Investigation on the hot crack sensitivity of a nickel-based single crystal superalloy fabricated by epitaxial laser metal forming

被引:15
作者
Chen, Zhiguo [1 ,2 ]
Li, Wenjie [1 ]
Wang, Li [2 ]
Wei, Xiang [2 ]
Liu, Zhiwei [1 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[2] Hunan Univ Humanities, Dept Mat Engn, Sci & Technol, Loudi 417000, Peoples R China
关键词
Epitaxial laser metal forming(E-LMF); Nickel -based single crystal superalloy; Cooling conditions; Crack mechanism; Deposition strategy; STRAY-GRAIN FORMATION; POWDER DEPOSITION; MICROSTRUCTURE FORMATION; GROWTH; MECHANISM; SUBSTRATE; LIQUATION; ZONE; ORIENTATION; INCONEL-738;
D O I
10.1016/j.jallcom.2022.167436
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, the epitaxial laser metal forming(E-LMF) process was used to deposit a nickel-based single crystal superalloy under different cooling conditions, and its microstructure and formation mechanism were investigated. The results reveal that an epitaxial microstructure with an almost crack-free is formed under air-cooling, while water-cooling increases the hot crack sensitivity of the deposited due to the thermal stress accumulation. In the case of water-cooling, almost all cracks arise in the overlap zone, with a few cracks appearing in other regions. The element distribution analysis and grain boundary angle analysis show that micro-segregation, as well as high angle grain boundaries, result in typical solidification cracks. In the case of air-cooling, the crystal orientation of the deposited zone is consistent with that of the substrate, although there are some stray grains in the top zone. As the bottom layers are annealed for a longer time than the upper layers, the gamma' phase is precipitated more at the bottom than at the top. (c) 2022 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 45 条
  • [41] Phase field modeling of solidification microstructure evolution during welding
    Yu, Fengyi
    Wei, Yanhong
    Ji, Yanzhou
    Chen, Long-Qing
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2018, 255 : 285 - 293
  • [42] A novel method to prevent cracking in directed energy deposition of Inconel 738 by in-situ doping Inconel 718
    Zhang, Xiaoqiang
    Chai, Ze
    Chen, Huabin
    Xu, Jijin
    Xu, Luming
    Lu, Hao
    Chen, Xiaoqi
    [J]. MATERIALS & DESIGN, 2021, 197 (197)
  • [43] Boundary liquation and interface cracking characterization in laser deposition of Inconel 738 on directionally solidified Ni-based superalloy
    Zhong, ML
    Sun, HQ
    Liu, WJ
    Zhu, XF
    He, JJ
    [J]. SCRIPTA MATERIALIA, 2005, 53 (02) : 159 - 164
  • [44] Effects of process parameters on microstructure and cracking susceptibility of a single crystal superalloy fabricated by directed energy deposition
    Zhou, Zhipeng
    Lei, Qian
    Yan, Zhou
    Wang, Zi
    Shang, Yijing
    Li, Yunping
    Qi, Huan
    Jiang, Liang
    Liu, Yong
    Huang, Lan
    [J]. MATERIALS & DESIGN, 2021, 198
  • [45] Causes analysis on cracks in nickel-based single crystal superalloy fabricated by laser powder deposition additive manufacturing
    Zhou, Zhipeng
    Huang, Lan
    Shang, Yijing
    Li, Yunping
    Jiang, Liang
    Lei, Qian
    [J]. MATERIALS & DESIGN, 2018, 160 : 1238 - 1249