Effects of Overload on Thermal Decomposition Kinetics of Cross-Linked Polyethylene Copper Wires

被引:0
|
作者
Jia, Yizhuo [1 ]
Man, Pengrui [1 ]
Guo, Xinyao [1 ]
Deng, Liang [1 ]
Li, Yang [1 ]
机构
[1] China Peoples Police Univ, Forens Sci Inst, Langfang 065000, Peoples R China
关键词
overload fault; cross-linked polyethylene copper wire; thermal decomposition; reaction mechanism; functional group; PYROLYSIS; DEGRADATION; COMBUSTION; POLYMERS; FTIR; PE;
D O I
10.3390/polym15193954
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
During an overload fault in an energized wire, the hot metal core modifies the structure of the insulation material. Therefore, understanding the thermal decomposition kinetics of the insulation materials of the overloaded wire is essential for fire prevention and control. This study investigates the thermal decomposition process of new and overloaded cross-linked polyethylene (XLPE) copper wires using thermogravimetry-Fourier-transform infrared spectroscopy and cone calorimetry. The thermal decomposition onset temperature and activation energy of the overloaded XLPE insulation materials were reduced by approximately 15 K and 20 kJ mol(-1), respectively, and its reaction mechanism function changed from D-ZLT(3) to A2 (0 < alpha < 0.5). The FTIR shows that the major spectral components produced during the pyrolysis of the XLPE insulation material are C-H stretching, H2O, CO2, C-H scissor vibrations, and C=O and C=C stretching. Additionally, the four functional groups in the PE chains produced the spectral components in the following decreasing order of wavenumber: C-H stretching > CO2 > C-H scissor vibration > C=O and C=C stretching.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] THERMAL ANALYSES OF CROSS-LINKED POLYETHYLENE
    Polansky, R.
    ADVANCES IN ELECTRICAL AND ELECTRONIC ENGINEERING, 2007, 6 (03) : 121 - 126
  • [2] Thermal aging of cross-linked polyethylene
    Boukezzi, Larbi
    Nedjar, Mohammed
    Mokhnache, Leila
    Lallouani, Mohamed
    Boubakeur, Ahmed
    ANNALES DE CHIMIE-SCIENCE DES MATERIAUX, 2006, 31 (05): : 561 - 569
  • [3] INFLUENCE OF COPPER ON THE THERMAL-OXIDATION STABILITY OF CROSS-LINKED POLYETHYLENE
    VONGENTZKOW, W
    PIEPER, D
    SIEMENS FORSCHUNGS-UND ENTWICKLUNGSBERICHTE-SIEMENS RESEARCH AND DEVELOPMENT REPORTS, 1979, 8 (06): : 309 - 312
  • [4] KINETICS OF THERMAL-DECOMPOSITION OF CROSS-LINKED POLY(ETHER URETHANE) ELASTOMERS
    VOLKOVA, NN
    OLKHOV, YA
    BATURIN, SM
    SMIRNOV, LP
    VYSOKOMOLEKULYARNYE SOEDINENIYA SERIYA A, 1978, 20 (01): : 199 - 206
  • [5] The composites of cross-linked polyethylene with enhanced thermal conductivity
    Latko-Duralek, Paulina
    Salasinska, Kamila
    Kubis, Michal
    Kozera, Paulina
    Pietrak, Karol
    Rojewski, Szymon
    Jurczyk-Kowalska, Magdalena
    Szlazak, Karol
    Lapka, Piotr
    Boczkowska, Anna
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2024, 149 (10) : 4385 - 4396
  • [6] THERMAL-OXIDATION OF PHOTOCHEMICALLY CROSS-LINKED POLYETHYLENE
    LITSOV, NI
    JAKOVLEV, VB
    NIKOLAEVSKAJA, VI
    POLYMER DEGRADATION AND STABILITY, 1991, 32 (01) : 1 - 7
  • [7] Thermal conductivity of silane cross-linked polyethylene composites
    Poostforush, Md.
    Azizi, H.
    Ghasemi, I.
    BULGARIAN CHEMICAL COMMUNICATIONS, 2016, 48 : 125 - 130
  • [8] Thermal decomposition of cross-linked polybutadiene and its copolymers
    Jiang, DD
    Levchik, GF
    Levchik, SV
    Wilkie, CA
    POLYMER DEGRADATION AND STABILITY, 1999, 65 (03) : 387 - 394
  • [9] MORPHOLOGY OF CROSS-LINKED POLYETHYLENE
    不详
    EPRI JOURNAL, 1983, 8 (08): : 47 - 47
  • [10] PHOTODEGRADATION OF CROSS-LINKED POLYETHYLENE
    TORIKAI, A
    ASADA, S
    FUEKI, K
    POLYMER PHOTOCHEMISTRY, 1986, 7 (01): : 1 - 11