Effects of microstrcture composition and orientation on micro mechanical properties of linear friction welding joint weld zone for heteromorphic TC17 titanium alloy

被引:3
|
作者
Xiao, Xuan [1 ]
Mao, Yue [1 ]
Qin, Dingqiang [1 ]
Wang, Xincheng [1 ]
Fu, Li [1 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Shaanxi Key Lab Frict Welding Technol, Xian 710072, Shaanxi, Peoples R China
关键词
NANO-INDENTATION METHODS; PLASTIC PROPERTIES; TI-5AL-2SN-2ZR-4MO-4CR TI17; MICROSTRUCTURE; METALS;
D O I
10.1007/s10853-023-09008-y
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, the microstructure and micro mechanical property of linear friction welded joint for heteromorphic TC17 titanium alloy were investigated by nanoindentation testing and electron backscatter diffraction technique. The results show that the special microstructure in the weld zone (WZ) of the joint has great effects on its micro mechanical property. The WZ is composed of the transformed beta phase, which exists in the form of equiaxed substructure, and the microstructure of the WZ can be divided into two parts along the centerline of the weld based on its main orientation. The WZ of the TC17 (alpha + beta) side has the main orientation < 112 > and < 111 >, while the TC17 (beta) side has the main orientation < 101 >. Meanwhile, more high angle grain boundaries (HAGB) are found in the WZ of the TC17 (alpha + beta) side. These microstructure characteristics have a significant impact on the micro mechanical property of the WZ. Due to more HAGB are in the WZ of the TC17 (alpha + beta) side than the TC17 (beta) side, the interface strengthening effect is a slightly stronger in the TC17 (alpha + beta) side, which leads to better elastic modulus, hardness, and fracture toughness. While the TC17 (alpha + beta) side microstructure has the {101} < 111 > and {112} < 111 > slip modes that are easier activated under RD direction force, so the microstructure in the WZ of the TC17 (alpha + beta) side has a smaller yield strength and a larger hardening exponent than that in the WZ of the TC17 (beta) side. In addition, it was also found that the area in the edge of the WZ near thermo-mechanically affected zone of the TC17 (alpha + beta) side (TC17 (alpha + beta)-TMAZ) has the minimum micro mechanical property and is the weak area of the WZ, which is related to the lower degree of recrystallization compared to other areas of the WZ. This area has the smallest elastic modulus (146.4 MPa), hardness (3.4 GPa), yield strength (904 MPa), and fracture toughness (0.173 MPa*m1/2), while the hardening exponent is 0.107. The macro tensile fracture location also matches the weak area in the WZ of the joints. Besides, it was also found that the average yield strength and tensile strength of the joint are 1016 MPa and 1065 MPa, while the elastic modulus and elongation are 111.2 GPa and 2.1%. And the microhardness distribution of the joint presents a "w" shape, which is due to lower phase alpha/beta interface content in the WZ of the LFW joint for heteromorphic TC17 alloy and leads to the minimum mechanical property.
引用
收藏
页码:16208 / 16224
页数:17
相关论文
共 48 条
  • [1] Structure and mechanical property of wedge linear friction welding joint of TC17 titanium alloy
    Jin J.
    Tao J.
    Ji Y.
    Zhang C.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2021, 42 (05): : 18 - 22
  • [2] Microstructure and mechanical properties of linear friction welding joint of TC17 titanium alloy fabricated by laser forming
    Jin J.
    Guo D.
    Liu Q.
    Zhang T.
    Ji Y.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (06): : 126 - 130
  • [3] Influence of heat treatment on microstructure and mechanical properties of TC17(α+β)/TC17(β) linear friction welding joint
    Li J.
    Zhang T.
    Guo D.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2018, 39 (05): : 97 - 100and120
  • [4] Study of the Microstructure and Fracture Toughness of TC17 Titanium Alloy Linear Friction Welding Joint
    Li, Xiaohong
    He, Jianchao
    Ji, Yajuan
    Zhang, Tiancang
    Zhang, Yanhua
    METALS, 2019, 9 (04):
  • [5] Structure and mechanical property of TC17 linear friction welding joint
    Ji Y.
    Zhang T.
    Zhang L.
    Guo D.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (09): : 156 - 160
  • [6] Study on Linear Friction Welding Process and Microstructure Analysis of TC17 Titanium Alloy
    Li Ju
    Chang Chuanchuan
    Li Xiaohong
    Tao Jun
    Zhang Chuanchen
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (03) : 940 - 946
  • [7] Study on Residual Stress and Optimization of Welding Parameters in Linear Friction Welding of TC17 Titanium Alloy
    Gong, Hai
    Liu, Meiqin
    Zhang, Tao
    He, Yongbiao
    Wu, Yunxin
    Yu, Zhouxiang
    MATERIALS, 2022, 15 (24)
  • [8] Residual stresses in linear friction welding of TC17 titanium alloy considering phase fraction
    He, Peng
    Wu, Yun-xin
    Zhang, Tao
    Chen, Song-yi
    Zhang, Chen
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2024, 34 (01) : 184 - 193
  • [9] Enhancing the mechanical properties of electron beam welded TC17 titanium alloy joint by post-weld heat treatment
    Liu, Hanging
    Wang, Haomin
    Zhang, Zhen
    Huang, Zhiyong
    Liu, Yongjie
    Wang, Qingyuan
    Chen, Qiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 810
  • [10] Microstructure and properties of linear friction welded joint of hyperoxia TC4/TC17 dissimilar titanium alloys
    Chang C.
    Zhang T.
    Li J.
    Liu J.
    Hanjie Xuebao/Transactions of the China Welding Institution, 2019, 40 (12): : 109 - 114and120