Current-induced solder evolution and mechanical property of Sn-3.0Ag-0.5Cu solder joints under thermal shock condition

被引:12
作者
Li, Shengli [1 ]
Hang, Chunjin [1 ,2 ]
Zhang, Wei [1 ]
Guan, Qilong [1 ]
Tang, Xiaojiu [1 ]
Yu, Dan [3 ]
Ding, Ying [3 ]
Wang, Xiuli [3 ]
机构
[1] Harbin Inst Technol, State Key Lab Adv Welding & Joining, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Zhengzhou Res Inst, Zhengzhou 450041, Peoples R China
[3] Beijing Inst Control Engn, Beijing 100094, Peoples R China
基金
中国国家自然科学基金;
关键词
SAC305; Twins; Electromigration; Cryogenic temperature; Shear strength; INTERMETALLIC COMPOUND FORMATION; MICROSTRUCTURAL EVOLUTION; CURRENT-DENSITY; BETA-SN; ELECTROMIGRATION; GROWTH; CU; DIFFUSION; INTERFACE; BEHAVIOR;
D O I
10.1016/j.jallcom.2023.172519
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Solder joint reliability suffers great challenges due to high current density and miniature solder bump diameter of electronic packages at cryogenic temperature. To tackle these issues, the solder microstructure evolution and the corresponding failure mechanism should be emphasized. In this study, the current-induced microstructure characteristics and mechanical behavior of Sn-3.0Ag-0.5Cu (SAC305) solder joints during thermal shock process was thoroughly addressed over cycles by combining diffusional, electrical, thermal and mechanical features. This result verified that the combining method of thermal shock and electromigration (EM) contributed to the atom diffusion and high thermal stress formation, further causing intermetallic compound (IMC) growth, the repaid dissolution of Cu pad and high thermal stress of the solder joints. High stress induced by either the thermal expansion mismatch of different component, large temperature change (Delta T =346 degrees C) and severe lattice distortion became the direct reason for twins and cracks formation of SAC305 solder joints. The combination of crack propagated along the interface and the quick dissolution of Cu substrate at the corner accelerated the eventually failure of the solder joints. Moreover, as the thermal chock cycles was extended, the initiation and propagation of cracks at the cathode side weaken the cathodic shear strength. High stress-induced twin formation at the interface effectively moderated the shear strength degradation due to anode IMC growth after 9 cycles. This study contributed to thoroughly grasp the failure mechanism of the solder joints and design the twinstrengthened Sn-based solder joints under the coupling effects of extreme temperature variation and current stressing.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Electromigration Behavior in Sn-37Pb and Sn-3.0Ag-0.5Cu Flip-Chip Solder Joints under High Current Density
    Sang-Su Ha
    Jong-Woong Kim
    Jeong-Won Yoon
    Sang-Ok Ha
    Seung-Boo Jung
    Journal of Electronic Materials, 2009, 38 : 70 - 77
  • [32] SN-3.0AG-0.5CU COMPOSITE SOLDER REINFORCED BY MULTILAYER GRAPHENE
    Huang, Yilong
    Xiu, Ziyang
    Tian, Yanhong
    2016 CHINA SEMICONDUCTOR TECHNOLOGY INTERNATIONAL CONFERENCE (CSTIC), 2016,
  • [33] Effects of Surface Finishes and Current Stressing on Interfacial Reaction Characteristics of Sn-3.0Ag-0.5Cu Solder Bumps
    Kim, Jae-Myeong
    Jeong, Myeong-Hyeok
    Yoo, Sehoon
    Park, Young-Bae
    JOURNAL OF ELECTRONIC MATERIALS, 2012, 41 (04) : 791 - 799
  • [34] Solder Volume Effects on the Microstructure Evolution and Shear Fracture Behavior of Ball Grid Array Structure Sn-3.0Ag-0.5Cu Solder Interconnects
    Li, X. P.
    Xia, J. M.
    Zhou, M. B.
    Ma, X.
    Zhang, X. P.
    JOURNAL OF ELECTRONIC MATERIALS, 2011, 40 (12) : 2425 - 2435
  • [35] Effects of Mixed Percentage on the Microstructure and Mechanical Properties of Sn-52In/Sn-3.0Ag-0.5Cu Hybrid Solder Joints
    Zhao, W. T.
    Ren, J.
    Huang, M. L.
    JOURNAL OF ELECTRONIC MATERIALS, 2024, : 6463 - 6470
  • [36] Study of microstructure, growth orientations and shear performance of Cu/Sn-3.0Ag-0.5Cu/Cu solder joints by using thermal gradient bonding
    Zhang, Zezong
    Hu, Xiaowu
    Chen, Wenjing
    Tan, Sifan
    Chen, Bin
    Wang, Jue
    Jiang, Lan
    Huang, Yifan
    Zhu, Guangyu
    He, Yinshui
    Jiang, Xiongxin
    Li, Qinglin
    MATERIALS CHARACTERIZATION, 2023, 203
  • [37] Fracture behavior and constitutive relations of Sn-3.0Ag-0.5Cu solder alloy at cryogenic temperature
    Li, Shengli
    Hang, Chunjin
    Zhang, Wei
    Tian, Yanhong
    Yu, Dan
    Ding, Ying
    Wang, Xiuli
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 896
  • [38] Effect of temperature on shear properties of Sn-3.0Ag-0.5Cu and Sn-58Bi solder joints
    Jeong, Min-Seong
    Lee, Dong-Hwan
    Yoon, Jeong-Won
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 903
  • [39] Cross-solder interaction on interfacial reactions in Ni/Sn-3.0Ag-0.5Cu/Cu solder interconnects
    Fan, M.
    Huang, M. L.
    Zhao, N.
    2016 17TH INTERNATIONAL CONFERENCE ON ELECTRONIC PACKAGING TECHNOLOGY (ICEPT), 2016, : 542 - 545
  • [40] The Evolution of IMCs in Single Crystal Sn3.0Ag0.5Cu and Sn3.0Ag3.0Bi3.0In BGA Solder Joints with Au/Ni/Cu Pads Under Current Stressing
    Yu Tian
    Yishu Wang
    Fu Guo
    Limin Ma
    Jing Han
    Journal of Electronic Materials, 2019, 48 : 2770 - 2779