Effect of cryogenic treatment on wear behavior of Sleipner cold work tool steel

被引:52
作者
Kara, Fuat [1 ]
Kucuk, Yilmaz [2 ]
Ozbek, Onur [3 ]
Ozbek, Nursel Altan [4 ]
Gok, Mustafa Sabri [2 ]
Altas, Emre [2 ]
Uygur, Ilyas [1 ]
机构
[1] Duzce Univ, Dept Mech Engn, TR-81620 Duzce, Turkiye
[2] Bartin Univ, Dept Mech Engn, TR-74100 Bartin, Turkiye
[3] Duzce Univ, Gumusova Vocat Sch Higher Educ, TR-81850 Duzce, Turkiye
[4] Duzce Univ, Dr Engin PAK Cumayeri Vocat Sch Higher Educ, TR-81700 Duzce, Turkiye
关键词
Sleipner steel; Cryogenic treatment; Wear rate; Tribology; CARBIDE PRECIPITATION; MECHANICAL-PROPERTIES; MICROSTRUCTURE;
D O I
10.1016/j.triboint.2023.108301
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Cryogenic treatment, also known as subzero heat treatment, is a cooling process that complements conventional heat treatment to improve the properties of metals. Unlike coatings, it is a one-time, inexpensive, permanent operation that affects the entire part. This method is mainly applied to tool steels used in mold making. In this study, the changes caused by the effects of shallow and deep cryogenic treatment on Sleipner cold work tool steel were investigated in terms of microhardness, microstructure, coefficient of friction (COF), and wear rate (WR). For this purpose, the test specimens were subjected to the cryogenic treatments performed at two different temperatures (80 degrees C for the shallow cryogenic treatment (SCT) and 180 degrees C for the deep cryogenic treatment (DCT)) and various retention times (12 h, 24 h for SCT and 12 h, 24 h, 36 h for DCT). Dry sliding wear tests were carried out under different loads (10 N and 20 N) and varying test durations (60, 120, and 240 min) at a constant sliding speed of 0.075 m/s. According to the microhardness results, it was determined that the cryogenic treatment increased the hardness by 6.53 %. According to the microstructure investigations, a more homogeneous structure was observed with the cryogenic treatment, and secondary carbide precipitations were detected. It was observed that the conventional heat-treated (CHT) sample gave the highest COF value with an average coefficient of friction of 0.63. The lowest COF value of 0.58 was observed in the DCT-12 sample. After the wear tests, the lowest wear rate value for both load values was obtained from the DCT-36 specimen.
引用
收藏
页数:11
相关论文
共 28 条
[1]   Surface Integrity of NiTi Shape Memory Alloy in Milling with Cryogenic Heat Treated Cutting Tools under Different Cutting Conditions [J].
Altas, Emre ;
Altin Karatas, Meltem ;
Gokkaya, Hasan ;
Akinay, Yuksel .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2021, 30 (12) :9426-9439
[2]   Effect of deep cryogenic treatment on the formation of nano-sized carbides and the wear behavior of D2 tool steel [J].
Amini, Kamran ;
Akhbarizadeh, Amin ;
Javadpour, Sirus .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2012, 19 (09) :795-799
[3]  
Arslan KF, 2010, THESIS SAKARYA U
[4]   Analyzing the influence of a deep cryogenic treatment on the mechanical properties of blanking tools by using the short-time method PhyBaLCHT [J].
Blinn, B. ;
Winter, S. ;
Weber, M. ;
Demmler, M. ;
Krausel, V. ;
Beck, T. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 824
[5]   Effects of deep cryogenic treatment on microstructure, impact toughness and wear resistance of an AISI D6 tool steel [J].
Cardoso, P. H. S. ;
Israel, C. L. ;
da Silva, M. B. ;
Klein, G. A. ;
Soccol, L. .
WEAR, 2020, 456
[6]   Effect of deep cryogenic treatment on the carbide precipitation and tribological behavior of D2 steel [J].
Das, D. ;
Dutta, A. K. ;
Toppo, V. ;
Ray, K. K. .
MATERIALS AND MANUFACTURING PROCESSES, 2007, 22 (04) :474-480
[7]  
Dhokey N. B., 2021, Materials Today: Proceedings, V43, P3006, DOI 10.1016/j.matpr.2021.01.361
[8]  
Dixit S. S., 2013, INT J ENG SCI, V2, P16
[9]   Microstructure and Hardness of Cold Work Vanadis 6 Steel after Subzero Treatment at-140°C [J].
Durica, Juraj ;
Ptacinova, Jana ;
Hudakova, Maria ;
Kusy, Martin ;
Jurci, Peter .
ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2018, 2018
[10]   Life time improvement of D7 tool steel by cryogenic treatment [J].
Hariharan, K. B. ;
Saravanan, S. ;
Parkunam, N. .
MATERIALS TODAY-PROCEEDINGS, 2020, 21 :619-621