Cementless binder based on high-calcium fly ash with calcium nitrate additive

被引:2
作者
Usanova, K. [1 ]
Barabanshchikov, Yu. G. [1 ]
Dixit, S. [2 ,3 ,4 ]
机构
[1] Peter Great St Petersburg Polytech Univ, St Petersburg, Russia
[2] Uttaranchal Univ, Div Res, Dehra Dun, India
[3] Lovely Profess Univ, Div Res & Dev, Phagwara, Punjab, India
[4] Khalifa Univ, Abu Dhabi, U Arab Emirates
来源
MAGAZINE OF CIVIL ENGINEERING | 2023年 / 124卷 / 08期
基金
俄罗斯科学基金会;
关键词
fly ash; microsilica; silica fume; early strength agent; calcium nitrate; X-ray diffraction analysis; strength; heat release; differential thermal analysis; heat of hydration; phase composition; SILICA FUME; EXPANSION; HYDRATION; PASTE;
D O I
10.34910/MCE.124.5
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Fly ash from Berezovskaya Thermal Power Plant, containing a lot of CaO, in combination with silica fume does not expand and exhibits the properties of a binder. However, the strength of this binder is low. The addition of Ca(NO3)2 significantly increases the strength of the binder. The work aims to study the effect of Ca(NO3)2 additive on the strength, heat of hydration, and phase composition of hydration products of the binder based on high-calcium fly ash and silica fume. The results of X-ray diffraction and Differential Thermal Analysis show that the main phases formed during the hydration of binder with the calcium nitrate additive in various dosages are lime, calcium hydroxide, ettringite, CSH(II) type silicates and calcium aluminosilicates, corresponding to such minerals as gismondine, yugavaralite, goosecreekite. When hardening in water, the residual amount of lime after 7 days is sharply reduced. An increase in the dosage of Ca(NO3)2 from 1.5 to 11.8 % leads to a decrease in the CaO content by almost 2 times. With an increase in the dosage of calcium nitrate, the content of portlandite noticeably decreases, and a significant increase in the amount of calcium hydroaluminosilicates, especially the composition of CAS2H4, is observed. A study of the heat release process showed that calcium nitrate greatly accelerates the process in the first 60 minutes of hydration. However, then the composition with the addition of Ca(NO3)2 is inferior in the rate of heat release to binder without the additive. When testing a mortar with polyfractional sand, the addition of Ca(NO3)2 more than doubled the compressive strength of the mortar.
引用
收藏
页数:14
相关论文
共 33 条
  • [1] A Step towards Concrete with Partial Substitution of Waste Glass (WG) in Concrete: A Review
    Ahmad, Jawad
    Zhou, Zhiguang
    Usanova, Kseniia Iurevna
    Vatin, Nikolai Ivanovich
    El-Shorbagy, Mohammed A.
    [J]. MATERIALS, 2022, 15 (07)
  • [2] Concrete with Partial Substitution of Waste Glass and Recycled Concrete Aggregate
    Ahmad, Jawad
    Martinez-Garcia, Rebeca
    de-Prado-Gil, Jesus
    Irshad, Kashif
    El-Shorbagy, Mohammed A.
    Fediuk, Roman
    Vatin, Nikolai Ivanovich
    [J]. MATERIALS, 2022, 15 (02)
  • [3] Demolition Waste Potential for Completely Cement-Free Binders
    Alani, Ahmed Anees
    Lesovik, Ruslan
    Lesovik, Valery
    Fediuk, Roman
    Klyuev, Sergey
    Amran, Mugahed
    Ali, Mujahid
    de Azevedo, Afonso R. G.
    Vatin, Nikolai Ivanovich
    [J]. MATERIALS, 2022, 15 (17)
  • [4] Influence of Silica Fume on High-Calcium Fly Ash Expansion during Hydration
    Barabanshchikov, Yurii
    Usanova, Kseniia
    [J]. MATERIALS, 2022, 15 (10)
  • [5] Influence of Electrostatic Precipitator Ash "Zolest-Bet" and Silica Fume on Sulfate Resistance of Portland Cement
    Barabanshchikov, Yury
    Usanova, Kseniia
    Akimov, Stanislav
    Uhanov, Aleksandr
    Kalachev, Andrej
    [J]. MATERIALS, 2020, 13 (21) : 1 - 13
  • [6] Physico-chemical interaction between mineral admixtures and OPC-calcium sulfoaluminate (CSA) cements and its influence on early-age expansion
    Chaunsali, Piyush
    Mondal, Paramita
    [J]. CEMENT AND CONCRETE RESEARCH, 2016, 80 : 10 - 20
  • [7] Effects of calcium nitrate and triisopropanolamine on the setting and strength evolution of Portland cement pastes
    Chikh, N.
    Cheikh-Zouaoui, M.
    Aggoun, S.
    Duval, R.
    [J]. MATERIALS AND STRUCTURES, 2008, 41 (01) : 31 - 36
  • [8] Study of the effect of calcium nitrate, calcium formate, triethanolamine, and triisopropanolamine on compressive strength of Portland-pozzolana cement
    Derakhshani, Aliakbar
    Ghadi, Arezoo
    Vahdat, Seyed Ebrahim
    [J]. CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 18
  • [9] ICSC Problems and Perspectives of highcalcium fly ash from heat power plants in the composition of "green" building materials
    Domanskaya, Irina
    Oleynik, Valentina
    Minyazev, Denis
    [J]. INTERNATIONAL CONFERENCE ON SUSTAINABLE CITIES (ICSC 2016), 2016, 6
  • [10] Working mechanism of calcium nitrate as an accelerator for Portland cement hydration
    Dorn, Tobias
    Hirsch, Tamino
    Stephan, Dietmar
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2023, 106 (01) : 752 - 766