Effects of Ce-Modified TiN Inclusions on the Fatigue Properties of Gear Steel 20CrMnTi

被引:10
作者
Wang, Jian [1 ,2 ]
Peng, Jun [1 ,2 ]
Zhang, Fang [1 ,2 ]
Li, Yujie [1 ,2 ]
Zhang, Xin [1 ,2 ]
An, Shengli [1 ,2 ]
机构
[1] Inner Mongolia Univ Sci & Technol, Sch Mat & Met, Baotou 014010, Peoples R China
[2] Inner Mongolia Univ Sci & Technol, Inner Mongolia Key Lab Adv Ceram Mat & Devices, Baotou 014010, Peoples R China
基金
中国国家自然科学基金;
关键词
gear steel; high cycle fatigue; crystallography; finite element analysis; MECHANICAL-PROPERTIES; GRAIN-REFINEMENT; BEARING STEEL; MICROSTRUCTURE; TOUGHNESS; ALLOYS;
D O I
10.3390/cryst13071071
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
In this paper, the results of a study on the influences of different morphologies, types, and sizes of inclusions on the fatigue lives of 20CrMnTi are reported. The results show that the addition of the rare earth element Ce can lead to the formation of spherical CeAlO3-TiN inclusions in 20CrMnTi. The fatigue performance of 20CrMnTi-Ce was significantly improved compared to that of 20CrMnTi. Using the "edge-to-edge matching" crystallographic theory, CeAlO3 was validated as a suitable hetero-nucleus core for TiN, and the following best orientation relationships between them were determined: [010]TiN//[2(11) over bar 1] CeAlO3 &(002) TiN//(11(2) over bar 1)(CeAlO3). The fatigue cycle times of 20CrMnTi-Ce range up to 10(7), and this value is higher than that of 20CrMnTi without Ce. As the size of the TiN inclusions increases, the maximum stress of the steel matrix also increases. Also, the high-stress and low-life regions noticeably increase, thus increasing the possibility of a fatigue fracture. Under the same sizes of inclusions, the high-stress and low-life regions of square TiN are larger than those of circular TiN.
引用
收藏
页数:12
相关论文
共 25 条
[1]   Influence of the addition of gadolinium on the microstructure and mechanical properties of duplex stainless steel [J].
Ahn, Ji-Ho ;
Jung, Hyun-Do ;
Im, Jae-Han ;
Jung, Ki Ho ;
Moon, Byung-Moon .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 658 :255-262
[2]   Refinement of Solidification Structure of H13 Steel by Rare Earth Sulfide [J].
Bao, Daohua ;
Cheng, Guoguang ;
Huang, Yu ;
Qiao, Tong ;
Dai, Weixing .
STEEL RESEARCH INTERNATIONAL, 2022, 93 (01)
[3]  
BROOKSBANK D, 1969, J IRON STEEL I, V207, P474
[4]   Microstructure and mechanical properties of high boron white cast iron with about 4 wt% chromium [J].
Chen, Xiang ;
Li, Yanxiang ;
Zhang, Huiming .
JOURNAL OF MATERIALS SCIENCE, 2011, 46 (04) :957-963
[5]  
[丁文华 DING Wenhua], 2007, [材料导报, Materials Review], V21, P67
[6]   In-depth analysis of the fatigue mechanism induced by inclusions for high-strength bearing steels [J].
Gu, Chao ;
Liu, Wen-qi ;
Lian, Jun-he ;
Bao, Yan-ping .
INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2021, 28 (05) :826-834
[7]   Influence of dissolved cerium and primary inclusion particles of Ce2O3 and CeS on solidification behavior of Fe-0.20mass%C-0.02 mass%P alloy [J].
Guo, MX ;
Suito, H .
ISIJ INTERNATIONAL, 1999, 39 (07) :722-729
[8]   Propensities of crack interior initiation and early growth for very-high-cycle fatigue of high strength steels [J].
Hong, Youshi ;
Lei, Zhengqiang ;
Sun, Chengqi ;
Zhao, Aiguo .
INTERNATIONAL JOURNAL OF FATIGUE, 2014, 58 :144-151
[9]  
Hui W.J., 1998, Spec. Steel, V19, P8
[10]  
[栗宏伟 Li Hongwei], 2015, [钢铁研究学报, Journal of Iron and Steel Research], V27, P49