Investigation of the temperature and DOD effect on the performance-degradation behavior of lithium-sulfur pouch cells during calendar aging

被引:20
作者
Capkova, Dominika [1 ]
Knap, Vaclav [2 ]
Fedorkova, Andrea Strakova [1 ]
Stroe, Daniel-Ioan [3 ]
机构
[1] Pavol Jozef Safarik Univ Kosice, Dept Phys Chem, Kosice 04154, Slovakia
[2] Czech Tech Univ, Fac Elect Engn, Prague 16627, Czech Republic
[3] Aalborg Univ, Dept Energy, DK-9220 Aalborg, Denmark
关键词
Li-S pouch cell; Battery degradation; Calendar aging; Differential voltage analysis; Self; -discharge; INCREMENTAL CAPACITY ANALYSIS; SELF-DISCHARGE BEHAVIOR; POLYSULFIDE SHUTTLE; CYCLE LIFE; IN-SITU; X-RAY; BATTERIES; CATHODE; INSIGHT; ANODE;
D O I
10.1016/j.apenergy.2022.120543
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
High-energy density sulfur cathodes are one of the most promising possibilities to replace currently used intercalation cathodes in lithium-ion batteries in future applications. However, lithium-sulfur batteries are still the subject of research due to unsatisfactory capacity retention and cycle performance. The cause of insufficient properties is the shuttle effect of higher polysulfides which are formed in a high voltage plateau. In an effort to optimize storage conditions of lithium-sulfur (Li-S) batteries, long-term calendar aging tests at various temperatures and depth-of-discharge were performed on pre-commercial 3.4 Ah Li-S pouch cells. The decrease in performance over two years of calendar aging in five stationary conditions was analyzed using non-destructive electrochemical tests. The negative effect on Li-S cell performance was more pronounced for temperature than for depth-of-discharge. The analyses of self-discharge and shuttle current were performed and as expected, the highest values were measured in a fully charged state where higher polysulfides are present. Furthermore, internal resistance was analyzed where an increase of resistance was observed for a discharged state due to the formation of a passivation layer from discharge products (Li2S2, Li2S). To maximize the life of the Li-S battery, storage at high temperatures and in a fully charged state should be avoided.
引用
收藏
页数:11
相关论文
共 96 条
[1]   A gelatin-based artificial SEI for lithium deposition regulation and polysulfide shuttle suppression in lithium-sulfur batteries [J].
Akhtar, Naseem ;
Sun, Xiaogang ;
Akram, Muhammad Yasir ;
Zaman, Fakhar ;
Wang, Weikun ;
Wang, Anbang ;
Chen, Long ;
Zhang, Hao ;
Guan, Yuepeng ;
Huang, Yaqin .
JOURNAL OF ENERGY CHEMISTRY, 2021, 52 (52) :310-317
[2]   Characterization of high-power lithium-ion batteries by electrochemical impedance spectroscopy. II: Modelling [J].
Andre, D. ;
Meiler, M. ;
Steiner, K. ;
Walz, H. ;
Soczka-Guth, T. ;
Sauer, D. U. .
JOURNAL OF POWER SOURCES, 2011, 196 (12) :5349-5356
[3]   Lithium-Ion Battery Degradation Indicators Via Incremental Capacity Analysis [J].
Ansean, David ;
Manuel Garcia, Victor ;
Gonzalez, Manuela ;
Blanco-Viejo, Cecilio ;
Carlos Viera, Juan ;
Fernandez Pulido, Yoana ;
Sanchez, Luciano .
IEEE TRANSACTIONS ON INDUSTRY APPLICATIONS, 2019, 55 (03) :2992-3002
[4]  
Balagopal B, 2018, 2018 IEEE INT C IND, DOI [10.1109/ieses.2018.8349846, DOI 10.1109/IESES.2018.8349846]
[5]   Extensive aging analysis of high-power lithium titanate oxide batteries: Impact of the passive electrode effect [J].
Bank, Thomas ;
Feldmann, Jan ;
Klamor, Sebastian ;
Bihn, Stephan ;
Sauer, Dirk Uwe .
JOURNAL OF POWER SOURCES, 2020, 473
[6]   New insights into the limiting parameters of the Li/S rechargeable cell [J].
Barchasz, Celine ;
Lepretre, Jean-Claude ;
Alloin, Fannie ;
Patoux, Sebastien .
JOURNAL OF POWER SOURCES, 2012, 199 :322-330
[7]   An accelerated calendar and cycle life study of Li-ion cells [J].
Bloom, I ;
Cole, BW ;
Sohn, JJ ;
Jones, SA ;
Polzin, EG ;
Battaglia, VS ;
Henriksen, GL ;
Motloch, C ;
Richardson, R ;
Unkelhaeuser, T ;
Ingersoll, D ;
Case, HL .
JOURNAL OF POWER SOURCES, 2001, 101 (02) :238-247
[8]   Corrosion of lithium metal anodes during calendar ageing and its microscopic origins [J].
Boyle, David T. ;
Huang, William ;
Wang, Hansen ;
Li, Yuzhang ;
Chen, Hao ;
Yu, Zhiao ;
Zhang, Wenbo ;
Bao, Zhenan ;
Cui, Yi .
NATURE ENERGY, 2021, 6 (05) :487-494
[9]   Main aging mechanisms in Li ion batteries [J].
Broussely, M ;
Biensan, P ;
Bonhomme, F ;
Blanchard, P ;
Herreyre, S ;
Nechev, K ;
Staniewicz, RJ .
JOURNAL OF POWER SOURCES, 2005, 146 (1-2) :90-96
[10]   Investigations of lithium-sulfur batteries using electrochemical impedance spectroscopy [J].
Canas, Natalia A. ;
Hirose, Kei ;
Pascucci, Brigitta ;
Wagner, Norbert ;
Friedrich, K. Andreas ;
Hiesgen, Renate .
ELECTROCHIMICA ACTA, 2013, 97 :42-51