (904 MPa), and fracture toughness (0.173 MPa*m1/2), while the hardening exponent is 0.107. The macro tensile fracture location also matches the weak area in the WZ of the joints. Besides, it was also found that the average yield strength and tensile strength of the joint are 1016 MPa and 1065 MPa, while the elastic modulus and elongation are 111.2 GPa and 2.1%. And the microhardness distribution of the joint presents a "w" shape, which is due to lower phase alpha/beta interface content in the WZ of the LFW joint for heteromorphic TC17 alloy and leads to the minimum mechanical property.
引用
收藏
页码:16208 / 16224
页数:17
相关论文
共 48 条
  • [21] Microstructure Characteristics and Mechanical Properties of Inertia Friction Welding Joint of α plus ß Titanium Alloy in Welding State/Post-Weld Heat Treatment State
    Wu Yanquan
    Zhou Jun
    Zhang Chunbo
    Liang Wu
    Li Rui
    Qin Feng
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (06) : 2144 - 2150
  • [22] Microstructure and mechanical properties of linear friction welding joint of TC21/TC4-DT
    Zhang C.
    Zhang T.
    Jin J.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 133 - 137
  • [23] Microstructure and Mechanical Properties of TC4 Titanium Alloy Joint Fabricated By Vortex Flow-Based Friction Stir Welding
    Liu, Xiaochao
    Zhang, Pengyu
    Li, Wentao
    Ye, Tao
    Xia, Chuanchao
    Zhang, Tairui
    Shi, Junmiao
    Xie, Jilin
    Ni, Zhonghua
    CHINESE JOURNAL OF MECHANICAL ENGINEERING, 2024, 37 (01)
  • [24] Linear friction welding of a beta titanium alloy: experimental investigations on microstructure evolution and mechanical properties
    Wang, Xinyu
    Li, Wenya
    Ye, Qing
    Yang, Xiawei
    Ma, Tiejun
    Vairis, Achilles
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2020, 25 (08) : 625 - 636
  • [25] Influence of Welded Pores on Very Long-Life Fatigue Failure of the Electron Beam Welding Joint of TC17 Titanium Alloy
    Liu, Fulin
    Zhang, Hong
    Liu, Hanqing
    Chen, Yao
    Kashif, Khan Muhammad
    Wang, Qingyuan
    Liu, Yongjie
    MATERIALS, 2019, 12 (11)
  • [26] Effect of Tool-Pin Profile on Weld Zone and Mechanical Properties in Friction Stir Welding of Aluminium Alloy
    Prakash, Prashant
    Jha, Sanjay Kumar
    Lal, Shree Prakash
    PERTANIKA JOURNAL OF SCIENCE AND TECHNOLOGY, 2018, 26 (02): : 853 - 862
  • [27] Microstructure and Mechanical Properties of Heat Treatment TA15/ TC17 Titanium Alloy by Laser Deposition Repair
    Bian H.
    Zuo S.
    Qu S.
    Yang G.
    Wang W.
    Xiyou Jinshu/Chinese Journal of Rare Metals, 2020, 44 (05): : 455 - 461
  • [28] Microstructural and mechanical properties of a beta-type titanium alloy joint fabricated by friction stir welding
    Liu, Huihong
    Fujii, Hidetoshi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 711 : 140 - 148
  • [29] Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint
    Ma, T. J.
    Li, W. Y.
    Zhong, B.
    Zhang, Y.
    Li, J. L.
    SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2012, 17 (03) : 180 - 185
  • [30] Microstructure and mechanical properties of joint welds formed by linear friction welding in Al-Cu-Mg alloy
    Kiselyeva, S.K.
    Astanin, Vas V.
    Gareeva, L.
    Bychkov, V.M.
    Medvedev, A.Y.
    Musin, F.F.
    Alexandrov, I.V.
    Journal of Engineering Science and Technology Review, 2014, 7 (05) : 32 - 35