共 50 条
Biosynthesis of MgO Nanoparticles and Their Impact on the Properties of the PVA/Gelatin Nanocomposites for Smart Food Packaging Applications
被引:10
作者:
Rabee, Marwa
[1
,2
]
Elmogy, Soma Ahmed
[3
]
Morsy, Mohamed
[4
,5
]
Lawandy, Samir
[3
]
Zahran, Magdy Abdle Hamid
[6
]
Moustafa, Hesham
[1
,2
]
机构:
[1] Natl Inst Stand NIS, Dept Polymer Metrol & Technol, Giza 12211, Egypt
[2] Natl Inst Stand NIS, Bioanal Lab, Giza 12211, Egypt
[3] Natl Inst Stand NIS, Mat Testing & Surface Chem Anal Lab, Giza 12211, Egypt
[4] Housing & Bldg Natl Res Ctr HBRC, Bldg Phys & Environm Inst, Giza 12611, Egypt
[5] British Univ Egypt BUE, Nanotechnol Res Ctr NTRC, Cairo 11837, Egypt
[6] Menoufia Univ, Fac Sci, Organ Chem, Shibin Al Kawm 32511, Egypt
关键词:
active and intelligent packaging;
biosynthesis MgO NPs;
Boswellia serrata gum;
PVA/gelatin;
mechanicalproperties;
humidity-sensing properties;
MAGNESIUM-OXIDE NANOPARTICLES;
GELATIN;
FILMS;
ANTIOXIDANT;
STARCH;
D O I:
10.1021/acsabm.3c00723
中图分类号:
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
Fabricating active and intelligent packaging materials has become the highest demand for catering to market needs, especially after the COVID-19 pandemic, for ensuring food safety. Thus, the wider objective of this article was to promote active and smart packaging biofilms possessing antibacterial and humidity-sensing properties for sustainable poly(vinyl alcohol) (PVA)/gelatin (Ge) reinforced with biosynthesized magnesium nanoparticles (MgO NPs) by a solvent-casting route. The UV-visible spectrum has been utilized to determine the optimized biosynthesized MgO NPs and then the nanostructure of optimized MgO NPs investigated by varying techniques such as XRD, SEM-EDX, TEM, FT-IR, and thermogravimetric analysis. Four MgO NPs proportions (i.e., 1, 3, 5, and 10 wt %) were used to fabricate PVA/Ge biofilms. In the biofilms system, the tensile results showcased that the nanocomposite film containing 5 wt % of MgO NPs had the highest tensile strength value (i.e., 22.10 MPs) compared to the other biofilms or the unfilled blank (i.e., 6.30 MPs). Correspondingly, the humidity-sensing data revealed that the PVA/Ge-1% MgO NPs sensor had higher sensitivity over a broad range of relative humidity from (7-97% RH) and at 100 Hz. Additionally, the hydrophobicity of biofilms, measured by water contact angle, UV-stability, and antioxidant and antibacterial properties was also analyzed to possibly use these biofilms in active food packaging with extended shelf life of foodstuffs. However, the PVA/Ge-1% MgO NPs biofilm was predominately found to possess attractive sensing properties and could be considered as a sensor for intelligent food packaging.
引用
收藏
页码:5037 / 5051