Regulation of precipitation behavior among T1, S', and θ' phases in Al-Cu-Li-(Mg-Ag) alloys by optimizing Ag/Mg ratios

被引:31
作者
Xu, Xuanxi [1 ,2 ]
Wu, Guohua [1 ,2 ]
Zhang, Liang [1 ,2 ]
Tong, Xin [1 ,2 ]
Qi, Fangzhou [1 ,2 ]
Guo, Youjie [1 ,2 ]
Li, Liangbin [3 ]
Xiong, Xunman [3 ]
Wang, Cunlong [4 ]
机构
[1] Shanghai Jiao Tong Univ, Natl Engn Res Ctr Light Alloy Net Forming, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
[2] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, State Key Lab Met Matrix Composites, Shanghai 200240, Peoples R China
[3] Jiangxi Ganfeng Lithium Co Ltd, Xinyu 338004, Jiangxi, Peoples R China
[4] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212013, Jiangsu, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2023年 / 876卷
基金
中国国家自然科学基金;
关键词
Al-Cu-Li alloys; Ag; mg ratio; Precipitation behavior; Mechanical properties; Fracture; MINOR SOLUTE ADDITIONS; MECHANICAL-PROPERTIES; T-1; PHASE; MG CONCENTRATION; KINETICS; AG; EVOLUTION; MICROSTRUCTURE; STRENGTH; QUANTIFICATION;
D O I
10.1016/j.msea.2023.145158
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In third-generation Al-Cu-Li alloys, T1, S', and & theta;' precipitates are the primary strengthening phases, and the strength-ductility synergy of the alloys depends strongly on their precipitation behavior. This study aimed to regulate the precipitation behavior among these precipitates by optimizing Ag/Mg ratio in Al-Cu-Li alloys, and its influence on mechanical properties and fracture mechanism was investigated. To this end, four alloys were designed with a total content of 1.1 wt% of Ag and Mg, and an Ag/Mg ratio ranging from 0.24 to 5.63. The results shows that an increase in the Ag/Mg ratio dramatically accelerated the ageing process and shortened the peak ageing time. At 150 degrees C, the precipitation sequence of alloys with an Ag/Mg ratio below 0.95 was SSS & RARR;GPB zone +& delta;& PRIME;/& beta;'& RARR;S'+T1, which transformed into SSS & RARR;GP zone +& delta;& PRIME;/& beta;'& RARR;& theta;'+T1 when the Ag/Mg ratio was above 1.87. The T1, S', and & theta;' precipitates coexisted and were dispersedly distributed among studied alloys with an Ag/Mg ratio ranging from 0.95 to 1.87. An Ag/Mg ratio of 1.87 resulted in the fastest ageing hardening response and the highest strength (YS = 705 MPa, UTS = 717 MPa) because of the highest volume fraction of T1 precipitates. Moreover, the fracture mode changed from transgranular fracture to intergranular fracture with increasing Ag/ Mg ratio due to the difference in distribution and number density of these precipitates between the matrix and grain boundary.
引用
收藏
页数:16
相关论文
共 50 条
  • [31] Aging precipitation of Al-Mg-Si alloys with additions of Ag and Cu
    Nishikubo, M.
    Matsuda, K.
    Oe, Y.
    Nakamura, J.
    Ikeno, S.
    ALUMINIUM ALLOYS 2014 - ICAA14, 2014, 794-796 : 981 - +
  • [32] Complex Precipitation Sequences of Al-Cu-Li-(Mg)Alloys Characterized in Relation to Thermal Ageing Processes
    Zhen Gao
    Jiang-Hua Chen
    Shi-Yun Duan
    Xiu-Bo Yang
    Cui-Lan Wu
    ActaMetallurgicaSinica(EnglishLetters), 2016, 29 (01) : 94 - 103
  • [33] Complex Precipitation Sequences of Al-Cu-Li-(Mg) Alloys Characterized in Relation to Thermal Ageing Processes
    Gao, Zhen
    Chen, Jiang-Hua
    Duan, Shi-Yun
    Yang, Xiu-Bo
    Wu, Cui-Lan
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2016, 29 (01) : 94 - 103
  • [34] Effect of be addition on the precipitation behaviors and mechanical properties in Al-Cu-Li-Mg-Zr-(Ag) alloys
    Kim, JK
    Chung, DS
    Park, HS
    Enoki, M
    PRICM 5: THE FIFTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, PTS 1-5, 2005, 475-479 : 381 - 384
  • [35] Microstructure of Al-5Cu-1Li-0.6Mg-0.5Ag-0.5Mn Alloys
    Chen, Wenzheng
    Zhang, Wenlong
    Ding, Dongyan
    Xiao, Daihong
    METALS, 2021, 11 (01) : 1 - 13
  • [36] Precipitation Hardening and Statistical Modeling of the Aging Parameters and Alloy Compositions in Al-Cu-Mg-Ag Alloys
    Al-Obaisi, A. M.
    El-Danaf, E. A.
    Ragab, A. E.
    Soliman, M. S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (06) : 2432 - 2444
  • [37] Hardening Behavior in Aged Al-4%Cu-0.3%Mg Alloys with 0.5 and 2%Ag Additions
    Moreno Palmerin, Joel
    Dorantes Rosales, Hector J.
    Lopez Hirata, Victor M.
    Cayetano Castro, Nicolas
    Gonzalez Velazquez, Jorge L.
    Morales Ramirez, Angel de J.
    MATERIALS TRANSACTIONS, 2009, 50 (12) : 2785 - 2789
  • [38] The influence of preaging on the strength and precipitation behavior of a deformed Al-Cu-Mg-Ag alloy
    Bai, Song
    Yi, Xinlei
    Liu, Zhiyi
    Wang, Jian
    Zhao, Juangang
    Ying, Puyou
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 764 : 62 - 72
  • [39] Temperature Ranges of Phase Transformations and Mechanical Properties of Alloys of the Al - Cu - Mg - Ag System with Various Cu/Mg Ratios
    V. V. Teleshov
    E. Ya. Kaputkin
    A. P. Golovleva
    N. P. Kosmacheva
    Metal Science and Heat Treatment, 2005, 47 : 139 - 144
  • [40] Combined Effect of Ag and Mg Additions on Localized Corrosion Behavior of Al-Cu Alloys with High Cu Content
    Wang, Jian
    Liu, Zhiyi
    Bai, Song
    Cao, Jing
    Zhao, Juangang
    Zeng, Diping
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (09) : 6108 - 6117