Effect of Two-Step Sintering on the Mechanical and Electrical Properties of 5YSZ and 8YSZ Ceramics

被引:6
|
作者
Li, Yunpeng [1 ,2 ]
Sun, Hongqian [1 ]
Song, Jing [1 ]
Zhang, Zhiyu [1 ]
Lan, Hao [3 ]
Tian, Liangliang [4 ]
Xie, Keqiang [2 ]
机构
[1] Chinese Acad Sci, Inst Proc Engn, Natl Engn Res Ctr Green Recycling Strateg Met Reso, Beijing 100190, Peoples R China
[2] Kunming Univ Sci & Technol, Coll Met & Energy Engn, Kunming 650093, Peoples R China
[3] Chinese Acad Sci, Ganjiang Innovat Res Inst, Ganzhou 341119, Peoples R China
[4] Chongqing Univ Arts & Sci, Sch Elect Informat & Elect Engn, Chongqing 402160, Peoples R China
关键词
YSZ; two-step sintering; grain refining; fracture toughness; electrical conductivity; YTTRIA-STABILIZED ZIRCONIA; SOLID-ELECTROLYTE; 8Y-FSZ CERAMICS; TEMPERATURE; MICROSTRUCTURE; DENSIFICATION; CONDUCTIVITY; STRENGTH; ALUMINA; PHASES;
D O I
10.3390/ma16052019
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Yttria-stabilized zirconia (YSZ) has been widely used in structural and functional ceramics because of its excellent physicochemical properties. In this paper, the density, average gain size, phase structure, and mechanical and electrical properties of conventionally sintered (CS) and two-step sintered (TSS) 5YSZ and 8YSZ are investigated in detail. As the grain size of YSZ ceramics became smaller, dense YSZ materials with a submicron grain size and low sintering temperature were optimized in terms of their mechanical and electrical properties. 5YSZ and 8YSZ in the TSS process significantly improved the plasticity, toughness, and electrical conductivity of the samples and significantly suppressed the rapid grain growth. The experimental results showed that the hardness of the samples was mainly affected by the volume density, that the maximum fracture toughness of 5YSZ increased from 3.514 MPa center dot m(1/2) to 4.034 MPa center dot m(1/2) in the TSS process, an increase of 14.8%, and that the maximum fracture toughness of 8YSZ increased from 1.491 MPa center dot m(1/2) to 2.126 MPa center dot m(1/2), an increase of 42.58%. The maximum total conductivity of the 5YSZ and 8YSZ samples under 680 degrees C increased from 3.52 x 10(-3) S/cm and 6.09 x 10(-3) S/cm to 4.52 x 10(-3) S/cm and 7.87 x 10(-3) S/cm, an increase of 28.41% and 29.22%, respectively.
引用
收藏
页数:15
相关论文
共 50 条
  • [11] MICROWAVE SINTERING OF NANOCRYSTALLINE 8YSZ: EFFECT OF HEATING SCHEDULE ON MICROSTRUCTURE, IONIC CONDUCTIVITY, AND MECHANICAL PROPERTIES
    Valefi, Mahdiar
    Falamaki, Cavus
    Fattahi, Ahad
    Ebadzadeh, Touraj
    INTERNATIONAL JOURNAL OF NANOSCIENCE, 2009, 8 (03) : 293 - 298
  • [12] The influence of hafnium removal on the microstructure and properties of 8YSZ ceramics
    Li, Yunpeng
    Sun, Hongqian
    Song, Jing
    Zhang, Zhiyu
    Lan, Hao
    Tian, Liangliang
    Xie, Keqiang
    CERAMICS INTERNATIONAL, 2023, 49 (18) : 29564 - 29572
  • [13] Microstructure and mechanical properties of 8YSZ ceramics by liquid-phase sintering with CuO-TiO2 addition
    Hong-ming Zhou
    Yan-jun Guo
    Jian Li
    Dan-qing Yi
    Lai-rong Xiao
    Journal of Central South University, 2012, 19 : 1196 - 1201
  • [14] Microstructure and mechanical properties of 8YSZ ceramics by liquid-phase sintering with CuO-TiO2 addition
    周宏明
    郭雁军
    李荐
    易丹青
    肖来荣
    JournalofCentralSouthUniversity, 2012, 19 (05) : 1196 - 1201
  • [15] Microstructure and mechanical properties of 8YSZ ceramics by liquid-phase sintering with CuO-TiO2 addition
    Zhou Hong-ming
    Guo Yan-jun
    Li Jian
    Yi Dan-qing
    Xiao Lai-rong
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2012, 19 (05) : 1196 - 1201
  • [16] Electrical and Mechanical Properties of 5YSZ Tubular Thin Film Prepared by Screen Printing Method
    Ghatee, Mojtaba
    Salari, Farid
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2016, 13 (02) : 373 - 381
  • [17] Effect of Manganese Oxide on the Sintered Properties of 8YSZ
    Zhou, Hongming
    Li, Jian
    Yi, Danqing
    Xiao, Lairong
    2011 INTERNATIONAL CONFERENCE ON PHYSICS SCIENCE AND TECHNOLOGY (ICPST), 2011, 22 : 14 - 19
  • [18] Influence of Borosilicate Addition on Mechanical Properties and Sinterability of 8YSZ
    Aktas, B.
    ACTA PHYSICA POLONICA A, 2016, 129 (04) : 677 - 679
  • [19] Effect of isothermal treatment on sintering and properties of YSZ ceramics
    Brinkiene, K.
    Cesniene, J.
    Kapokaite-Dickuviene, R.
    MECHANIKA 2007, PROCEEDINGS, 2007, : 54 - 56
  • [20] Mechanical and electrical properties of 3Y-TZP/SiC and 8YSZ/SiC nanocomposites
    Niihara, K
    Bamba, N
    Choa, YH
    Sekino, T
    ADVANCES IN CERAMIC MATRIX COMPOSITES IV, 1999, 96 : 197 - 208