Investigation of Microstructure, Mechanics, and Corrosion Properties of Ti6Al4V Alloy in Different Solutions

被引:7
作者
Ghisheer, Mohammed M. M. [1 ]
Esen, Ismail [1 ]
Ahlatci, Hayrettin [2 ]
Akin, Bengue [2 ]
机构
[1] Karabuk Univ, Mech Engn Dept, TR-78050 Karabuk, Turkiye
[2] Karabuk Univ, Met & Mat Engn Dept, TR-78050 Karabuk, Turkiye
关键词
Ti6Al4V; mechanical; NaCl; HCl; TITANIUM-ALLOYS; WEAR BEHAVIOR; RESISTANCE; INTEGRITY;
D O I
10.3390/coatings14030277
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
There is a scarcity of research on the characterization of the behaviour of titanium and its alloys in highly corrosive environments. These materials are highly recommended for use in various industries such as aviation, maritime, medical, and chemical, due to their perceived superior corrosion resistance. This research examines the mechanical and corrosion characteristics of Ti6Al4V material when exposed to solutions containing 9% NaCl, 25% HCl, and a mixture of 9% NaCl and 25% HCl. Prior to the corrosion process, the prefabricated Ti6Al4V samples underwent microstructure analysis, hardness assessment, and wear evaluation. The microstructure characterization revealed that the microstructure of the Ti6Al4V alloy is composed of alpha and modified beta phases. The Ti6Al4V sample's hardness value was determined to be 334.23 HB. The Ti6Al4V sample's wear rate was determined to be 0.0033 g/Nm, while the friction coefficient was determined to be 0.0326. Corrosion testing was conducted at intervals of 24, 48, 72, 168, and 336 h. Based on the corrosion rate measurements, the sample exhibited the minimum corrosion rate of 1.928519 mg/(dm2 center dot day) in a 9% NaCl environment. The sample with a combination of 9% NaCl and 25% HCl had the maximum corrosion rate, measured at 6.493048 mg per square decimetre per day. The formation of a larger oxide layer in the Ti6Al4V corrosion sample immersed in a 9% NaCl solution serves as a protective barrier on the surface and enhances its resistance to corrosion.
引用
收藏
页数:17
相关论文
共 50 条
[21]   Microstructure and tribological properties of cold sprayed WCp/Ti composite coatings on Ti6Al4V titanium alloy [J].
Xu, Yaxin ;
Ge, Jiejie ;
Li, Wenya .
TRIBOLOGY INTERNATIONAL, 2024, 192
[22]   Cryogenic turning of Ti6Al4V alloy [J].
Sola, R. ;
Veronesi, P. .
METALLURGIA ITALIANA, 2020, 112 (7-8) :28-36
[23]   Wear Property of Ti6Al4V Alloy with Different Hydrogen Contents [J].
Yuan Baoguo ;
Wang Chengguo ;
Wei Shengquan ;
Chen Fucai ;
Xue Kemin .
RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (02) :399-402
[24]   Corrosion study of laser cladded Ti-6Al-4V alloy in different corrosive environments [J].
Nabhani, Mohammad ;
Razavi, Reza Shoja ;
Barekat, Masoud .
ENGINEERING FAILURE ANALYSIS, 2019, 97 :234-241
[25]   The effect of anodizing conditions on the corrosion resistance of Ti6Al4V titanium alloy [J].
Lepicka, Magdalena ;
Gradzka-Dahlke, Malgorzata ;
Sobolewski, Andrzej .
MATERIALS TESTING, 2015, 57 (05) :393-397
[26]   Pitting corrosion studies on Ti6Al4V alloy weldments in marine environment [J].
Raja, V. K. Bupesh ;
Palanikumar, K. ;
Sai, Arja Sri ;
Goud, Bandi Vedaraj .
INDIAN JOURNAL OF GEO-MARINE SCIENCES, 2019, 48 (08) :1179-1182
[27]   Corrosion of an Additively Manufactured Ti6Al4V Alloy in Saline and Acidic Media [J].
Mora-Sanchez, Hugo ;
Collado-Vian, Miguel ;
Mohedano, Marta ;
Arrabal, Raul ;
Matykina, Endzhe .
MATERIALS, 2024, 17 (03)
[28]   Effect of microstructure and cutting speed on machining behavior of Ti6Al4V alloy [J].
Telrandhe, Sagar V. ;
Saxena, Ashish K. ;
Mishra, Sushil .
JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2017, 31 (05) :2177-2184
[29]   Spark plasma sintering of Ti6Al4V metal matrix composites: Microstructure, mechanical and corrosion properties [J].
Singh, Neera ;
Ummethala, Raghunandan ;
Karamched, Phani Shashanka ;
Sokkalingam, Rathinavelu ;
Gopal, Vasanth ;
Manivasagam, G. ;
Prashanth, Konda Gokuldoss .
JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 865
[30]   Effects of Y addition on microstructure and mechanical properties of TiC/Ti6Al4V composites [J].
Wang, Xiang ;
Ma, Xuliang ;
Nie, Qidong ;
Wang, Mingjia .
INTERMETALLICS, 2012, 31 :242-248