The mechanism for Li-addition induced homogeneous deformation in Mg-4.5wt.% Li alloy

被引:9
|
作者
Xu, Jing [1 ,2 ]
Guan, Bo [1 ,2 ]
Xin, Yunchang [1 ,3 ,4 ]
Li, Xiao [5 ]
Wu, Peidong [6 ]
Huang, Xiaoxu [4 ]
Liu, Qing [1 ]
机构
[1] Nanjing Tech Univ, Key Lab Light Weight Mat, Nanjing 210009, Peoples R China
[2] Jiangxi Acad Sci, Inst Appl Phys, Nanchang 330029, Peoples R China
[3] Suzhou Lab, Suzhou 215028, Peoples R China
[4] Chongqing Univ, Coll Mat Sci & Engn, Int Joint Lab Light Alloys, Chongqing 400030, Peoples R China
[5] Huzhou Univ, Sch Engn, Huzhou 313000, Peoples R China
[6] McMaster Univ, Dept Mech Engn, Hamilton, ON L8S 4L7, Canada
基金
中国国家自然科学基金;
关键词
Magnesium alloy; Plastic deformation; Slip; Twinning; Modeling; GREATER-THAN SLIP; X-RAY-DIFFRACTION; MAGNESIUM ALLOYS; RARE-EARTH; MG ALLOYS; CRYSTAL PLASTICITY; TEXTURE DEVELOPMENT; TENSILE PROPERTIES; GRAIN-GROWTH; LESS-THAN;
D O I
10.1016/j.ijplas.2023.103763
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The mechanism by which Li additions induce a more homogeneous deformation was systematically investigated in this study by comparing the deformation behavior of pure Mg and Mg-4.5 wt. % Li using experiments, crystal plasticity simulations, and theoretical calculations. The results of the digital image correlation measurements showed that under tension along the transverse direction (TD), strong localized deformation bands with an angle of approximately 20 degrees with respect to the TD were observed in pure Mg, but were absent in Mg-4.5 wt.% Li. Slip trace analyses indicated that basal slip was the predominant deformation mode for pure Mg, whereas that for Mg-4.5 wt.% Li was prismatic slip. A high relative activity of pyramidal (c+a) slip, approximately 17 %, was observed in Mg-4.5 wt.% Li at a high strain of 10 %. Contraction or double twins were hardly detected during the entire tension process. Crystal plasticity simulations revealed that the 4.5 wt.% Li addition dramatically reduced the critical resolved shear stress (CRSS) ratio of pyramidal (c+a) slip: prismatic slip: basal slip, which was 31.5:21:1 for pure Mg and 4.3:1.3:1 for Mg-4.5 wt.% Li. Theoretical calculations using the CRSS ratios determined by simulations revealed that easy and uniform deformation propagation induced by a dramatically reduced CRSS ratio of prismatic slip to basal slip played a more important role in improving the deformation homogeneity, in addition to the enhanced activity of pyramidal (c+a) slip. The mechanisms for how Li additions improve the ductility of Mg are also revisited in this paper.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] The Corrosion Behaviors of an As-Rolled Mg-8Li (in wt.%) Alloy in Two Differently Concentrated NaCl Solutions
    Wang, Baojie
    Hou, Jiyu
    Luan, Jiyu
    Xu, Daokui
    Sun, Haijing
    Sun, Jie
    COATINGS, 2022, 12 (03)
  • [42] Superplasticity of fine-grained Mg-10Li alloy prepared by severe plastic deformation and understanding its deformation mechanisms
    Jeong, H. T.
    Lee, S. W.
    Kim, W. J.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2024, 12 (01) : 316 - 331
  • [43] Characterization of Hot Deformation Behavior and Processing Maps of Mg-3Sn-2Al-1Zn-5Li Magnesium Alloy
    Guo, Yuhang
    Xuanyuan, Yaodong
    Lia, Chunnan
    Yang, Sen
    METALS, 2019, 9 (12)
  • [44] The influence of Zn addition on microstructure of an Al-1.7 Cu-4.0 Li-0.4 Mg alloy
    Liu, Dan-yang
    Ma, Yun-long
    Li, Jin-feng
    Huang, Cheng
    Wang, Yang
    Wang, Zhi-xiu
    Zhang, Rui-feng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (02): : 2423 - 2439
  • [45] Improved ductility of hot extruded Mg-0.5Zn-0.5Zr-1RE alloy by Li addition
    Maleki, Milad
    Rostami, Hamid
    Mirzadeh, Hamed
    Emamy, Massoud
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 30 : 5820 - 5825
  • [46] Effect of strain rate on deformation behaviour of a Mg-8.5Li-1Zn alloy sheet at room temperature
    Takada, H
    Kikuchi, S
    Tsukada, T
    Kubota, K
    Hatta, N
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 271 (1-2): : 251 - 256
  • [47] Influence of the Hot Deformation Conditions on the Texture Evolution in Mg-8Li-5Zn-2Re Alloy
    Gai Dengyu
    Liu Jie
    Li Qunxia
    Chen Zhaoyun
    Zhang Milin
    RARE METAL MATERIALS AND ENGINEERING, 2013, 42 (04) : 673 - 678
  • [48] Effect of strain rate on deformation behaviour of a Mg-9Li-2Zn alloy sheet at room temperature
    Li, H. B.
    Ji, H. B.
    Yao, G. C.
    Liu, Z. G.
    Liu, Y. H.
    Yu, H. J.
    MAGNESIUM TECHNOLOGY 2006, PROCEEDINGS, 2006, : 195 - 199
  • [49] Corrosion behavior of as-cast Mg-8Li-3Al+xCe alloy in 3.5wt% NaCl solution
    Manivannan, S.
    Dinesh, P.
    Mahemaa, R.
    MariyaPillai, Nandhakumaran
    Babu, S. P. Kumaresh
    Sundarrajan, Srinivasan
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2016, 23 (10) : 1196 - 1203
  • [50] Effect of Surfactants on the Corrosion Protectability of Calcium Phosphate Conversion Coatings on Duplex Structured Mg-8Li (in Wt.%) Alloy
    Hou, Jiyu
    Wang, Baojie
    Xu, Daokui
    Cui, Liji
    Sun, Jie
    COATINGS, 2022, 12 (08)