The Study on Corrosion Resistance of Ti-6Al-4V ELI Alloy with Varying Surface Roughness in Hydrofluoric Acid Solution

被引:1
|
作者
Wang, Han [1 ]
Cheng, Quanshi [2 ]
Chang, Zhuo [3 ]
Wang, Kedi [1 ]
Gao, Xuemin [2 ]
Fan, Xueling [1 ]
机构
[1] Xi An Jiao Tong Univ, Sch Aerosp Engn, Xian Key Lab Extreme Environm & Protect Technol, Xian 710049, Peoples R China
[2] Henan Aerosp Precis Machining Co Ltd, Henan Key Lab Fastening Connect Technol, Xinyang 464000, Peoples R China
[3] Xi An Jiao Tong Univ, Sch Aerosp Engn, Lab Multiscale Mech & Med Sci, State Key Lab Strength & Vibrat Mech Struct, Xian 710049, Peoples R China
关键词
Ti-6Al-4V ELI; corrosion resistance; surface morphology; surface roughness; mechanical property recession; TITANIUM; BEHAVIOR;
D O I
10.3390/met14030364
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion resistance of titanium alloy poses a crucial challenge, significantly affecting its prospect for service and application. The present study aimed to investigate the corrosion resistance of Ti-6Al-4V ELI alloys with varying surface roughness in hydrofluoric acid solution, in order to assess the influence of roughness on their corrosion resistance performance. The weight loss percentage, surface morphology evolution, and roughness variation of Ti-6Al-4V ELI alloys before and after exposure to hydrofluoric acid corrosion were characterized. While the weight loss and weight loss percentage of the Ti-6Al-4V ELI alloy increased with prolonged corrosion, the overall weight loss rate decreased. The accumulation of TiF3 phases and depletion of the Ti-6Al-4V ELI matrix mutually led to the alterations of the surface roughness. Due to the inability to prevent fluoride ions from contacting with the Ti-6Al-4V ELI alloy, continuous corrosion occurred in hydrofluoric acid. Based on these experimental results and analysis, the corrosion mechanism of the Ti-6Al-4V ELI alloy corroded by hydrofluoric acid solution was elucidated. Furthermore, an analysis was conducted to explore the influence of corrosion time on mechanical properties by analyzing the decay in compressive properties of the Ti-6Al-4V ELI titanium alloy after hydrofluoric acid corrosion treatment. The bearing capacity of the Ti-6Al-4V ELI alloy deteriorated over the corrosion time.
引用
收藏
页数:13
相关论文
共 50 条
  • [11] Corrosion resistance of Ti-6Al-4V alloy with nitride coatings in Ringer's solution
    Pohrelyuk, I. M.
    Fedirko, V. M.
    Tkachuk, O. V.
    Proskurnyak, R. V.
    CORROSION SCIENCE, 2013, 66 : 392 - 398
  • [12] CORROSION BEHAVIOUR OF TITANIUM ALLOY Ti-6Al-4V ELI IN HANK'S SOLUTION WITH THE IMMERSION TEST METHOD
    Anderson, Sir
    Adriansyah
    Ramadino, Muhammad Rifo
    Nuswantoro, Nuzul Ficky
    Indra, Ade
    CERAMICS-SILIKATY, 2024, 68 (04) : 550 - 555
  • [13] STRUCTURE AND PITTING CORROSION OF Ti-6Al-4V ALLOY AND Ti-6Al-4V WELDS
    Ferdinandov, Nikolay Vasilev
    Gospodinov, Danail Dimitrov
    Ilieva, Mariana Dimitrova
    Radev, Rossen Hristov
    PROCEEDINGS OF THE 7TH INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND SYSTEMS, 2018, : 325 - 330
  • [14] Enhancing Biocompatibility and Corrosion Resistance of Ti-6Al-4V Alloy by Surface Modification Route
    Sarao, Tejinder Pal Singh
    Singh, Harpreet
    Singh, Hazoor
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2018, 27 (08) : 1388 - 1400
  • [15] Excimer laser surface treatment of Ti-6Al-4V alloy for corrosion resistance enhancement
    Yue, TM
    Yu, JK
    Mei, Z
    Man, HC
    MATERIALS LETTERS, 2002, 52 (03) : 206 - 212
  • [16] Enhancing Biocompatibility and Corrosion Resistance of Ti-6Al-4V Alloy by Surface Modification Route
    Tejinder Pal Singh Sarao
    Harpreet Singh
    Hazoor Singh
    Journal of Thermal Spray Technology, 2018, 27 : 1388 - 1400
  • [17] Machining of Ti-6Al-4V ELI Alloy: A brief review
    Anurag, R. Kumar
    Roy, S.
    Joshi, K. K.
    Sahoo, A. K.
    Das, R. K.
    3RD INTERNATIONAL CONFERENCE ON MATERIALS AND MANUFACTURING ENGINEERING 2018, 2018, 390
  • [18] Initial Cavitation Corrosion of Ti-6Al-4V Alloy in LiBr Solution
    Zhao Xiaobin
    Lin Cui
    Yang Ying
    Zhang Yifei
    RARE METAL MATERIALS AND ENGINEERING, 2017, 46 (12) : 3935 - 3940
  • [19] Initial Cavitation Corrosion of Ti-6Al-4V Alloy in LiBr Solution
    Zhao, Xiaobin
    Lin, Cui
    Yang, Ying
    Zhang, Yifei
    Xiyou Jinshu Cailiao Yu Gongcheng/Rare Metal Materials and Engineering, 2017, 46 (12): : 3935 - 3940
  • [20] INVESTIGATION OF CORROSION PROCESSING FOR Ti-6AL-4V IN HYDROFLUORIC-NITRIC ACID SYSTEM
    Lin, C.
    Hong, X. P.
    PROCEEDINGS OF THE ASME INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE 2011, VOL 1, 2011, : 349 - 355