Effect of Two-Step Sintering on the Mechanical and Electrical Properties of 5YSZ and 8YSZ Ceramics

被引:6
|
作者
Li, Yunpeng [1 ,2 ]
Sun, Hongqian [1 ]
Song, Jing [1 ]
Zhang, Zhiyu [1 ]
Lan, Hao [3 ]
Tian, Liangliang [4 ]
Xie, Keqiang [2 ]
机构
[1] Chinese Acad Sci, Inst Proc Engn, Natl Engn Res Ctr Green Recycling Strateg Met Reso, Beijing 100190, Peoples R China
[2] Kunming Univ Sci & Technol, Coll Met & Energy Engn, Kunming 650093, Peoples R China
[3] Chinese Acad Sci, Ganjiang Innovat Res Inst, Ganzhou 341119, Peoples R China
[4] Chongqing Univ Arts & Sci, Sch Elect Informat & Elect Engn, Chongqing 402160, Peoples R China
关键词
YSZ; two-step sintering; grain refining; fracture toughness; electrical conductivity; YTTRIA-STABILIZED ZIRCONIA; SOLID-ELECTROLYTE; 8Y-FSZ CERAMICS; TEMPERATURE; MICROSTRUCTURE; DENSIFICATION; CONDUCTIVITY; STRENGTH; ALUMINA; PHASES;
D O I
10.3390/ma16052019
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Yttria-stabilized zirconia (YSZ) has been widely used in structural and functional ceramics because of its excellent physicochemical properties. In this paper, the density, average gain size, phase structure, and mechanical and electrical properties of conventionally sintered (CS) and two-step sintered (TSS) 5YSZ and 8YSZ are investigated in detail. As the grain size of YSZ ceramics became smaller, dense YSZ materials with a submicron grain size and low sintering temperature were optimized in terms of their mechanical and electrical properties. 5YSZ and 8YSZ in the TSS process significantly improved the plasticity, toughness, and electrical conductivity of the samples and significantly suppressed the rapid grain growth. The experimental results showed that the hardness of the samples was mainly affected by the volume density, that the maximum fracture toughness of 5YSZ increased from 3.514 MPa center dot m(1/2) to 4.034 MPa center dot m(1/2) in the TSS process, an increase of 14.8%, and that the maximum fracture toughness of 8YSZ increased from 1.491 MPa center dot m(1/2) to 2.126 MPa center dot m(1/2), an increase of 42.58%. The maximum total conductivity of the 5YSZ and 8YSZ samples under 680 degrees C increased from 3.52 x 10(-3) S/cm and 6.09 x 10(-3) S/cm to 4.52 x 10(-3) S/cm and 7.87 x 10(-3) S/cm, an increase of 28.41% and 29.22%, respectively.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Two-Step Sintering Improved Compaction of Electrophoretic-Deposited YSZ Coatings
    Resetiana Dwi Desiati
    Anawati Anawati
    Eni Sugiarti
    Journal of Materials Engineering and Performance, 2022, 31 : 9888 - 9899
  • [32] Two-Step Sintering Improved Compaction of Electrophoretic-Deposited YSZ Coatings
    Desiati, Resetiana Dwi
    Anawati, Anawati
    Sugiarti, Eni
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2022, 31 (12) : 9888 - 9899
  • [33] Effect of alumina addition on initial sintering of cubic ZrO2 (8YSZ)
    Suarez, Gustavo
    Sakka, Yoshio
    CERAMICS INTERNATIONAL, 2010, 36 (03) : 879 - 885
  • [34] Surface temperature distribution on dense 8YSZ ceramics during the steady stage in AC flash sintering
    Zhu, Fengxian
    Peng, Xinyu
    Liu, Jinling
    Liu, Dianguang
    Ren, Ke
    Wang, Yiguang
    CERAMICS INTERNATIONAL, 2021, 47 (02) : 2884 - 2887
  • [35] Effect of La2O3 addition and sintering mode on the mechanical properties and microstructural evolution on an 8YSZ ceramic alloy
    Muthuchamy, A.
    Nagaraju, Nidhi
    Agrawal, Dinesh K.
    Annamalai, A. Raja
    CERAMICS INTERNATIONAL, 2019, 45 (03) : 3668 - 3674
  • [36] Micro structural control of stabilized zirconia ceramics (8YSZ) through modified conventional sintering methodologies
    Rajeswari, K.
    Reddy, A. Rajasekhar
    Hareesh, U. S.
    Saha, B. P.
    Johnson, R.
    SCIENCE OF SINTERING, 2010, 42 (01) : 91 - 97
  • [37] The effect of ZnO addition on the phase transformation, microstructure, and ionic conductivity of 8YSZ ceramics
    Johar, B.
    Zabar, Y.
    2ND INTERNATIONAL CONFERENCE ON GREEN DESIGN AND MANUFACTURE 2016 (ICONGDM 2016), 2016, 78
  • [38] Effect of powder dispersion on sintering behavior and mechanical properties of nanostructured 3YSZ ceramics
    Pradhan, Mamata
    Kapur, P. C.
    Pradip
    CERAMICS INTERNATIONAL, 2012, 38 (04) : 2835 - 2843
  • [39] Effect of Fe2O3 on properties and densification of 8YSZ by pulsed current activated sintering
    In-Jin Shon
    Song-Lee Du
    In-Yong Ko
    Jung-Mann Doh
    Jin-Kook Yoon
    Jeong-Hwan Park
    Electronic Materials Letters, 2011, 7 : 133 - 137
  • [40] Effect of Fe2O3 on properties and densification of 8YSZ by pulsed current activated sintering
    Shon, In-Jin
    Du, Song-Lee
    Ko, In-Yong
    Doh, Jung-Mann
    Yoon, Jin-Kook
    Park, Jeong-Hwan
    ELECTRONIC MATERIALS LETTERS, 2011, 7 (02) : 133 - 137