共 40 条
Porcelain Stoneware Tiles Based on Clays Mixture and Recycled Waste Glass Powder: Effect of Soaking Time
被引:1
作者:
Njindam, Oumarou Ramadan
[1
]
Njuhou, Saliou
[1
]
Pountouenchi, Amadou
[1
]
Mandou, Fadimatou Ngoungoure
[1
]
Mfomboum, Yacouba Kouotou
[1
]
Mountapbeme, Ibrahim Cherif
[1
]
Njoya, Iffat Qoudsiyyah Maury
[1
]
机构:
[1] Univ Yaounde I, Dept Inorgan Chem, Appl Inorgan Chem Lab, POB 812,3 315 Rue Univ, Yaounde, Cameroon
关键词:
Soaking time;
Waste glass powder;
Bloating;
Mechanical properties;
MECHANICAL-PROPERTIES;
TECHNOLOGICAL PROPERTIES;
FIRING TEMPERATURE;
CERAMIC PROPERTIES;
FLEXURAL STRENGTH;
RAW-MATERIAL;
MICROSTRUCTURE;
PHASE;
OPTIMIZATION;
EVOLUTION;
D O I:
10.1080/0371750X.2023.2274543
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
The effect of soaking time on the properties of porcelain stoneware tiles based on clay mixture and recycled waste glass powder was studied. Mixture was prepared and fired at 1150 degrees C. During firing, raw mixture was subjected to various soaking times: 30, 60, 90 and 120 min. The by-products were characterized by their linear shrinkage, water absorption, bulk density, flexural strength, X-ray diffraction (XRD) and scanning electron microscopy (SEM). The results were modelled by using different mathematical expressions. The results demonstrated that physico-mechanical properties of ceramic probe are significantly affected by soaking time. After 30 min, products satisfied the ISO 13006 standard condition for porcelain stoneware wall and floor tiles: water absorption value was lowest (0.07%) and mechanical strength value was 44.4 MPa. Prolonged soaking time was undesirable due to its negative effect (bloating) on the products' physical and mechanical performance. The XRD patterns indicated the presence of mullite, cristobalite, enstatite, anorthite, hematite and quartz as the main crystalline phases. SEM images of the tiles fired at 1150 degrees C for 30 min display a very close texture and dense microstructure.