Effect of diamond seeds size on the adhesion of CVD diamond coatings on WC-Co instrument

被引:16
|
作者
Sedov, Vadim [1 ]
Martyanov, Artem [1 ]
Ashkinazi, Evgeny [1 ]
Tiazhelov, Ivan [1 ]
Savin, Sergey [2 ]
Sovyk, Dmitry [1 ]
Mandal, Soumen [3 ]
Fedorov, Sergey [4 ]
Grigoriev, Sergey [4 ]
Ralchenko, Victor [1 ]
机构
[1] Russian Acad Sci, Prokhorov Gen Phys Inst, 38 Vavilov str, Moscow 119991, Russia
[2] Russian Technol Univ, MIREA, 78 Vernadsky Ave, Moscow 119454, Russia
[3] Cardiff Univ, Sch Phys & Astron, Queens Bldg, Cardiff, Wales
[4] Moscow State Technol Univ STANKIN, Vadkovsky Per 1, Moscow 127994, Russia
基金
俄罗斯科学基金会;
关键词
Diamond; Tungsten carbide; Multilayered films; Chemical vapor deposition; Microwave plasma; Adhesion; Cutting tools; SINGLE-CRYSTAL DIAMOND; TUNGSTEN CARBIDE; SUBSTRATE PRETREATMENTS; TRIBOLOGICAL PROPERTIES; ION-IMPLANTATION; GROWTH DYNAMICS; FILMS; NUCLEATION; DEPOSITION; PLASMA;
D O I
10.1016/j.surfin.2023.102861
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, we investigated the effect of the size of diamond seeds on the adhesion of multilayered poly-crystalline diamond (PCD) films, grown by microwave plasma-assisted chemical vapor deposition (MPCVD). For that, identical WC-Co substrates were separately seeded by a set of diamond powders with various average particle sizes from water-based suspensions using similar seeding procedures. This investigation included pow-ders with a difference in particle sizes of nearly 3 orders of magnitude: from 5 nm up to 2-4 mu m. Seeded substrates were used to grow 8-10 mu m thick multilayered PCD films using MPCVD with time-limited cycling injections of N2 gas. The Raman spectra and scanning electron microscopy (SEM) studies showed the similarity of microstructure and phase composition of all grown films, which confirmed that all films were grown in similar conditions. The performed scratch tests revealed sufficient differences in the adhesion of the films seeded with different diamond particles. The PCD film grown on 250-500 nm particles delaminated even before any mechanical investigations. The substrates seeded with 50 nm particles allowed the formation of the stable PCD film, but it started flaking under a load as small as 15 N. The 2-4 mu m powder allowed the formation of PCD film with decent adhesion, which had local flaking under scratch test, which can be explained by the inhomogeneity of seeds distribution. Detonation nanodiamond (DND) powders allowed the formation of continuous diamond films with decent adhesion, however, powders with positive zeta potential were superior due to a much lower agglomeration of separate particles.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] Adhesion between CVD diamond and WC-Co induced by high-pressure and high-temperature
    dos Santos, S. I.
    Balzaretti, N. M.
    da Jornada, J. A. H.
    DIAMOND AND RELATED MATERIALS, 2006, 15 (09) : 1457 - 1461
  • [22] Development of CVD WC-Co coatings
    Fitzsimmons, M
    Sarin, VK
    SURFACE & COATINGS TECHNOLOGY, 2001, 137 (2-3): : 158 - 163
  • [23] Improvement in the universality of high-performance CVD diamond coatings on different WC-Co substrates by introducing multilayered diamond/β-SiC composite
    Yuan, Ziyao
    Liu, Lusheng
    Song, Haozhe
    Lu, Zhigang
    Yang, Bing
    Xiong, Jiaji
    Huang, Nan
    Jiang, Xin
    DIAMOND AND RELATED MATERIALS, 2021, 116
  • [24] Investigation on adhesion of CVD diamond coatings
    Yang, Shi'e
    Bian, Chao
    Ma, Bingxian
    Li, Huijun
    Wang, Xiaoping
    Yao, Ning
    Zhang, Binglin
    Zhengzhou Daxue Xuebao/Journal of Zhengzhou University, 2003, 35 (01):
  • [25] Effect of Ta diffusion layer on the adhesion properties of diamond coating on WC-Co substrate
    Ma, Dan-dan
    Xue, Yan-peng
    Gao, Jie
    Ma, Yong
    Yu, Sheng-wang
    Wang, Yong-sheng
    Xue, Chen
    Hei, Hong-jun
    Tang, Bin
    APPLIED SURFACE SCIENCE, 2020, 527
  • [26] Effect of substrate temperature on SiC interlayers for diamond coatings deposition on WC-Co substrates
    Hei, Hongjun
    Shen, Yanyan
    Ma, Jing
    Li, Xiaojing
    Yu, Shengwang
    Tang, Bin
    Tang, Weizhong
    VACUUM, 2014, 109 : 15 - 20
  • [27] EFFECT OF SILICON DOPING IN CVD DIAMOND FILMS FROM MICROCRYSTALLINE TO NANOCRYSTALLINE ON WC-Co SUBSTRATES
    Zhang, Jianguo
    Cui, Yuxiao
    Shen, Bin
    Sun, Fanghong
    SURFACE REVIEW AND LETTERS, 2013, 20 (06)
  • [28] WC-Co(6%) surface pretreatments for improving diamond coating adhesion
    Borges, CFM
    Campillo, C
    Ilias, S
    Moisan, M
    INTERNATIONAL CONFERENCE ON PHENOMENA IN IONIZED GAS, VOL I, PROCEEDINGS, 1999, : 109 - 110
  • [29] Effect of WC-Co substrates pre-treatment and microstructure on the adhesive toughness of CVD diamond
    Kamiya, S
    Takahashi, H
    Polini, R
    D'Antonio, P
    Traversa, E
    DIAMOND AND RELATED MATERIALS, 2001, 10 (3-7) : 786 - 789
  • [30] DEPOSITION AND CHARACTERIZATION OF DIAMOND PROTECTIVE COATINGS ON WC-CO CUTTING TOOLS
    Tang, Y.
    Yang, S. L.
    Yi, W. W.
    Yang, Q.
    Li, Y. S.
    Hirose, A.
    Wei, R.
    ADVANCED CERAMIC COATINGS AND INTERFACES III, 2009, 29 (04): : 69 - +