Effect of High-Sintering-Temperature Reduction Behavior on Coke Solution Loss Reaction with Different Thermal Properties

被引:0
|
作者
Jin, Jin [1 ]
Wang, Qi [1 ,2 ]
Zhang, Song [2 ]
机构
[1] Univ Sci & Technol Liaoning, Sch Mat & Met, Anshan 114051, Peoples R China
[2] Key Lab Chem Met Engn Liaoning Prov, Anshan 114051, Peoples R China
基金
中国国家自然科学基金;
关键词
coke; sinter; thermal properties; coupling reactions; blast furnace; GAS-SOLID REACTIONS; BLAST-FURNACE; IRON-OXIDES; PART II; KINETICS; MODEL; MECHANISMS; EVOLUTION;
D O I
10.3390/met13010117
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
With the shortage of high-quality coking coal resources and the pursuit of low-cost smelting, the types and sources of coal have changed. Therefore, it is difficult to establish an effective correlation between the existing evaluation indexes of coke thermal performance and the production indexes of the blast furnace. The dissolution deterioration of coke directly affects the production benefits of the blast furnace, and the dissolution deterioration of blast furnace coke is the result of ore-coke coupling. To better understand the mechanism of the coupling reaction relative to the thermal properties of coke, this paper experimentally studies ore-coke coupling between two kinds of coke and one kind of blast furnace standing sinter which have different reactivities but are used in practical applications. This method adopts a matched thermogravimetric device. By analyzing and calculating the high-temperature reduction behavior and characteristics of the sinter and the dissolution loss behavior and characteristics of coke in the gas-solid coupling reaction test of coke and sinter, and comparing and fitting the coupling reaction factors of the coupling reaction and the thermal properties of coke, it was revealed that the real degradation behavior of coke was affected by the reduction reaction of the sinter. The results show that the temperature range with the best matching degree between the reduction reaction of oxygen supply from sinter and the gasification reaction of oxygen consumption from coke is at a position where the coupling factor is closest to 1. In the gas-solid coupling reaction between low-reactivity coke and sinter, the strongest dissolution rate, R-CSL, is approximately 1200 degrees C, while in the gas-solid coupling reaction between high-reactivity coke and sinter, the R-CSL is approximately 1100 degrees C. The minimum strength, CSCSL, of high-active coke and sinter after dissolution is approximately 1100 degrees C, while that of low-active coke and sinter after dissolution is approximately 1200 degrees C. It is shown that there is a good linear relationship between the R-CSL of high- and low-reactive coke and strength after dissolution loss CSCSL.
引用
收藏
页数:14
相关论文
共 50 条
  • [21] Experimental and numerical study on degradation behavior of coke with CO2 or H2O gasification reaction at high temperature
    Ono, Yuya
    Fukuda, Yuka
    Sumitani, Yuya
    Matsukawa, Yoshiya
    Saito, Yasuhiro
    Matsushita, Yohsuke
    Aoki, Hideyuki
    Shishido, Takahiro
    Okuyama, Noriyuki
    FUEL, 2022, 309
  • [22] Effect of temperature on thermal properties of high-strength concrete
    Kodur, VKR
    Sultan, MA
    JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2003, 15 (02) : 101 - 107
  • [23] Effect of Mineralogy and Carbon Structure on Coke Properties of Australian and Chinese Coals and Their High Temperature Behaviour
    Shen Fenglei
    Sushil, Gupta
    Veena, Sahajwalla
    Liu Yang
    Meng Qingbo
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2009, 16 : 373 - 379
  • [24] Degradation of Structure and Properties of Coke in Blast Furnace: Effect of High-Temperature Heat Treatment
    Chen, Jingbo
    Ren, Wei
    Guo, Yan
    Zhang, Shengfu
    CHARACTERIZATION OF MINERALS, METALS, AND MATERIALS 2022, 2022, : 163 - 175
  • [25] Effect of Air Temperature on the Thermal Behavior and Mechanical Properties of Wire Rod Steel during Stelmor Cooling
    Hwang, Joong-Ki
    ISIJ INTERNATIONAL, 2022, 62 (11) : 2343 - 2354
  • [26] Thermal Properties and Wetting Behavior of High Temperature Zn-Al-In Solders
    Tomasz Gancarz
    Janusz Pstruś
    Przemysław Fima
    Sylwia Mosińska
    Journal of Materials Engineering and Performance, 2012, 21 : 599 - 605
  • [27] Thermal Properties and Wetting Behavior of High Temperature Zn-Al-In Solders
    Gancarz, Tomasz
    Pstrus, Janusz
    Fima, Przemysaw
    Mosinska, Sylwia
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (05) : 599 - 605
  • [28] Study on the effect of surface area on the thermal behavior of crude oils with different properties
    Chen H.
    Liu X.
    Tan X.
    Tian X.
    Yang S.
    Yang R.
    Zhang C.
    Huagong Xuebao/CIESC Journal, 2021, 72 (06): : 3338 - 3348
  • [29] Effect of Solution Precursor on Microstructure and High-Temperature Properties of the Thermal Barrier Coating Made by Solution Precursor Plasma Spray (SPPS) Process
    Kebriyaei, Amir
    Rahimipour, Mohammad Reza
    Razavi, Mansour
    Herfati, Atabak Alizade
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2023, 32 (01) : 8 - 28
  • [30] Effect of Preoxidation O2 Concentration on the Reduction Reaction of NO by Char at High Temperature
    Fan, Weidong
    Li, Yu
    Xiao, Meng
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2013, 52 (18) : 6101 - 6111