Effects of preheating on laser beam-welded NSSC 2120 lean duplex steel

被引:2
作者
Landowski, Michal [1 ]
Simon, Soma Csaba [2 ]
Breznay, Csaba [2 ]
Fydrych, Dariusz [1 ]
Varbai, Balazs [2 ]
机构
[1] Gdansk Univ Technol, Inst Mfg & Mat Technol, Fac Mech Engn & Ship Technol, Gabriela Narutowicza St 11-12, PL-80233 Gdansk, Poland
[2] Budapest Univ Technol & Econ, Muegyetem Rkp 3, H-1111 Budapest, Hungary
关键词
Lean duplex steel; Laser beam welding; Preheating; Weld geometry; Pitting corrosion resistance; STAINLESS-STEEL; CORROSION-RESISTANCE; PHASE-TRANSFORMATIONS; HEAT-TREATMENT; NITROGEN; WELDABILITY; BEHAVIOR;
D O I
10.1007/s00170-023-12840-w
中图分类号
TP [自动化技术、计算机技术];
学科分类号
0812 ;
摘要
Duplex stainless steels show sustainable alternative for the conventional austenitic grades, with higher strength, higher resistance against stress corrosion cracking, and lower purchase cost. Thus, duplex stainless steel gains more attention in construction, oil and gas, and chemical industries. Among duplex stainless steels, low nickel and low molybdenum alloyed lean duplex stainless steel are a cost-effective substitution of austenitic grades. However, keeping the balanced ferrite/austenite phase ratio in the weld metal can be challenging, mostly for autogenous and low heat input welding processes. In our research, a newly developed NSSC 2120 lean duplex stainless steel grade was welded autogenously by fiber laser welding process. Different welding parameters and preheating temperatures were used during the experiments. The welds were evaluated by microscopic and metallographic techniques, and also by electrochemical corrosion measurements. The welding parameters and the preheating temperature greatly influenced the weld shape and the austenite content in the weld metal. It was found that the focus point distance from the sheet surface had significant effect on the weld geometry. Changing the focus point distance to + 2 mm, the penetration depth increased from 4.96 to 5.53 mm, and increased the austenite content by 2.6%. Due to the preheating the welds became wider and shallower, e.g., from 4.96 to 4.08 mm penetration depth, while the cross-section are increased from 5.10 to 6.12 mm2 at the same sample. The preheating resulted in more intergranular austenite formation, which meant maximum 4% increase in the weld metal. The increasing austenite content resulted in increasing pitting corrosion resistance in 3.5% NaCl electrolyte, the highest increase was 90 mV.
引用
收藏
页码:1039 / 1074
页数:36
相关论文
共 50 条
  • [31] Fatigue and Fatigue Crack Propagation of Laser Beam-Welded AA2198 Joints and Integral Structures
    Kashaev, Nikolai
    Chupakhin, Sergey
    Enz, Josephin
    Ventzke, Volker
    Groth, Anne
    Horstmann, Manfred
    Riekehr, Stefan
    11TH INTERNATIONAL FATIGUE CONGRESS, PTS 1 AND 2, 2014, 891-892 : 1457 - 1462
  • [32] Investigation of welding parameters on microstructure and mechanical properties of laser beam-welded joint of 2060 Al-Cu-Li alloy
    Gu, Cheng
    Wei, Yanhong
    Zhan, Xiaohong
    Zhang, Dan
    Ren, Shuai
    Liu, Hongbing
    Li, Hao
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2017, 91 (1-4) : 771 - 780
  • [33] Microstructure and mechanical properties of electron beam-welded AISI 409M-grade ferritic stainless steel
    Lakshminarayanan, A. K.
    Balasubramanian, V.
    Reddy, G. Madhusudhan
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2011, 55 (1-4) : 153 - 162
  • [34] INFLUENCE OF PARAMETERS OF LASER BEAM WELDING ON STRUCTURE OF 2205 DUPLEX STAINLESS STEEL
    Landowski, M.
    ADVANCES IN MATERIALS SCIENCE, 2019, 19 (01): : 21 - 31
  • [35] Effect of Nitrogen on Weldability and the Microstructure in Laser Beam Welding of Duplex Stainless Steel
    Xia, Yunxing
    Amatsu, Kenshiro
    Miyasaka, Fumikazu
    Mori, Hiroaki
    MATERIALS PROCESSING FUNDAMENTALS 2021, 2021, : 201 - 209
  • [36] Effect of heat input on the corrosion resistance of the cold worked 2304 lean duplex stainless steel GMAW welded joint
    Souza, Carla S.
    Soares, Renata B.
    de Faria, Ricardo A. D.
    Bracarense, Alexandre Q.
    Castro, Maria das M. R.
    Lins, Vanessa de F. C.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (03): : 409 - 418
  • [37] Effect of heat treatment on structure and properties of GTAW and laser beam welded super-duplex stainless steel joints
    Qi, Kai
    Wang, Guangjin
    Jin, Yunxue
    Gu, Jiayang
    Zhang, Zhongyu
    Tao, Yanwu
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2020, 34 (1-3):
  • [38] Microstructure, mechanical, and corrosion properties of electron beam-welded commercially pure titanium after laser shock peening
    Chattopadhyay, Angshuman
    Muvvala, Gopinath
    Sarkar, Sagar
    Racherla, Vikranth
    Nath, Ashish Kumar
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 118 (1-2) : 343 - 364
  • [39] Numerical investigation of laser beam-welded AA2198 joints under different artificial ageing conditions
    Examilioti, T. N.
    Germanou, A.
    Papanikos, P.
    Kashaev, N.
    Klusemann, B.
    Alexopoulos, N. D.
    23 EUROPEAN CONFERENCE ON FRACTURE, ECF23, 2022, 42 : 244 - 250
  • [40] Influence of cobalt addition in the fusion zone of duplex stainless steel welded with pulsed Nd:YAG laser
    da Cruz Junior, Eli Jorge
    Varasquim, Francisco Mateus Faria de Almeida
    Ventrella, Vicente Afonso
    Calliari, Irene
    Gennari, Claudio
    Seloto, Bruna Berbel
    Zambon, Andrea
    Settimi, Alessio Giorgio
    WELDING IN THE WORLD, 2025,