Enhancement of low-temperature toughness of Fe-Mn-C-Al alloy by rare earth Ce-modified inclusions

被引:9
作者
Yang, Guang-kai [1 ]
Zhuang, Chang-ling [1 ,2 ]
Li, Yi-zhuang [3 ]
Hu, Chen [2 ]
Li, Shao-bo [4 ]
机构
[1] Guizhou Univ, Coll Mat & Met, Guiyang 550025, Guizhou, Peoples R China
[2] Univ Hong Kong, Dept Mech Engn, Hong Kong 999077, Peoples R China
[3] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Liaoning, Peoples R China
[4] Guizhou Univ, State Key Lab Publ Big Data, Guiyang 550025, Guizhou, Peoples R China
基金
中国国家自然科学基金;
关键词
Fe-Mn-C-Al alloy; Rare earth; Low-temperature toughness; Inclusion; Fracture; TWINNING-INDUCED PLASTICITY; CHARPY IMPACT TOUGHNESS; MECHANICAL-PROPERTIES; TWIP STEEL; MICROSTRUCTURE; AUSTENITE; EMBRITTLEMENT; EVOLUTION; STRENGTH; FRACTURE;
D O I
10.1007/s42243-023-01130-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Fe-Mn-C-Al alloys have been recognized as promising materials for certain low-temperature applications due to their exceptional mechanical properties and cost-effectiveness. However, their limited low-temperature toughness restricts their large-scale applications in specific scenarios. The influence of trace amounts of rare earth cerium (Ce) on the low-temperature toughness of Fe-18Mn-0.6C-1.8Al alloys was investigated. The addition of Ce effectively alters the inclusions in the alloy, transforming large-sized irregular inclusions into fine ellipsoidal rare earth inclusions. This leads to a significant reduction in both the proportion and average size of the inclusions, resulting in their effective dispersion throughout the matrix and improved cryogenic performance. The presence of Ce-containing inclusions within the matrix reduces stress concentration, thereby inhibiting microcrack formation and improving impact absorption energy. Specifically, the addition of rare earth Ce alters the fracture behavior of the material at room temperature and low temperature, changing from brittle cleavage fracture to a more ductile failure mode. The impact toughness of the Fe-Mn-C-Al alloy is significantly improved by the addition of 0.0048 wt.% Ce, particularly at - 196 degrees C where the impact toughness reaches 103.6 J/cm2, representing an impressive improvement of 87.3%.
引用
收藏
页码:157 / 173
页数:17
相关论文
共 50 条
[41]   Synergistic effect of the multi-factors and deformation mechanisms on the low-temperature impact toughness in Ti-6Al-4V-0.55Fe alloy [J].
Li, Feng ;
Zhan, Chao ;
Fan, Cuntie ;
Gao, Zhenyuan ;
Feng, Liang ;
Chang, Hui .
MATERIALS CHARACTERIZATION, 2025, 227
[42]   Promising elevated temperature mechanical properties of novel lightweight Fe47Mn25Al13Cr7Ni5C3 medium-entropy alloy [J].
Gu, Gang Hee ;
Lee, Jae Heung ;
Kwon, Hyeonseok ;
Kim, Hyoung Seop .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 893
[43]   Effect of hot deformation conditions on magnetic properties of rare earth free magnetic Mn-Al-C alloy [J].
Dehghan, H. ;
Ebrahimi, S. A. Seyyed .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2019, 477 :55-61
[44]   Intercritical Annealing Temperature: Influence on the Mechanical Properties of Low Alloy Dual-Phase Fe/0.08C/0.4Mn Steel [J].
Ogunmefun, Anthony Olakunle ;
Jamiru, Tamba ;
Sadiku, Emmanuel Rotimi ;
Obadele, Babatunde Abiodun ;
Olorundaisi, Emmanuel .
2019 OPEN INNOVATIONS CONFERENCE (OI), 2019, :141-146
[45]   Effect of Solution Treatment Temperature on Microstructure and Properties of Fe-0.72Mn-3.7Al-0.53C Low-Density Cast Steel [J].
Song, Nan ;
Zhao, Weimin ;
Dong, Lishan ;
Zhou, Xinshan .
METALS, 2022, 12 (08)
[46]   Enhancement of strength and ductility of Fe-13Al-16Mn-5Ni-0.8C steel by annealing at high temperature [J].
Kumar, Nikhil ;
Singh, Kritika ;
Singh, Aparna .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
[47]   Texture and structure contribution to low-temperature plasticity enhancement of Mg-Al-Zn-Mn Alloy MA2-1hp after ECAP and annealing [J].
Serebryany, V. N. ;
D'yakonov, G. S. ;
Kopylov, V. I. ;
Salishchev, G. A. ;
Dobatkin, S. V. .
PHYSICS OF METALS AND METALLOGRAPHY, 2013, 114 (05) :448-456
[48]   Texture and structure contribution to low-temperature plasticity enhancement of Mg-Al-Zn-Mn Alloy MA2-1hp after ECAP and annealing [J].
V. N. Serebryany ;
G. S. D’yakonov ;
V. I. Kopylov ;
G. A. Salishchev ;
S. V. Dobatkin .
The Physics of Metals and Metallography, 2013, 114 :448-456
[49]   Alloy Design, Combinatorial Synthesis, and Microstructure-Property Relations for Low-Density Fe-Mn-Al-C Austenitic Steels [J].
Raabe, D. ;
Springer, H. ;
Gutierrez-Urrutia, I. ;
Roters, F. ;
Bausch, M. ;
Seol, J. -B. ;
Koyama, M. ;
Choi, P. -P. ;
Tsuzaki, K. .
JOM, 2014, 66 (09) :1845-1856
[50]   Enhanced High-Temperature Strength of a Low-Density Dispersion-Strengthened Fe-Mn-Al-C Steel [J].
Wu, Zhiqiang ;
Hasan, Md Nzmul ;
Zhou, Honggang ;
Hu, Jun ;
Liu, Longfei ;
Lu, Liwei ;
An, Xianghai .
ADVANCED ENGINEERING MATERIALS, 2022, 24 (05)