Preparing hydrophobic alkali-activated slag mortar with lotus-leaf-like microstructure by adding polydimethylsiloxane (PDMS)

被引:10
作者
Tang, Desha [1 ]
Yang, Changhui [1 ,2 ]
Shen, Chen [1 ]
Yu, Linwen [1 ,2 ]
Tian, Yi [1 ,3 ]
Zhu, Xiaohong [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
[2] Chongqing Engn Res Ctr High Performance Concrete, Chongqing 400045, Peoples R China
[3] Cent South Univ, Sch Civil Engn, Changsha, Peoples R China
基金
中国国家自然科学基金;
关键词
Alkali-activated slag; Polydimethylsiloxane (PDMS); Hydrophobic; Micro papillary; INVERSE GAS-CHROMATOGRAPHY; SURFACE HETEROGENEITY; SODIUM-HYDROXIDE; SULFATE ATTACK; PORE STRUCTURE; CONTACT-ANGLE; CEMENT PASTES; CONCRETE; STRENGTH; DURABILITY;
D O I
10.1016/j.conbuildmat.2023.134148
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this study, polydimethylsiloxane (PDMS) was applied for overall hydrophobic modification of alkali-activated slag (AAS) mortars aiming to reduce its high water sorptivity. The effects of the amount and viscosity of PDMS on the water absorption characteristics and mechanical properties of AAS mortars were investigated. Meanwhile, MIP, the surface contact angle of AAS mortars and SEM-EDS, Inverse gas chromatography (IGC), FT-IR, XRD of hardened AAS pastes were performed for analyzing the modification mechanisms. The results indicated that the water sorptivity of PDMS-modified AAS mortar decreased by 90 %, and the contact angle of the inner surface increased from 14 degrees to 128 degrees when the dosage of PDMS reached 8 % (by weight of binder). The main modification mechanisms of PDMS in AAS system can be summarized as: Firstly, the formation of hydrophobic coatings on the surface due to the cross-linking reaction between C-S-H gel and PDMS reduces the surface energy and the hydrophilicity of hardened AAS pastes, achieving chemical modification; Secondly, the hierarchical structures formed by micro papillary increases the surface roughness, thus enhancing the hydrophobic effect further through physical modification. Moreover, the coarsening of capillary pores also reduces the capillary force during water absorption process. Meanwhile, the addition of PMDS maintains comparable strength development of AAS mortars, which is beneficial for the practical application.
引用
收藏
页数:14
相关论文
共 85 条
[1]   Introducing inverse gas chromatography as a method of determining the surface heterogeneity of minerals for flotation [J].
Ali, S. S. M. ;
Heng, J. Y. Y. ;
Nikolaev, A. A. ;
Waters, K. E. .
POWDER TECHNOLOGY, 2013, 249 :373-377
[2]  
[Anonymous], 1999, 176711999 GBT
[3]   The effect of fiber properties on high performance alkali-activated slag/silica fume mortars [J].
Aydin, Serdar ;
Baradan, Bulent .
COMPOSITES PART B-ENGINEERING, 2013, 45 (01) :63-69
[4]   Resistance of alkali-activated slag concrete to acid attack [J].
Bakharev, T ;
Sanjayan, JG ;
Cheng, YB .
CEMENT AND CONCRETE RESEARCH, 2003, 33 (10) :1607-1611
[5]   Sulfate attack on alkali-activated slag concrete [J].
Bakharev, T ;
Sanjayan, JG ;
Cheng, YB .
CEMENT AND CONCRETE RESEARCH, 2002, 32 (02) :211-216
[6]   Optimum design of alkali activated slag concretes for the low oxygen/chloride ion permeability and thermal conductivity [J].
Balcikanli, Mtizeyyen ;
Ozbay, Erdogan .
COMPOSITES PART B-ENGINEERING, 2016, 91 :243-256
[7]   Influence of activator type on hydration kinetics, hydrate assemblage and microstructural development of alkali activated blast-furnace slags [J].
Ben Haha, M. ;
Le Saout, G. ;
Winnefeld, F. ;
Lothenbach, B. .
CEMENT AND CONCRETE RESEARCH, 2011, 41 (03) :301-310
[8]  
Cassie A.B.D, Wettability of Porous Surfaces
[9]   Experimental Study on the Durability of Alkali-Activated Slag Concrete after Freeze-Thaw Cycle [J].
Chen, Bin ;
Wang, Jun .
ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2021, 2021
[10]   Deterioration mechanism of plain and blended cement mortars partially exposed to sulfate attack [J].
Chen, Fei ;
Gao, Jianming ;
Qi, Bing ;
Shen, Daman .
CONSTRUCTION AND BUILDING MATERIALS, 2017, 154 :849-856