Performance deterioration of municipal solid waste incineration fly ash-based geopolymer under sulfuric acid attack

被引:17
作者
Bai, Yanying [1 ,2 ]
Guo, Weichao [1 ,2 ]
Zhao, Qingxin [1 ,2 ]
Zhang, Ningtao [2 ]
Xue, Caihong [1 ,2 ]
Wang, Shuai [2 ]
Song, Yongpeng [2 ]
机构
[1] Yanshan Univ, State Key Lab Metastable Mat Sci & Technol, Qinhuangdao 066000, Peoples R China
[2] Yanshan Univ, Hebei Prov Engn Res Ctr Harmless Synergist Treatme, Qinhuangdao 066000, Peoples R China
基金
中国国家自然科学基金;
关键词
Geopolymer; Municipal solid waste incineration fly ash; Sulphuric acid resistance; Leaching concentration; Heavy metals; HEAVY-METALS; RED MUD; RESISTANCE; SULFATE; HYDRATION; CONCRETE; SOLIDIFICATION; DURABILITY; MORTAR; SLAG;
D O I
10.1016/j.conbuildmat.2023.131847
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This study assessed the durability of the geopolymer arranged from red mud-slag activated by carbide slagmunicipal solid waste incineration fly ash (CRMG) as heavy metal solidification and stabilization binder exposed to sulfuric acid solution. Ordinary Portland cement (OPC) as control group. CRMG and OPC samples were immersed in solutions at pH = 3 and pH = 7 for 112 days. The sulfuric acid resistance of the samples was evaluated through visual observation, weight changes, compressive strength, as well as XRD, SEM, DTG, and FTIR. The results showed that CRMG had a higher acid buffering capacity than OPC in terms of visual appearance and mass loss. The compressive strength of CRMG slightly increased during the initial stage of immersion due to the production of geopolymer gel and the filling effect of a small amount of ettringite and gypsum, but decreased after 7 days due to the formation of a large amount of ettringite and gypsum which induce serious expansion and server cracking. CRMG's compressive strength remained higher than OPC's after 112 days of exposure to the acid solution, with a 20% loss in compressive strength. The leaching concentration of CRMG was far lower than the national standard. The study's conclusions could help reduce the environmental risks associated with solid waste disposal and provide a theoretical framework for the use of MSWI fly ash based geopolymer.
引用
收藏
页数:12
相关论文
共 55 条
[1]   Synthesis, processing, characterization, and applications of red mud/carbon nanotube composites [J].
Abbasi, Saloumeh Mesgari ;
Rashidi, Alimorad ;
Ghorbani, Azam ;
Khalaj, Gholamreza .
CERAMICS INTERNATIONAL, 2016, 42 (15) :16738-16743
[2]   Metakaolin-red mud/carbon nanotubes geopolymer nanocomposite: mechanical properties and structural studies [J].
Ahmadi, Hamidreza ;
Khalaj, Gholamreza ;
Najafi, Abolhassan ;
Abbasi, Saloumeh Mesgari ;
Safari, Masumeh .
MATERIALS RESEARCH EXPRESS, 2022, 9 (02)
[3]   Effect of slag content and activator dosage on the resistance of fly ash geopolymer binders to sulfuric acid attack [J].
Aiken, Timothy A. ;
Kwasny, Jacek ;
Sha, Wei ;
Soutsos, Marios N. .
CEMENT AND CONCRETE RESEARCH, 2018, 111 :23-40
[4]   Environmental, physical and structural characterisation of geopolymer matrixes synthesised from coal (co-)combustion fly ashes [J].
Alvarez-Ayuso, E. ;
Querol, X. ;
Plana, F. ;
Alastuey, A. ;
Moreno, N. ;
Izquierdo, M. ;
Font, O. ;
Moreno, T. ;
Diez, S. ;
Vazquez, E. ;
Barra, M. .
JOURNAL OF HAZARDOUS MATERIALS, 2008, 154 (1-3) :175-183
[5]   Effects of adding sugarcane bagasse ash on the properties and durability of concrete [J].
Andrade Neto, Jose da Silva ;
Santos de Franca, Mavisson Julio ;
de Amorim Junior, Nilson Santana ;
Ribeiro, Daniel Veras .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 266
[6]   Sulfuric acid resistance of blended ash geopolymer concrete [J].
Ariffin, M. A. M. ;
Bhutta, M. A. R. ;
Hussin, M. W. ;
Tahir, M. Mohd ;
Aziah, Nor .
CONSTRUCTION AND BUILDING MATERIALS, 2013, 43 :80-86
[7]   Low carbon binder preparation from slag-red mud activated by MSWI fly ash-carbide slag: Hydration characteristics and heavy metals' solidification behavior [J].
Bai, Yanying ;
Guo, Weichao ;
Zhang, Yangyang ;
Xue, Caihong ;
Xu, Zehua ;
Gao, Qingyu ;
Xiao, Chang ;
Zhao, Qingxin .
JOURNAL OF CLEANER PRODUCTION, 2022, 374
[8]   Geopolymer bricks prepared by MSWI fly ash and other solid wastes: Moulding pressure and curing method optimisation [J].
Bai, Yanying ;
Guo, Weichao ;
Wang, Jianwei ;
Xu, Zehua ;
Wang, Shuai ;
Zhao, Qingxin ;
Zhou, Jinman .
CHEMOSPHERE, 2022, 307
[9]   Resistance of geopolymer materials to acid attack [J].
Bakharev, T .
CEMENT AND CONCRETE RESEARCH, 2005, 35 (04) :658-670
[10]   Influence of slag chemistry on the hydration of alkali-activated blast-furnace slag - Part II: Effect of Al2O3 [J].
Ben Haha, M. ;
Lothenbach, B. ;
Le Saout, G. ;
Winnefeld, F. .
CEMENT AND CONCRETE RESEARCH, 2012, 42 (01) :74-83