Investigations on microstructure and mechanical properties of cast Mg-Gd-Y-Zn-Zr-Nd alloy

被引:24
作者
Dang, Cong [1 ]
Dou, Xiaoxu [1 ]
Wang, Jingfeng [1 ]
Yu, Di [1 ]
Wang, Jinxing [1 ]
Lu, Ruopeng [2 ]
Hou, Hua [2 ,3 ]
Zhao, Yuhong [2 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Natl Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
[2] North Univ China, Coll Mat Sci & Engn, Taiyuan 030051, Peoples R China
[3] Taiyuan Univ Sci & Technol, Coll Mat Sci & Engn, Taiyuan 030024, Peoples R China
来源
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T | 2023年 / 24卷
关键词
Mg-Gd-Y-Zn-Zr-Nd alloy; Heat treatment; Precipitates; LPSO phase; Mechanical properties; STACKING ORDERED PHASE; MAGNESIUM SINGLE-CRYSTALS; AGE-HARDENING RESPONSE; HIGH-STRENGTH; HEAT-TREATMENT; TENSILE PROPERTIES; BEHAVIOR; EVOLUTION; PRECIPITATION; MORPHOLOGY;
D O I
10.1016/j.jmrt.2023.04.089
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Different solution treatments were carried out on the semi-continuously cast Mg-9.55Gd-2.27Y-1.28Zn-0.55Zr-0.11Nd (wt.%) alloy at temperatures of 480 & DEG;C, 500 & DEG;C, and 520 & DEG;C. It was found that the different solution treatment temperatures led to different phase con-stitutions of the alloy. The Mg3RE-type eutectic phases transform into long period stacking order (LPSO) phases with various morphologies after solution treatment. Increasing the solution temperature resulted in larger grain size, greater number of lamellar LPSO phases, and segregation of Zr element. Block LPSO phases also shifted to rod LPSO phase. After ageing treatment, the special spatial structure consisting of prismatic b' precipitates, basal g' precipitates, and lamellar LPSO phases hindered dislocation movement effectively, leading to high strength. However, the accumulation of massive dislocations promoted the premature formation of cracks at the grain boundary and LPSO/Mg matrix interface, resulting in a rapid decrease in ductility of the alloy. After solution treatment at 480 & DEG;C for 12 h and aged at 200 & DEG;C for 48 h, the Mg-9.55Gd-2.27Y-1.28Zn-0.55Zr-0.11Nd alloy exhibited favorable comprehensive mechanical properties at room temperature: ultimate tensile strength (UTS) of 383 MPa, tensile yield strength (TYS) of 269 MPa, and fracture elongation (EL) of 5.1%. & COPY; 2023 Published by Elsevier B.V. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).
引用
收藏
页码:4852 / 4862
页数:11
相关论文
共 50 条
[41]   Effect of heat treatment on mechanical properties and microstructure evolution of Mg-9.5Gd-4Y-2.2Zn-0.5Zr alloy [J].
Zheng, Jie ;
Yan, Zhaoming ;
Ji, Jinsheng ;
Shi, Yusha ;
Zhang, Heng ;
Zhang, Zhimin ;
Xue, Yong .
JOURNAL OF MAGNESIUM AND ALLOYS, 2022, 10 (04) :1124-1132
[42]   Effects of Gd, Y Content on the Microstructure and Mechanical Properties of Mg-Gd-Y-Nd-Zr Alloy [J].
Tang, Changping ;
Wu, Kai ;
Liu, Wenhui ;
Feng, Di ;
Wang, Xuezhao ;
Miao, Guodong ;
Yang, Maomao ;
Liu, Xiao ;
Li, Quan .
METALS, 2018, 8 (10)
[43]   Microstructure and mechanical properties of a peak-aged Mg-5Y-2.5Nd-1.5Gd-0.5Zr casting alloy [J].
Tian, Zheng ;
Yang, Qiang ;
Guan, Kai ;
Meng, Jian ;
Cao, Zhanyi .
JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 731 :704-713
[44]   Microstructure and Mechanical Properties of As-cast Mg-Sm-Gd-Zn-Zr Alloy [J].
Qin C. ;
Che C. ;
Cheng L. ;
Deng R. ;
Zhang H. ;
Wu F. ;
Pan W. .
Zhongguo Xitu Xuebao/Journal of the Chinese Rare Earth Society, 2021, 39 (03) :523-530
[45]   Effect of pack-forging on microstructure and properties of Mg-Gd-Y-Zn-Zr alloy [J].
Wei, Xiaoxiao ;
Jin, Li ;
Liu, Chuanlai ;
Wang, Fenghua ;
Dong, Shuai ;
Dong, Jie .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 802
[46]   Section dimension induced microstructure and mechanical properties variations of sequential solidified sand-cast Mg-10Gd-0.2La-0.1Zn-0.4Zr (wt%) alloy [J].
Lin, Jinming ;
Fu, Penghuai ;
Wang, Yingxin ;
Ding, Yiwen ;
Liu, Hong ;
Peng, Liming ;
Ding, Wenjiang .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 897
[47]   Effect of heat treatment on microstructure, mechanical, corrosion and biocompatibility of Mg-Zn-Zr-Gd-Nd alloy [J].
Jana, Anuradha ;
Das, Mitun ;
Balla, Vamsi Krishna .
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 821
[48]   Study on the assemblage of Y and Gd on microstructure and mechanical properties of hot extruded Mg-Al-Zn alloy [J].
Bu, Fanqiang ;
Yang, Qiang ;
Qiu, Xin ;
Zheng, Tian ;
Zhang, Deping ;
Niu, Xiaodong ;
Li, Yangde ;
Liu, Xiaojuan ;
Meng, Jian .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 639 :198-207
[49]   Effect of Zn on the Mechanical Properties and Microstructure of as-Cast and Solution-Treated Mg-6Y-2Nd-1Gd-0.5Zr Alloys [J].
Tao, J. Q. ;
Huang, S. H. ;
Zhao, G. Z. ;
Huang, Z. W. ;
Wu, Y. ;
Wan, Y. Y. ;
Li, M. .
STRENGTH OF MATERIALS, 2019, 51 (04) :609-615
[50]   Microstructure and mechanical properties of the hot-rolled Mg-Y-Nd-Zr alloy [J].
Wang, Xiao ;
Liu, Chuming ;
Xu, Lu ;
Xiao, Hongchao ;
Zheng, Liang .
JOURNAL OF MATERIALS RESEARCH, 2013, 28 (10) :1386-1393